the company i was dealing with, ShenZhen Victpower Technology Co. Ltd and the one that actually shipped the item was Delong China Electron CO LTD
U've been warn
[img]http


















agniusm wrote:Have purchased 24 20Ah A123 prismatic cells from china. Today i have received these cells, made in Korea.


liveforphysics wrote:Was that 20Ah pouch that says "made in USA" included in your shipment?
Because those pouches are exclusively made in Korea. No USA A123 pouch cell mfg exists.

toolman2 wrote:liveforphysics wrote:Was that 20Ah pouch that says "made in USA" included in your shipment?
Because those pouches are exclusively made in Korea. No USA A123 pouch cell mfg exists.
ive had heaps of them that say USA as well as Korea, and they ALL have over 19.5ah and can output 300a+ (around 1m ohm, and all seeming pretty dam genuine)
come to think of it in over $5000 worth of these cells, ive only had one that was a bit low in volts on arrival (had self discharge) but now even it came good, so 100% success rate even from some shady Chinese vendors. your out of luck man, just double check the volts, and try charging one..


agniusm wrote:Have purchased 24 20Ah A123 prismatic cells from china. Today i have received these cells, made in Korea. All the cells show below 1V and dropping.




bigmoose wrote:Were the tabs different lengths on the "US" cells versus the "Korea" cells? With the US tab length longer?

miro13car wrote:agniusm,
from your Google data sheet ,
only made in Korea cells are around 1V , all USA-made cells are OK above 3V , right?