Got something to sell? Have extra parts that need a good home? Have something that others would need to complete their kits? Post it up here and see if anyone else is searching for what you are selling. Guest may post replies to topics already here. All topics here will expire after 90 days of inactivity.

All sold!

Postby sangesf » Tue Nov 22, 2011 2:01 am

Have for sale THIS time...

Batch of 60AH slightly used TS cells (The versions with the "Yttrium" added-e.g. LiFeYPo4), these have only been cycled (IN USE) 10-15 each and only down to 40AH max.

I have tested the last 20 of these that I have and ALL of them have 60AH+ (61.3ah-61.6ah. at 1C.
Didn't test over 1.6c because I only have 100a test.. ALL at least 60AH (60.4ah-61.0ah) at 100a.
(3.65v down to 2.7v)
I have at least 8 available and maybe all 20..
Qty:1 = $72 (included shipping)
Qty:2-4 = $68 (included shipping)
Qty:5-8 = $62 (included shipping)

ONLY SHIPPING WITHIN CONTINENTAL USA.. (FREE Shipping)
If you are in Hawaii, Alaska or anywhere outside of USA, I will NOT ship.


This offer is only good for the next 36 hours so act FAST!!
After 36 hours, I will sell them to someone locally.
Last edited by sangesf on Sun Nov 27, 2011 12:06 pm, edited 1 time in total.
sangesf
100 kW
100 kW
 
Posts: 1036
Joined: Fri Nov 14, 2008 8:13 pm

Re: Ok, sold out of HiPower cells.. NOW have 60AH Thundersky

Postby sangesf » Wed Nov 23, 2011 6:51 pm

Sold 5 of them...

3 left...
24 hour extension!
sangesf
100 kW
100 kW
 
Posts: 1036
Joined: Fri Nov 14, 2008 8:13 pm

Re: Ok, sold out of HiPower cells.. NOW have 60AH Thundersky

Postby sangesf » Fri Nov 25, 2011 7:03 pm

1 gone..

2 left....

Last two Available... Last 12 hours... Then gone.
sangesf
100 kW
100 kW
 
Posts: 1036
Joined: Fri Nov 14, 2008 8:13 pm

Re: Ok, sold out of HiPower cells.. NOW have 60AH Thundersky

Postby sangesf » Sun Nov 27, 2011 12:05 pm

ALL gone... Last two were sold locally..
sangesf
100 kW
100 kW
 
Posts: 1036
Joined: Fri Nov 14, 2008 8:13 pm


Return to Items for Sale - Used

Who is online

Users browsing this forum: The Mighty Volt and 1 guest