Wcarrothers wrote:Will post up photos but the military lion battery is so small you would not know it was there. It actually fits in my under seat bag. 14ah in 15 volt mode..
This kind?

- DSC04987.JPG (45.12 KiB) Viewed 1284 times

- DSC04988label.JPG (81.2 KiB) Viewed 1284 times
If so, there's some specs I found for it here:
viewtopic.php?p=473003#p473003reagarding current limits on it:
Max limits are 6A continuous or 18A for 5 seconds in 30V mode, and 12A continuous or 36A for 5 seconds in 15V mode.
I suspect you are within it's limitations, but it would be good to have a wattmeter on it to find out.

FWIW, I'd love to have a boxful of these to play with. They are a nice package for low-power ebikes.