Recent content by Hassan

  1. H

    DIY Spotwelder

    Thankyou for suggestion. Yes i have looked into those threads before posting but i couldn't find anything specific to my problem . If i decrease my weldtime pulse, it doesn't weld properly so after over an hour of trial and error i found 220ms to be the best pulse time. I donot have the budget...
  2. H

    DIY Spotwelder

    Hi Guys, I want to build a 18650 batterypack of 403VDC of an Electric vehicle. The battery has 5 Segments of 19s8p. The connections are done via copper-nickel(0.1mm copper and 0.1mm Pure nickel) sandwich method. I have built my own spotwelder using MOT. i have used 35mm2 copper wire for...