you built 5 packs from 18650 cells and now you have 5 batterys with 12v and 30AH with bms each and you want to connect it in series?
there is no 12v lithium pack possible with 18650 cells. 3s is 10.8V and 4s is 14,4V. what did you built there?
you can not connect batterys with bms in series...
hi guys!
i have the phaserunner without the cycle analyst and im trying to limit the speed with a pot on the hall-throttle line. i can limit the speed from 60km/h to about 25km/h this way but i have no torque with this setup. also slightly downhill road and it starts going too fast.
my goal is...
you are so right. i will never forget soldering the xt60 connector to my 16s7p (21700) battery where i forgott to isolate the ground which was already soldered before connecting the positive wire to the xt60 and shorted the 2 pins with the iron. will never forget this event. same from me: dont...
thank you for answer.
cos i use the PR outside i removed all connecors and extended the wires soldering it. then i use the original dashboard for lights controll and speed so i need to split the hall signal for speed monitor so there are 2 controller connected to the hall sensor and i can choose...
hi folks,
after connecting the phaserunner for the first time i started autotune and the motor started to shake violently, the phase wires got hot and error message occured that there is a problem with the hall sensor. i thought the motor is scrap and tryed another but with the same result. so...