Postby bigmoose » Fri Mar 02, 2012 10:37 pm

Don't know if you gents know about the ACDC_EL750B Load. Rated 750 watts 150 amps max, 55 volts max. It will do constant current, or constant resistance and is externally programmable. You can parallel them also. They are not in production anymore, but there are some floating around from time to time. I snagged 5 of them during the past year for a project that I finished up around Christmas. If a couple of these would help someone out, let me know.
Attachments
3384_EL-750B.pdf
(328.89 KiB) Downloaded 74 times
bigMoose's electronic pieces & parts (GENUINE IRFB4110Pbf's, Nomex 410, AntiCorrosion Grease, Current Sensors) available HERE.
Thanks to Justin ebikes.ca for securing the board then setting us FREE! Tech Tips in the WiKi: http://endless-sphere.com/w
"Live simply. Love generously. Care deeply. Speak kindly. Leave the rest to God..." all the best, Dave
User avatar
bigmoose
10 MW
10 MW
 
Posts: 2451
Joined: Thu Aug 06, 2009 3:05 pm
Location: Northern Ohio, USA

Re: 1000W Discharger Project

Postby CamLight » Sat Mar 03, 2012 2:46 am

Alan B wrote:Eagle is common but a painful program to learn and use and expensive to do anything commercial with, so I keep looking for other choices.
I've used it for all my commercial stuff for years now (several dozen boards). While it was...umm...interesting, to learn IMO it's a great package for the price. I haven't found any other that gives you that much for the dollar without being just as tough to master.

But, many people do find it exasperating to use so I can understand that you're still looking. :D
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: 1000W Discharger Project

Postby CamLight » Sat Mar 03, 2012 2:47 am

magudaman wrote:So now I should be able to make my 10 boards and order all of the components from digikey.

Great news, congrats!
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: 1000W Discharger Project

Postby Alan B » Sat Mar 03, 2012 9:16 am

Comparing prices, diptrace is cheaper than eagle for similar capability, though comparisons are not exact.

Reports are that diptrace is easier to learn compared to eagle, and not a command line program with graphics glued on like eagle but an integrated graphical system. Diptrace supposedly has a better system for pad layout and multiple component placement with array feature.

One problem with eagle for a "for profit" but occasional user the pricing is pretty high. "Light" versions of both programs are under $100 but standard versions jump to $900 for eagle vs $350 for diptrace, and Pro versions soar to $1600 for eagle and $700 for diptrace.

I've installed diptrace to give it a shot. Free version is 300 pins, 2 signal layers, non-profit. Includes schematic, PCB layout, parts libraries and autorouter. G code converter to make pcb on CNC router is free.

http://www.cadsoftusa.com/shop/pricing/

http://www.diptrace.com/order.php?en=1


Nice progress on the discharger. :)
-- Alan W6AKB Cromotored FS GreyBorg, Novara MTB 9C, eBikeE Bent BMC, myEbikeWeb and Thanks to Justin at ebikes.ca for rescuing this forum!
User avatar
Alan B
1.21 GW
1.21 GW
 
Posts: 3877
Joined: Sat Sep 11, 2010 7:43 am
Location: San Francisco Bay Area, USA

Re: 1000W Discharger Project

Postby CamLight » Sun Mar 04, 2012 1:26 am

Alan B wrote:Comparing prices, diptrace is cheaper than eagle for similar capability, though comparisons are not exact.

Looking forward to hearing what you think of DipTrace! I've heard some not-so-good things about DipTrace (in addition to Eagle) but it's such a personal choice for so much of it. Trying both programs, all of them actually, is really the best way to go IMHO.
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: 1000W Discharger Project

Postby magudaman » Mon Mar 05, 2012 2:48 pm

Got all the parts ordered. Ended up being kind of a pricy project once everything was said and done but I'm having fun with it too. I finished my board design yesterday and made some final modifications today. It should be ready for etching as soon as my parts arrive later this week.

I'm now messing with the layout on my heatsink. I plan on having the buss bar running down the middle and the their will of course be 10 of those resistors too:

Image

I ended up shrinking the board down from my initial size to make it so it will fit. I now only have room for 1 fastener that will hold down the board but with the FET attached too I think it should be ok.

Image

I am of course going to have to beef up the traces with some solder.

I ran my numbers again and should be able to run 300 amps for single cell 3.7 lithium batteries while still keeping a little head room for junction temp. Total dissipation of 1100w.
Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby darkshirikens » Fri Mar 09, 2012 5:32 am

You know lately ive been thinking of building a single cell and pack charger for myself and i really didn't know where to really start with the single cell I've read around though i seen things about resistors but which one i don't know , but for the whole pack i was just going to use the light bulb trick to drain the pack. im not electronically inclined and reading parts in this thread gave me a slight headache trying to figure out what i could use for what i need so i need help mainly with the single cell discharger or pack or something that can work for both and what im looking for is like .5c through 5c on a headway pack with 12ah cells.
Schwinn Sidewinder Crystalyte 7240 controller, X5305 motor, Headway 72v 12ah 50/100 bms done !!!
Next project on way: Crystalyte Ht rear 3525
darkshirikens
100 W
100 W
 
Posts: 118
Joined: Thu Jun 10, 2010 2:58 am
Location: Pennslyvania

Re: 1000W Discharger Project

Postby CamLight » Sat Mar 10, 2012 12:25 am

darkshirikens wrote:You know lately ive been thinking of building a single cell and pack charger for myself and i really didn't know where to really start with the single cell I've read around though i seen things about resistors but which one i don't know , but for the whole pack i was just going to use the light bulb trick to drain the pack. im not electronically inclined and reading parts in this thread gave me a slight headache trying to figure out what i could use for what i need so i need help mainly with the single cell discharger or pack or something that can work for both and what im looking for is like .5c through 5c on a headway pack with 12ah cells.

It would probably be best to post this in a new thread. That way many more people can read it, and help you, and any responses won't distract from the ongoing 1,000W discharger thread.
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: 1000W Discharger Project

Postby magudaman » Wed Mar 14, 2012 4:50 pm

Thanks John for trying to keep the tread on topic. All the parts have arrived and it has kept me very busy the last couple days! No task has completely failed but nothing has gone smoothly either. The day the parts arrived I started my work on creating the boards. This proved to be a real nightmare. Since I was now trying to do 10x boards at once the board area was much larger than doing a single board like I had test. I did finally get one of my transfers to actually work well enough that I proceeded with the etching. Of course it wasn't until after I do all this that find out there is actually a paper specifically made for this type of transfer, Pulsar Toner Paper. And just to rub a bit of salt into the wound it also available from digikey for a fairly reasonable ~$1.2 a sheet. Apparently it makes crystal clear traces and as soon as it touches water the paper falls right off, no scraping or extending soaking.

Image

The boards turned out pretty nice and all the traces seem to survive and make connections. Now even though I only have a total of hand full of components I still have to solder 36 leads per boards, so 10 boards became fairly tedious pretty fast.

The end product:

Image

Image

The final specs of a single board:

200V Max
30a max
110w Continuous

After that was finally complete it was time to get the heat sink all prepped for the mounting of the 10 boards, 10 current sense resistors, and bus bar. I laid out the part in cad then place them on the heat sink. This was a bit of a challenge since the sink actually already had a good 15 or so holes in it. I then marked all the holes on the sink and started drilling . With in a couple holes I broke a drill off deep in the sink. GRRRR. The bit wasn't the sharpest and had clogged. I then had to move that hole and a couple other holes around to make sure everything would line up. I had originally planned to tap all the 40 or so holes but gave up on that after my 4-40 tap bottomed out and broke off in another hole. Luckily I was able to extract the piece. I decided to go to a #4 screw. After all the holes were drill out some more I added a small chamfer and then sanded the sink up to 1500 grit (overkill). It did really shine up nice even with the million plus holes:

Image (damn Finger!)

I went ahead and put together the bus bar which is 0.5 x 0.25 and created a fuse holder. I currently only have a couple fuses and will need to order some 300 amp ones for the real test.


Now it was time to assembly line the devices on the heat sink. I laid down the resistor with heat sink grease, put all the wires on the boards and then attached them to the sink. After some testing I found 2 boards were not working. After some testing I found the connector was missing a solder on the one and the other had a small trace bridge. Once I started testing all the boards I did notice their current varied by about 4-5% which I assume is due to the 5% 25w resistor. I should have incorporated a little trim pot on the board to compensate for that.

Image

Now what’s left is soldering up the jumper wires that inter connect all the boards, building a case/fan holder, and integrating the microcontroller . I’ll of course post here once I do some full battery tests with manual control. I’m really excited to be able to do 100 amp tests on a couple cells I have around. I also wanted to test a couple of RC Lipo Packs and see how they hold up.

So if I was to do the process again I would go try to go with a TO-247 package FET so I could use less total devices. The other thing that would greatly simplify the process is getting away from a separate current sense shunt. I should have no problem using a wire based sense resistor though I would give up some resolution. I want to start messing around with surface mount stuff so I don’t have drill the boards but I think silk screens become much more important.

So got all the boards interconnected and have been doing some full discharge test with only one fan. I emptied my A123 to zero volts on accident :oops: I pushed that little 12v pack to 140 amps or around 1200 or 1300 watts intermittently. I then did my big headway packs both about 450wh at 50v 20 amps. Everything worked absolutely beautifully. The sink was keeping nice a cool at around 44C to 52C (17C ambient) with the fets at around 60C on the one side and 82c on the other (fan was blowing on one end). With two fans blowing I'll get more balanced air and I'm sure warmer weather shouldn't be a problem even at 1200W. Holds the current perfectly too.

gotta hurry off to work, hopefully I can read over this tonight and figure out what I missed and doesn't make any sense

Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby CamLight » Thu Mar 15, 2012 3:18 pm

magudaman wrote:The final specs of a single board:

200V Max
30a max
110w Continuous

<snip>

So if I was to do the process again I would go try to go with a TO-247 package FET so I could use less total devices. The other thing that would greatly simplify the process is getting away from a separate current sense shunt. I should have no problem using a wire based sense resistor though I would give up some resolution. I want to start messing around with surface mount stuff so I don’t have drill the boards but I think silk screens become much more important.

So got all the boards interconnected and have been doing some full discharge test with only one fan. I emptied my A123 to zero volts on accident :oops: I pushed that little 12v pack to 140 amps or around 1200 or 1300 watts intermittently. I then did my big headway packs both about 450wh at 50v 20 amps. Everything worked absolutely beautifully. The sink was keeping nice a cool at around 44C to 52C (17C ambient) with the fets at around 60C on the one side and 82c on the other (fan was blowing on one end). With two fans blowing I'll get more balanced air and I'm sure warmer weather shouldn't be a problem even at 1200W. Holds the current perfectly too.

gotta hurry off to work, hopefully I can read over this tonight and figure out what I missed and doesn't make any sense


That's great news, congratulations!!! :mrgreen: :mrgreen: :mrgreen:

Be careful when using copper wire as a current sense resistor (if I understood you correctly). Their resistance changes MUCH more as they heat up vs. a current sense resistor. Up to 40-50 times more. That will cause your current to drift a lot as the wire heats up.

If the hot-end FETs are about 82C on the outside, they're "case" temperature (measured in the middle of the plate touching the heat sink) is probably about 90C. Are you still using the AOT410L? If so, with a junction-to-case resistance of (worst case) 0.45C/W, the FET junctions are operating at 90C + (110W*0.45C/W) = 140C if at a 110W power level. That's a great temperature to use as the maximum for long-term reliability (80% of the 175C max).

If you can get all the FETs down to 62C (assume 70C "case" temp), that brings your junction temp down to 70C + (110W*0.45C/W) = 120C....very nice.

Assuming 120C junction, and assuming that you're operating each FET at 110W, you have a system thermal resistance of...
120C - 25C ambient = 95C temp rise
110W/FET x 10 FETs = 1100W total
95C / 1100W = 0.0864C/W system thermal resistance

Those FETs have a 175C max temp rating. That's a 150C allowable temp rise at 25C room temp. For max power, 150C / 0.0864 = 1,736W (if you can get all FETs down to 62C in your above described test).

For high reliability, i.e., not operating at max temp, the allowable temp rise = 140C (80% of 175C) - 25C ambient = 115C. For high-rel power, 115C / 0.0864 = 1,330W.

I would expect that you could start discharges at up to 2,000W without problems as long as the power level dropped (as the pack discharged) to below 1700W in, perhaps, 15 seconds or so.

Nicely done!!!!!
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: 1000W Discharger Project

Postby frodus » Thu Mar 15, 2012 3:51 pm

This is a great project and I've been following closely, as well as talking with John (who f*cking rocks BTW). He helped me figure out max heat dissipation for my Darlington Pairs, heatsink and fans which really helped. Just need to get some proto-board and mod the circuit I was using with some of the Mod's John was talking about.

Keep us updated on this, it's almost like we have an open source discharger here.
Travis Gintz
Electro Motive Force, LLC.
EV Consulting and Sales
User avatar
frodus
100 kW
100 kW
 
Posts: 1475
Joined: Mon Mar 03, 2008 2:24 pm
Location: Portland, OR

Re: 1000W Discharger Project

Postby kfong » Thu Mar 15, 2012 8:33 pm

Nice work Magudaman, is the based off the national dummy load circuit? Or the CBA. I think I might build one.
kfong
1 MW
1 MW
 
Posts: 1646
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: 1000W Discharger Project

Postby magudaman » Sun Mar 18, 2012 11:26 am

kfong wrote:Nice work Magudaman, is the based off the national dummy load circuit? Or the CBA. I think I might build one.


Thanks Kfong, well I started with it based on the national dummy load but then was shown it is just really a well known current sink circuit. Once I knew that there are tons of examples of these things all over. It also took some tuning to figure out why my setup was blowing up at over 35V. It turned out the gate capacitance was actually slowing down the speed in which the op amp could react to changes in current. This was probably brought out even more though because I had gone to a fairly low resistance shunt.

CamLight wrote:
That's great news, congratulations!!! :mrgreen: :mrgreen: :mrgreen:

Be careful when using copper wire as a current sense resistor (if I understood you correctly). Their resistance changes MUCH more as they heat up vs. a current sense resistor. Up to 40-50 times more. That will cause your current to drift a lot as the wire heats up.

If the hot-end FETs are about 82C on the outside, they're "case" temperature (measured in the middle of the plate touching the heat sink) is probably about 90C. Are you still using the AOT410L? If so, with a junction-to-case resistance of (worst case) 0.45C/W, the FET junctions are operating at 90C + (110W*0.45C/W) = 140C if at a 110W power level. That's a great temperature to use as the maximum for long-term reliability (80% of the 175C max).

If you can get all the FETs down to 62C (assume 70C "case" temp), that brings your junction temp down to 70C + (110W*0.45C/W) = 120C....very nice.

Assuming 120C junction, and assuming that you're operating each FET at 110W, you have a system thermal resistance of...
120C - 25C ambient = 95C temp rise
110W/FET x 10 FETs = 1100W total
95C / 1100W = 0.0864C/W system thermal resistance

Those FETs have a 175C max temp rating. That's a 150C allowable temp rise at 25C room temp. For max power, 150C / 0.0864 = 1,736W (if you can get all FETs down to 62C in your above described test).

For high reliability, i.e., not operating at max temp, the allowable temp rise = 140C (80% of 175C) - 25C ambient = 115C. For high-rel power, 115C / 0.0864 = 1,330W.

I would expect that you could start discharges at up to 2,000W without problems as long as the power level dropped (as the pack discharged) to below 1700W in, perhaps, 15 seconds or so.

Nicely done!!!!!


Thanks John it was your devices that inspired me and your circuit that got me started on this whole project! Thanks for the new thermal analysis, I'm loving those numbers! I need to get both fan mounted properly and really get a better idea of how it is working. The FET I ended up using is a FairChild FDP61N20
http://www.fairchildsemi.com/ds/FD/FDP61N20.pdf
It rated at .3c/w max!!! :twisted:

I get those fans mounted properly and get some even heat on the sink then do some more thermal measurements.
Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby magudaman » Tue Apr 03, 2012 4:11 pm

Making progress on the software side now:

Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby jateureka » Thu Apr 12, 2012 10:08 pm

Nice work!

I looked into something similar to this a while back for slightly lower power to test battery capacity but ended up buying a tester for 600W.
Here are the related threads:
500W active load 100V 50A http://endless-sphere.com/forums/viewtopic.php?f=14&t=7446&start=75
Battery capacity tester / active load circuit http://endless-sphere.com/forums/viewtopic.php?f=14&t=17692
Last edited by jateureka on Sun May 20, 2012 8:45 pm, edited 2 times in total.
Bafang; Mac; Ezee; Easy2Ride; PowerPed; Nope; Condor; Aprilia; eLation V2; Razor
jateureka
1 kW
1 kW
 
Posts: 412
Joined: Tue Apr 06, 2010 7:18 pm
Location: Brisbane QLD Australia

Re: 1000W Discharger Project

Postby Gregory » Sun Apr 22, 2012 6:44 pm

Hi Magudaman, great work on this discharger. Good write up too.

How's the software side coming together?
And do you have any thoughts on your plans for this - selling a kit? Open source? Retail?

Cheers,
Greg


1) x5305 Hub Motor in a 24" Sun rim with 10G spokes, Kelly 72601 controller, 74V 10Ah Turnigy LiPo 20C Battery and CycleAnalyst
2) Mac 10T rear hub in a 700C "comfort bike" 15S 5Ah LiPo, stock 28A Xie Cheng controller
User avatar
Gregory
1 kW
1 kW
 
Posts: 434
Joined: Fri Jul 27, 2007 9:18 pm
Location: Perth, Western Australia

Re: 1000W Discharger Project

Postby magudaman » Thu May 17, 2012 1:26 pm

Gregory wrote:Hi Magudaman, great work on this discharger. Good write up too.

How's the software side coming together?
And do you have any thoughts on your plans for this - selling a kit? Open source? Retail?

Cheers,
Greg


Thanks Greg for the compliment, I did finish writing the software and have the beast fully working. I got myself pretty tied up in trying to make my board schematic sort of dropped the whole thing. So I recently decided to make the board schematic a little easier and just be the power supply stuff and controller. I put the fan speed controller and filtering on another board, this should make it a bit easier to put together. My original intention wasn't to really sell these guys but I had thought about trying to get some boards made from the design.

I still think it would be really cool to sell 100w units, heat sinks and all at a reasonable price that could be networked together to create 500w or 1000w or really any combination. Then have a control board that is a separate purchase either analog control (cheap unit) or a digital controller (more expensive but has constant watts and voltage cutoff). I still just don't know that it would be cost effective verse something like a CBA with amplifiers. Really I have too many projects going on already.
Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby HPEV_llc » Fri May 18, 2012 3:19 am

magudaman wrote:So, I blew up my CBA recently and have found it to be rather undersized for sometime now so I figured it was time to build my own serious discharger.


So how did you "blow up" your CBA? Was it operator error or equipment fault?

By the way, great job on your discharger! I'm looking to do charge and discharge testing as well myself and if you could set something up that could use a 1,000 watt charger and/or a 1,000 watt power supply and allow for controlling and data logging 1kW charge or discharge that would be fantastic.
HPEV LLC
High Performance EV
Design::Consulting::Education
HPEV_llc
1 µW
1 µW
 
Posts: 4
Joined: Mon May 24, 2010 12:28 pm

Re: 1000W Discharger Project

Postby frodus » Tue Jul 10, 2012 4:33 pm

how'd this go?

I'm building my op-amps soon, trying to drive with one pot, filtering heavily on the op-amp input.

Using an off the shelf Voltage/Current controller and Temperature controller to alarm and shut down when setpoints are reached.
Travis Gintz
Electro Motive Force, LLC.
EV Consulting and Sales
User avatar
frodus
100 kW
100 kW
 
Posts: 1475
Joined: Mon Mar 03, 2008 2:24 pm
Location: Portland, OR

Re: 1000W Discharger Project

Postby reagle » Thu Jul 12, 2012 9:36 pm

I may be a bit late to chime in here, but Dave Jones over at EEVBLOG had a nice tutorial on making constant current loads:
http://www.eevblog.com/2010/08/01/eevbl ... y-testing/
reagle
100 W
100 W
 
Posts: 134
Joined: Fri Nov 07, 2008 5:33 pm
Location: Upstate NY

Re: 1000W Discharger Project

Postby magudaman » Tue Aug 14, 2012 5:27 pm

reagle wrote:I may be a bit late to chime in here, but Dave Jones over at EEVBLOG had a nice tutorial on making constant current loads:
http://www.eevblog.com/2010/08/01/eevbl ... y-testing/


I love that guy, I wish he live next door to me and I could just walk over and get a hand on some of this stuff!

So the project is basically done. I have the thing in a case with the controller and fan filter hardware all running beautifully. I have a little additional polishing happening in the code but is fully functional in both constant watt mode and constant current. I have still yet to integrate capacity measurement directly into the unit. The fans are temperature controlled and filtered by my sort of buck converter. Here are some final photos:

Image

Image

Image

Thanks for all the help with everything! I still want to consider building some boards with surface mount components and the through hole fet and the fuse. Maybe with some more searching I can get a TO-247 and get to 200w per fet (EDIT OF HOW ABOUT TO-263 and 300w!!!)! Less modules would be really nice!
Lightning Moto Prototype:
4100w BMC 2 Stage Reduction
16s2p Headway 10ah
70a Ecrazyman Custom
User avatar
magudaman
10 kW
10 kW
 
Posts: 759
Joined: Tue Jul 10, 2007 5:41 pm
Location: Bay Area, CA

Re: 1000W Discharger Project

Postby jateureka » Tue Aug 14, 2012 10:26 pm

Awesome looking beasty, nice work!
Bafang; Mac; Ezee; Easy2Ride; PowerPed; Nope; Condor; Aprilia; eLation V2; Razor
jateureka
1 kW
1 kW
 
Posts: 412
Joined: Tue Apr 06, 2010 7:18 pm
Location: Brisbane QLD Australia

Re: 1000W Discharger Project

Postby Gregory » Tue Aug 14, 2012 11:13 pm

Nice work, looks very pro.


1) x5305 Hub Motor in a 24" Sun rim with 10G spokes, Kelly 72601 controller, 74V 10Ah Turnigy LiPo 20C Battery and CycleAnalyst
2) Mac 10T rear hub in a 700C "comfort bike" 15S 5Ah LiPo, stock 28A Xie Cheng controller
User avatar
Gregory
1 kW
1 kW
 
Posts: 434
Joined: Fri Jul 27, 2007 9:18 pm
Location: Perth, Western Australia

Re: 1000W Discharger Project

Postby CamLight » Wed Aug 15, 2012 12:13 am

Nicely done, congratulations!
Looking forward to hearing about your upgrades!
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Previous

Return to Battery Technology

Who is online

Users browsing this forum: dnmun, sacko and 5 guests