Ah yes, I see now, my mistake, sorry I think that must be 13s14p, I'm pretty sure I counted 13 cells per group.
Looking at the videos I made, under max load, the other cells (roughly) drop about 100mV - 120mV, while group 1 would drop about 300mV, which results in a 200mV difference.
(At 51V...