New battery technology posts are a dime a dozen but this one comes with pedigree (the guy was co-creator of the Li battery): https://news.utexas.edu/2017/02/28/goodenough-introduces-new-battery-technology
It seems to tick all the boxes, safer, more energy dense, high charge and discharge rates...