Postby Thud » Mon Mar 12, 2012 12:34 am

Kfong asked:
Todd I'm interested in how you are doing internal splines, I have a keyway I need to do on a project and trying different ideas without having to resort to a broach.

I don't know if this is applicable but I though i would share it here & not polute the other sprocket thread.

Any one who follows my threads knows my distain for over priced bicycle parts & my afliction to serial right side drive systems...
Enter the ASC crossfire: a $25 doallar part that has 3 pawles & is one tough hombre. Reason? cause I can't justify spending 80+ dollars on White industries freewheel. Don't get me wrong, they are top of the line for the purpouse. they have limitations in other applications also but thats another discusion.
Tonight i succeded in cutting the splines in a hardend chromoly standard freewheel. like this


& some stills of the tool & the parts:
version 1 almost worked...
Image
version 4 after working out all the kinks:
Image
Image
And the end results:
Image
Image
get some......

All information & advice provided by Thud are "Open Source" & free for personal use & distribution under the following agreement linked below.
http://creativecommons.org/licenses/by-nc-nd/3.0/
User avatar
Thud
10 MW
10 MW
 
Posts: 2386
Joined: Thu Aug 20, 2009 6:20 am
Location: West Michigan,USA

Re: Spline cutting in hardened freewheels.

Postby etard » Mon Mar 12, 2012 1:48 am

Dibs! :lol: How cool is this?! Absolutely brilliant my man, I can't wait for my package to arrive.
Four wheels moves the body, Two wheels moves the soul
Thanks to Justin @ http://www.ebike.ca He brings the soul to ES
User avatar
etard
10 MW
10 MW
 
Posts: 2031
Joined: Sun Aug 03, 2008 3:28 pm
Location: Redlands, CA

Re: Spline cutting in hardened freewheels.

Postby liveforphysics » Mon Mar 12, 2012 2:28 am

You manage to impress me time after time Thud. Brilliant grinding fixture. Brilliant DIY grinder. Brilliant indexing. I love it!

Can I ask how long it took and if you're willing to make more of them for the community?
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 11008
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: Spline cutting in hardened freewheels.

Postby amberwolf » Mon Mar 12, 2012 2:40 am

Needs a little snap-lock light up chevron over the index point...but if it had that then your grinder wheel would vanish as it went thru the glittery center, wouldn't it? ;)


Very nice and very simple setup!
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13819
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: Spline cutting in hardened freewheels.

Postby Miles » Mon Mar 12, 2012 5:52 am

Nice one! :D
User avatar
Miles
100 GW
100 GW
 
Posts: 9289
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Spline cutting in hardened freewheels.

Postby Thud » Mon Mar 12, 2012 6:18 am

LFP asks:
"Can I ask how long it took and if you're willing to make more of them for the community?"


it takes a bit of time worrying the id open & then I made a total of 4 passes on 9 splines to make the cuts..& used a full sleeve of cut off wheels in the proccess
http://compare.ebay.com/like/2509660093 ... s&var=sbar

Need to time study the proccess a little more but it will be close to an hour of monkey busniess.

To answer the question: Of course.
Just send me freewhel & a package of dremel #426b (bulk cut off wheels) & return postage & i'll cut em out for ya'll & ship em back. For the same price Luke has established. :P
Also, luke I have a long stroke hydro press fabbed up & if your father isn't broaching much these days, I could continue the service for the board here if that guide we made found its way back here. (making a new one is on the projects list but this would save a bit of time) Just an offer to keep the projects rolling.

Of course a gratuity would never be refused to help aid funding for the Thud projects Lab. :mrgreen:

I also have a new bolt on reduction unit coming very soon......I'll prolly post it in this thread for feedback.
thanks for the encouragment guy's.
get some......

All information & advice provided by Thud are "Open Source" & free for personal use & distribution under the following agreement linked below.
http://creativecommons.org/licenses/by-nc-nd/3.0/
User avatar
Thud
10 MW
10 MW
 
Posts: 2386
Joined: Thu Aug 20, 2009 6:20 am
Location: West Michigan,USA

Re: Spline cutting in hardened freewheels.

Postby bigmoose » Mon Mar 12, 2012 7:18 am

Todd, great use of wooden fixtures for metal working! It is amazing what your creativity can accomplish. The only twist here would be the wifey would not be preparing me dinner again after I showered her beloved washer and dryer with metal filings! :mrgreen:
bigMoose's electronic pieces & parts (GENUINE IRFB4110Pbf's, Nomex 410, AntiCorrosion Grease, Current Sensors) available HERE.
Thanks to Justin ebikes.ca for securing the board then setting us FREE! Tech Tips in the WiKi: http://endless-sphere.com/w
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave
User avatar
bigmoose
10 MW
10 MW
 
Posts: 2475
Joined: Thu Aug 06, 2009 3:05 pm
Location: Northern Ohio, USA

Re: Spline cutting in hardened freewheels.

Postby bobc » Mon Mar 12, 2012 7:35 am

Superb solution for RH drive enthusiasts - love it!
Any concerns about heating effects? Obviously, if there were a worry you'd just have to grind a little slower ;^) - I guess the ratchet is on the outside part.
bobc
1 kW
1 kW
 
Posts: 439
Joined: Thu Jan 20, 2011 5:08 pm
Location: Knutsford England

Re: Spline cutting in hardened freewheels.

Postby kfong » Mon Mar 12, 2012 9:48 am

Thanks for the post Todd, I knew you would come up with something unique and brilliant. It gives me lots of ideas on making my own. Was wondering how you found the right size grind wheel. Stacks of dremel wheels, damn that's resourceful!
kfong
1 MW
1 MW
 
Posts: 1656
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: Spline cutting in hardened freewheels.

Postby Thud » Mon Mar 12, 2012 10:32 am

Kfong,
I remember where I saw this groove cutting set up on the board: page 2 about 1/2 way down:
viewtopic.php?f=28&t=13532&start=15

Also I have seen a clapper head built & set up on a drill press quill for plunging small trunions into gun recievers (gunsmiths have all sorts of goodies) this can be scaled to any size to cut metal befor its heat treated to hardnes & tempered. (once its hardend you only option is grinding :evil: )
hope that helps.
T
get some......

All information & advice provided by Thud are "Open Source" & free for personal use & distribution under the following agreement linked below.
http://creativecommons.org/licenses/by-nc-nd/3.0/
User avatar
Thud
10 MW
10 MW
 
Posts: 2386
Joined: Thu Aug 20, 2009 6:20 am
Location: West Michigan,USA

Re: Spline cutting in hardened freewheels.

Postby kfong » Mon Mar 12, 2012 10:41 am

Another great find, I keep thinking I need the mill to spin. Forget how soft metal can be if you take light cuts and leverage. I'll have to try these methods. With a CNC it makes the repetitive stuff easy.

Thud wrote:Kfong,
I remember where I saw this groove cutting set up on the board: page 2 about 1/2 way down:
http://endless-sphere.com/forums/viewto ... 2&start=15

Also I have seen a clapper head built & set up on a drill press quill for plunging small trunions into gun recievers (gunsmiths have all sorts of goodies) this can be scaled to any size to cut metal befor its heat treated to hardnes & tempered. (once its hardend you only option is grinding :evil: )
hope that helps.
T
kfong
1 MW
1 MW
 
Posts: 1656
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: Spline cutting in hardened freewheels.

Postby nicobie » Mon Mar 12, 2012 1:52 pm

That's pretty damn clever.

Amazing what can be done if one puts their mind to it.
Image

May your tote always stay tight and your edge eversharp :wink:

my eTownie build thread: viewtopic.php?f=6&t=23701
User avatar
nicobie
1 MW
1 MW
 
Posts: 1824
Joined: Thu Aug 07, 2008 1:48 pm
Location: Central Coast CA,USA

Re: Spline cutting in hardened freewheels.

Postby Byte » Mon Mar 12, 2012 3:05 pm

Awesome! I was reading that topic a few weeks ago and I was also thinking about something like this. But this is just awesome, so well-thought! You're a genius :mrgreen:
Bergli
Turnigy 80-100 130kv
10S 16Ah LiPo
Castle Creations HV 160
User avatar
Byte
100 W
100 W
 
Posts: 250
Joined: Thu Mar 04, 2010 9:39 am
Location: Venlo, Netherlands

Re: Spline cutting in hardened freewheels.

Postby drewjet » Mon Mar 12, 2012 3:05 pm

Nice job Thud. I love back yard engineering.
ImageSuzuki SP200, Mars Brushless, 300 Amp Kelly Controller,(18S12P) http://www.evalbum.com/1511
3220 Mountain Bike viewtopic.php?f=28&t=16705&p=244317#p244317
Suzuki Lipo Upgrade viewtopic.php?f=10&t=23088&p=335986#p335986
Race Bike viewtopic.php?f=3&t=32486
User avatar
drewjet
10 kW
10 kW
 
Posts: 895
Joined: Wed Jan 23, 2008 4:34 am
Location: Orlando, FL USA

Re: Spline cutting in hardened freewheels.

Postby etard » Mon Mar 12, 2012 3:57 pm

Thud, 2 comments:

1. The washing machine is supposed to be on the left
2. You have a couple packages coming this week (I hope 19t is what you wanted).
Four wheels moves the body, Two wheels moves the soul
Thanks to Justin @ http://www.ebike.ca He brings the soul to ES
User avatar
etard
10 MW
10 MW
 
Posts: 2031
Joined: Sun Aug 03, 2008 3:28 pm
Location: Redlands, CA

Re: Spline cutting in hardened freewheels.

Postby spinningmagnets » Mon Mar 12, 2012 4:56 pm

I love it! Great job Thud.

Freehubs are cheap and common, and can be easily adapted to be used as a jackshaft. A small track-cog on the left-side disk-brake flange could drive a chainring on the left-side rear-wheel axle. The two jackshaft freewheels isolate the motor input and the pedal input from each other without having to add a freewheeling Bottom-Bracket.

More options are a good thing....
User avatar
spinningmagnets
10 GW
10 GW
 
Posts: 4796
Joined: Fri Dec 21, 2007 10:27 pm
Location: Ft Riley, NE Kansas

Re: Spline cutting in hardened freewheels.

Postby RWP » Tue Mar 13, 2012 9:28 pm

So cool man!
Love your ingenuity and creativity.
User avatar
RWP
1 kW
1 kW
 
Posts: 385
Joined: Sat Dec 20, 2008 2:19 am
Location: SoCal, USA

Re: Spline cutting in hardened freewheels.

Postby mat h physics » Wed Mar 14, 2012 8:41 am

Very nice set up! 8)

People need to be aware of how hard metals are, as conventional cutting is not practical when hardened. The allotopic properties are what make steel so versatile.
As a rule of thumb, if you can't cut it with a file, grinding is the way to go. Unless of course you have access to an EDM machine. :lol:
Specialized Hardrock, still conventional.
Schwinn Avenue, still conventional.
mat h physics
100 W
100 W
 
Posts: 121
Joined: Tue Dec 07, 2010 12:49 pm
Location: Ral, NC

Re: Spline cutting in hardened freewheels.

Postby etard » Wed Mar 21, 2012 11:52 pm

Thud, you get those cutting wheels and freewheel?

I gotta say guys, this is a brilliant setup to go broached freewheels on the freehub! Mine slipped on like a glove and worked perfect from the get go. The only problem is the freehub blew chunks so if you go this route go ahead and lace a nice hub on your setup. Granted, I was pulling power launches using the low gear on the jr brute so that's 5kw with gearing that tops out at 20 mph, you do the math on that. 8) Of course this means that now I'm wanting to lace my Hadley hub into a Jetset rim with spokes that are all the same color... :wink:

thud, can I order another one?
Four wheels moves the body, Two wheels moves the soul
Thanks to Justin @ http://www.ebike.ca He brings the soul to ES
User avatar
etard
10 MW
10 MW
 
Posts: 2031
Joined: Sun Aug 03, 2008 3:28 pm
Location: Redlands, CA

Re: Spline cutting in hardened freewheels.

Postby Thud » Thu Mar 22, 2012 8:32 am

your stuff arived & 100 thanks for the pp.

I have a couple more I was training on (& actually much nicer than the prototype you have in hand)....I''ll ship you one tomorrow bud. sounds like its time to employ the cush drive sprockets to ease the impact on the free hub now...man its allways sump'n
get some......

All information & advice provided by Thud are "Open Source" & free for personal use & distribution under the following agreement linked below.
http://creativecommons.org/licenses/by-nc-nd/3.0/
User avatar
Thud
10 MW
10 MW
 
Posts: 2386
Joined: Thu Aug 20, 2009 6:20 am
Location: West Michigan,USA

Re: Spline cutting in hardened freewheels.

Postby Miles » Thu Mar 22, 2012 10:18 am

Thud wrote:sounds like its time to employ the cush drive sprockets to ease the impact on the free hub now...man its allways sump'n
If the freewheel in the freehub is redundant. Maybe you could make something like the Surly Fixxer, to lock it? There are a few fixed cassette hubs but they're all 6 speed, I think. eg: http://www.tartybikes.co.uk/135mm_fixed ... 10561.html
User avatar
Miles
100 GW
100 GW
 
Posts: 9289
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Spline cutting in hardened freewheels.

Postby Thud » Thu Mar 22, 2012 10:58 am

Thanks Miles,
Yes, the freehub is redundant....I was thinkin of just cleaning all the grease out & locking the freehub with some hi grade epoxy.
Not a fan of skewers either at these power levels, a solid axel will worke better with proper chain adjusters
get some......

All information & advice provided by Thud are "Open Source" & free for personal use & distribution under the following agreement linked below.
http://creativecommons.org/licenses/by-nc-nd/3.0/
User avatar
Thud
10 MW
10 MW
 
Posts: 2386
Joined: Thu Aug 20, 2009 6:20 am
Location: West Michigan,USA


Return to E-Bike Non-hub Motor Drives

Who is online

Users browsing this forum: Majestic-12 [Bot] and 15 guests