I'm looking for a steel frame for my e-bike, and found one which is very cheap, and it says 4130 Chromoly on it. Seller, of course, claims it is CrMo. Is there any simple way of checking whether it really is 4130 steel, or it's just made out of cheap, ordinary steel?