Urethane protection on Grayborg motor

Electric Motors and Controllers

Urethane protection on Grayborg motor

Postby esoria » Mon Feb 13, 2012 8:37 am

Hallo boys i want to share the Urethane isolation treatment on my Greyborg motor, i use this treatment on my previous motor like 5304, and in 2 year of daily commute in the rain, sun, ecc...
No problem, the water come inside of the motor, but can't create oxydation :)
Attachments
foto 1.JPG
foto 1.JPG (107.51 KiB) Viewed 3168 times
foto 2.JPG
foto 2.JPG (114.74 KiB) Viewed 3168 times
foto 3.JPG
foto 3.JPG (116.07 KiB) Viewed 3168 times
foto 4.JPG
foto 4.JPG (114.63 KiB) Viewed 3168 times
foto 5.JPG
foto 5.JPG (129.41 KiB) Viewed 3168 times
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby Philistine » Mon Feb 13, 2012 9:09 am

In addition to rust/waterproofing, does that also help with minimising heat damage to the windings? Can you give more info on the process and purpose of it?
User avatar
Philistine
1 MW
1 MW
 
Posts: 1981
Joined: Sun Aug 15, 2010 7:33 am

Re: Urethane protection on Grayborg motor

Postby esoria » Mon Feb 13, 2012 9:16 am

The protection is only for Rust-oxydation, not for heat...
Thi is Urethane insulation, dielectric, very very tought against scratch and strong above 250C,
with this system you can run the motor under water for many years :)
My 5304, with big holes in the cover run under water for years, and no oxydation!
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby ohzee » Mon Feb 13, 2012 9:28 am

wow yea that looks nice.
User avatar
ohzee
1 MW
1 MW
 
Posts: 1627
Joined: Wed Jul 20, 2011 1:13 pm
Location: Columbus Ohio USA

Re: Urethane protection on Grayborg motor

Postby itchynackers » Mon Feb 13, 2012 9:29 am

Care to post the type/brand of urethane you used?
9c 9x7f w/ 12awg phases
9c 8x8r w/ 10awg phases, temp sensor, vented
9c 6x10r w/ 10awg phases, temp sensor, liquid cooled, 3rd Place Pikes Peak 2012!

"Don't argue with the galactically stupid...they drag you down to their level and beat you with experience"
itchynackers
100 kW
100 kW
 
Posts: 1136
Joined: Sun Dec 27, 2009 11:11 am
Location: Janesville, WI

Re: Urethane protection on Grayborg motor

Postby Joseph C. » Mon Feb 13, 2012 9:42 am

Very nice.

If this works over a long period of time it will go a long way towards turning hub motors into proper mainstream consumer products. (If the problem with water ingress is anything like what Justin claims.)
Yellow Magpie - Home Of The Talented And The Interesting

http://yellowmagpie.com
Joseph C.
100 kW
100 kW
 
Posts: 1353
Joined: Thu Feb 03, 2011 8:43 am
Location: Ireland

Re: Urethane protection on Grayborg motor

Postby esoria » Mon Feb 13, 2012 9:55 am

http://crcind.com.au/red-urethane

This is similar to my spray, in italy have different name, but is Urethane from CRC brand...
In the manual you can see max temp 250F, but i personally tested above 250C without problem...
Is very very tought, and is not simple to scratch
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby neptronix » Mon Feb 13, 2012 1:43 pm

What i wonder is if this negatively effects heat dissipation... since you sorta have a blanket over the motor now.
ES facebook group: http://facebook.com/#!/home.php?sk=group_125035107565566&ap=1

The all-arounder: 8T MAC motor on a Trek 4500.
The girlfriend bike: 350W front MAC on a 700c Trek.
The wheelie machine: 20" Rear Magic Pie II on a Trek 4300 MTB
The Bus: ??? on a 'da bomb' cargo bike frame

Pro-tips for noobs: Avoid BMS Battery like the plague | Charge RC Lipos to 4.15v, stop discharging at 3.5-3.6v | Use torque plates/arms! | Rear mounted hubs are always best
User avatar
neptronix
100 GW
100 GW
 
Posts: 10251
Joined: Tue Jun 15, 2010 5:56 pm
Location: Salt Lake City, Utah

Re: Urethane protection on Grayborg motor

Postby esoria » Mon Feb 13, 2012 3:50 pm

with my previous motor i don't have more temp after Urethane, i always look temp with laser gun, and no difference :)
The varnish is i think only few micron and can't create difference in temperature
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby markobetti » Tue Feb 14, 2012 2:31 am

very smart. Man , i like that... This is the smartest mod that is not a waist of money like many other mods that eventually dont do anything except empty your pockets.. !
markobetti
10 kW
10 kW
 
Posts: 769
Joined: Fri Jul 17, 2009 1:28 am

Re: Urethane protection on Grayborg motor

Postby esoria » Tue Feb 14, 2012 5:46 am

With 10$ of Urethane, and some vent hole, you have a totally waterproof motor, and more fresh motor under high power output! :)
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby spkpn » Tue Feb 14, 2012 11:48 am

is urethane=ethylcarbamate?

Studies with rats, mice, and hamsters has shown that ethyl carbamate will cause cancer when it is administered orally, injected, or applied to the skin, but no adequate studies of cancer in humans caused by ethyl carbamate has been reported due to the ethical considerations of such studies.[13] However, in 2007, the International Agency for Research on Cancer raised ethyl carbamate to a Group 2A carcinogen that is "probably carcinogenic to humans," one level below fully carcinogenic to humans. IARC has stated that ethyl carbamate can be “reasonably anticipated to be a human carcinogen based on sufficient evidence of carcinogenicity in experimental animals.”[14] In 2006, the Liquor Control Board of Ontario in Canada rejected imported cases of sherry due to excessive levels of ethyl carbamate.
spkpn
10 W
10 W
 
Posts: 85
Joined: Tue Oct 04, 2011 5:44 pm

Re: Urethane protection on Grayborg motor

Postby gogo » Tue Feb 14, 2012 12:41 pm

spkpn wrote:is urethane=ethylcarbamate?

Studies with rats, mice, and hamsters has shown that ethyl carbamate will cause cancer when it is administered orally, injected, or applied to the skin, but no adequate studies of cancer in humans caused by ethyl carbamate has been reported due to the ethical considerations of such studies.[13] However, in 2007, the International Agency for Research on Cancer raised ethyl carbamate to a Group 2A carcinogen that is "probably carcinogenic to humans," one level below fully carcinogenic to humans. IARC has stated that ethyl carbamate can be “reasonably anticipated to be a human carcinogen based on sufficient evidence of carcinogenicity in experimental animals.”[14] In 2006, the Liquor Control Board of Ontario in Canada rejected imported cases of sherry due to excessive levels of ethyl carbamate.


Despite its common name, it is not a component of polyurethanes.
http://en.wikipedia.org/wiki/Ethyl_carbamate
User avatar
gogo
100 kW
100 kW
 
Posts: 1297
Joined: Mon Mar 17, 2008 2:20 pm
Location: Iowa USA

Re: Urethane protection on Grayborg motor

Postby esoria » Tue Feb 14, 2012 4:00 pm

http://it.rs-online.com/mobile/p/vernic ... e/0831141/
Datasheet

No toxic for human :)
Toxic like normal varnish
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby Doctorbass » Tue Feb 14, 2012 4:38 pm

It work well with the X5.. Last year, I applied this special motor purpose varnish in all my motor and never had any problem after!


This big size format cost only 7$ !! and i used like 1/3 for all my 3 X5

http://www.endless-sphere.com/forums/viewtopic.php?f=2&t=24830&hilit=varnish

Image

Image

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6522
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Urethane protection on Grayborg motor

Postby hydro-one » Tue Feb 14, 2012 4:52 pm

Thats Why they call you the Doc. Youve done everything, years before anyone else!!! :mrgreen: :mrgreen:

That does look like a great mod, i will be looking into getting that for my "racing setup" :mrgreen:
hydro-one
10 kW
10 kW
 
Posts: 703
Joined: Fri Dec 19, 2008 2:02 pm
Location: winipeg Canada

Re: Urethane protection on Grayborg motor

Postby esoria » Wed Feb 15, 2012 2:52 am

Good work Doc ;)
I have a question for you....
I see the varnish grab very very well on the stator, or in any rugged metal, but is more difficult for varnish grab to the magnets, because magnets is very very smooth like glass
You do something special on magnets? Scratch with sand paper? Or apply varnish and stop? :)
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby Doctorbass » Wed Feb 15, 2012 10:40 am

esoria wrote:Good work Doc ;)
I have a question for you....
I see the varnish grab very very well on the stator, or in any rugged metal, but is more difficult for varnish grab to the magnets, because magnets is very very smooth like glass
You do something special on magnets? Scratch with sand paper? Or apply varnish and stop? :)



I just cleaned rust and dust of rust around the magnets and fine cleaned everything with acetone.

to remove dust and particules, scotch tape or duck tape is working really well!


if you want to bake the varnish on teh magnet rotor, take care to not go over 60-70 celsius in the oven otherwise you will risk of reducing the magnet field intensity!!
Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6522
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Urethane protection on Grayborg motor

Postby esoria » Wed Feb 15, 2012 10:44 am

yes, usually i prepare in the oven at 50-60C maximum, but varnish on the magnet, don't grab well, not like normal metal...
But ok, if you don't scratch no problem
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby Doctorbass » Wed Feb 15, 2012 12:17 pm

esoria wrote:yes, usually i prepare in the oven at 50-60C maximum, but varnish on the magnet, don't grab well, not like normal metal...
But ok, if you don't scratch no problem



By experience, if you want the paint or varnish to resist scratch, you must wait couples of weeks before the curing time is totally done. than it will like an email
if you try scratching the varnish after two days or a week, you will be able to remive it.. but after few weeks, it's like an email. :wink:

This is also very important to not apply too thick coat.. otherwise it will take months to fully dry.

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6522
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Urethane protection on Grayborg motor

Postby markobetti » Thu Feb 16, 2012 2:45 am

Thank you doc for sharing this info with us
markobetti
10 kW
10 kW
 
Posts: 769
Joined: Fri Jul 17, 2009 1:28 am

Re: Urethane protection on Grayborg motor

Postby esoria » Thu Feb 16, 2012 5:12 am

Thanks Doc ;)
I try to cure for more week before use my motor, now is too much cold here for go in Bycicle :D
esoria
100 W
100 W
 
Posts: 128
Joined: Tue Sep 07, 2010 4:57 am

Re: Urethane protection on Grayborg motor

Postby The Mighty Volt » Sat Mar 17, 2012 10:24 am

Hi folks.

I bought this stuff recently.

ImageImage

http://www.ebay.co.uk/itm/MOTOR-INSULAT ... 521wt_1270


It is described as follows:

Ideal for electric motor windings, transformer coils, tesla coils, solonoid coils and almost any coil winding application that requires insulating, bonding & sealing. This varnish can also be used as an anti-tracking coat on printed circuit boards and components. Can be applied to windings using a small paint brush or components can be dipped.

General Description…
A reliable & convenient air-drying varnish designed for the electrical industry. Anti-tracking varnish provides a tough, impervious, insulating seal in difficult environments. The system dries rapidly in thin film to give very effective sealing off of electrical leakage paths together with excellent noise reduction characteristics. The cured product conforms to BS 5629 type 1.1 (IEC 464), has excellent resistance to transformer oils and moisture, and is suitable for use in Class B and F insulating systems. A low hazard fungicide is included in the varnished enamels, which gives a 0 rating (no growth) fungal resistance when tested to BS 3900 PTG6.

Specifications…
Drying Time Touch Dry In 15 Minutes
Hard Dry In 60 Minutes
Full Cure In 24 Hour
Method Brush, Dip or Spray
Breakdown Voltage (20°C) 1200v/m
l

might be worth a try, I can't seem to get the spray-on stuff in the UK/Ireland.
The Mighty Volt
10 MW
10 MW
 
Posts: 2498
Joined: Sat Oct 17, 2009 9:35 am
Location: Republic of Ireland.

Re: Urethane protection on Grayborg motor

Postby MAGICPIE3FOCUSPOWER » Tue Dec 25, 2012 9:23 am

esoria wrote:yes, usually i prepare in the oven at 50-60C maximum, but varnish on the magnet, don't grab well, not like normal metal...
But ok, if you don't scratch no problem


Yes I have the same problem.
So I sanded the magnets or re painted with normal gray primer.

I didn't like red urethane on the rotor, so removed all painted area :lol:

Normal gray primer is just fine it will hold until 110 celcius.
Nothing is perfect until I touch it...
MAGICPIE3FOCUSPOWER
100 W
100 W
 
Posts: 289
Joined: Thu Aug 23, 2012 4:03 am
Location: The Netherlands

Re: Urethane protection on Grayborg motor

Postby Punx0r » Fri Mar 22, 2013 10:56 am

If looking to clean up an already rusty rotor, how should the laminations be prepared? I'm wondering if sanding could potentially cause them to short to one another?
Punx0r
10 kW
10 kW
 
Posts: 815
Joined: Thu May 03, 2012 8:16 am
Location: England

Next

Return to Motor Technology

Who is online

Users browsing this forum: bearing, ZapPat and 4 guests