Have for sale THIS time...
Batch of 60AH slightly used TS cells (The versions with the "Yttrium" added-e.g. LiFeYPo4), these have only been cycled (IN USE) 10-15 each and only down to 40AH max.
I have tested the last 20 of these that I have and ALL of them have 60AH+ (61.3ah-61.6ah. at 1C.
Didn't test over 1.6c because I only have 100a test.. ALL at least 60AH (60.4ah-61.0ah) at 100a.
(3.65v down to 2.7v)
I have at least 8 available and maybe all 20..
Qty:1 = $72 (included shipping)
Qty:2-4 = $68 (included shipping)
Qty:5-8 = $62 (included shipping)
ONLY SHIPPING WITHIN CONTINENTAL USA.. (FREE Shipping)
If you are in Hawaii, Alaska or anywhere outside of USA, I will NOT ship.
This offer is only good for the next 36 hours so act FAST!!
After 36 hours, I will sell them to someone locally.