Prius 2001 modules, many rehydrated

Got something to sell? Have extra parts that need a good home? Have something that others would need to complete their kits? Post it up here and see if anyone else is searching for what you are selling. Guest may post replies to topics already here. All topics here will expire after 90 days of inactivity.

Prius 2001 modules, many rehydrated

Postby fredtr » Sun Nov 13, 2011 10:04 am

I picked up a Prius project which included a full set of 38 Prius 2001 battery modules. These are the ones the sides are all plastic. After 2004 the sides are partially metal. It looks like the previous owner followed the rehydrate instructions on many of these modules. You can see where he drilled the holes, refilled and sealed the holes with epoxy. These have been sitting for a while, the few that I have measured are around 7.4 volts, and I haven't charged any of them. Most have labels indicating voltage and the current they were tested at. The car these came off of has 38,000 miles. I'm located just north of Phoenix AZ, I don't want to ship them. The car had been from an area north of here that is not as hot in the summer. I'm asking $100 OBO for all of them, which is a very good value.

If I knew if it was ok to post my phone number and e-mail address here I would. But I will check responses and get back to you.

Fred
fredtr
10 mW
10 mW
 
Posts: 21
Joined: Sat Jul 25, 2009 5:37 pm

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 10:11 am

So you are selling 38 units for $100? What is the voltage on the labels?

I would agree that you probably shouldn't openly post your phone and email. The regular members here wouldn't do anything malicious with it, but you never know who might be passing through.
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby fredtr » Sun Nov 13, 2011 10:32 am

I just glanced at a few of them, the ones I looked at ranged from 7.4 to 7.96 volts. It is raining here right now, and they are outside under a tarp.

Yes I am selling all of them for $100. It would like for someone to do an EV project with them.

Fred
fredtr
10 mW
10 mW
 
Posts: 21
Joined: Sat Jul 25, 2009 5:37 pm

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 10:52 am

Ok, I was just wondering how close they were to the spec. Sounds like a great deal. I may be driving through AZ soon, I might be interested, but I have to check on some things. Do you know the approximate dimensions of ea unit?
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby fredtr » Sun Nov 13, 2011 11:12 am

Jay, I sent you a private message with my contact info.

Fred
fredtr
10 mW
10 mW
 
Posts: 21
Joined: Sat Jul 25, 2009 5:37 pm

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 11:14 am

I just saw this posted:
Each module is 11 x 4.75 x .75 and contains 6 cells in series for a total nominal voltage of 7.2v and 6.5 amps.


I'm assuming those are inch measurements. I know that you didn't make this post, but do they look like they are about that size in inch measurements?
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 11:19 am

Ok, got your PM, looks like those were in fact inch measurements. Thanks. I'll keep you posted if I can pull off this buy on this trip.
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 12:59 pm

What type of payment would you like? Would paypal work?
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby fredtr » Sun Nov 13, 2011 1:09 pm

Hello Jay, paypal is fine. My e-mail is in the private message I sent to you, which is also my paypal account. Is your trip for certain? Feel free to call me, or send your phone number and I will call you. I'm just getting into this Prius, but have been doing a lot of reading about the battery modules.

Fred
fredtr
10 mW
10 mW
 
Posts: 21
Joined: Sat Jul 25, 2009 5:37 pm

Re: Prius 2001 modules, many rehydrated

Postby Jay64 » Sun Nov 13, 2011 1:28 pm

My trip is not 100% planned out. I'm still in LA at the moment, but am thinking about going up to Colorado on the way out. I was thinking of going up through Vegas, which would put me past your location, so I wasn't sure of driving all the way back down in that direction before heading back home to Florida. But I guess I could swing by Phoenix and on to Albuquerque on the way up to Colorado. Might be a better drive this time a year than going to utah and cutting over. But that means I'm gonna have to miss my girls in Vegas. :evil: :evil: :evil: :evil: I'm still working out the details. :lol:
Johnson64.Com "The stone age didn't end because we ran out of stones."
EV Bikes:
'13 Zero S 11.4kwh.
GS500, ME0913, Sevcon Size 6 Controller, 90v40ah Lipo, GSXR suspension..
'87 Hurricane 600, ME0709, 48v/50a SLA, Kelly KD72400, Magura Throttle, High Current Cycle Analyst.
http://www.evalbum.com/2275
Raleigh beach cruiser: 9C rear hub, stock controller, 48v10ah lithium, Cycle Analyst.
Phat Chopper: 9C front hub, stock controller, 48v12ah a123s, Cycle Analyst.
User avatar
Jay64
1 GW
1 GW
 
Posts: 3129
Joined: Fri Nov 16, 2007 9:03 pm
Location: St. Petersburg, Florida

Re: Prius 2001 modules, many rehydrated

Postby Evoforce » Tue Nov 15, 2011 4:15 pm

I am interested in these and I am in the phx metro area.
"Energy is all consuming and it is never ending. It just changes form as it morphs through time and space... " Evoforce
                                                                                   Several 5403 motors,  no time to build projects! Phoenix Racer(5303) crystalyte suspension mtn bike LiFepo4 72/20.  (409) crystalyte 48 volt hardtail.  In process... Phoenix Cruiser(5304)  LiFePo4 48/20.  First electric bike a 2009 XB 502-700 style, 36/20 sla scooter bike.  All charged by solar!
Evoforce
10 kW
10 kW
 
Posts: 912
Joined: Tue Mar 09, 2010 2:45 am
Location: Fountain Hills Arizona


Return to Items for Sale - Used