Search results

  1. L

    Anything better than 18650-25R?

    I have 4 2s2p 50.2 v 32 amp yes they are heavier (11 kilos with padding cables and straps) and bugger me expensive.. they are strong though, my old pack (multistars) would sag down to 44.2 volts and get very warm at 12s 50 amp these sag to 47.6 and stay cool at 12s 60 amp
  2. L

    Super hiryuu - A BBS02 / Leafmotor / MXUS 3kW Dual sus. bike

    Old thread i know but i just ran my leaf at 50 volts 65 amps in a EEB frame, foookin great! thanks nep for the awesome thread!
  3. L

    Portable Range Extender

    Right, the pack I have are LiHV multistars, they don't go with anything I own and on their own they suck, so for now i used them in this idea, later I will use 18650s to keep the weight down, the point of this is i can charge both of my bikes and the wifes bike 60 48 and 36 volts respectively...
  4. L

    Portable Range Extender

    ha thanks they just sit there doing bugger all, eventually i will run a set of 18650s in there they are a lot lighter but for now this set up works as an emergency back up in a ruck sack
  5. L

    Portable Range Extender

    Not when the 2 batteries in question are too weak to keep up with the pack, they are old multistars that never really made the ebike grade
  6. L

    Portable Range Extender

    So though i love my E-bike I despise range anxiety.. I have tried the eco riding on longer trips, when faced with a headwind a lot of hills or you just want to be a spanner you can find yourself a long way from home with a almost empty battery, so I tried a trailer that was a mobile solar...
  7. L

    Bent the Doc Bass torque arms

    just an idea but whey didnt you make a mounting on the torqe arm for the rack
  8. L

    Super hiryuu - A BBS02 / Leafmotor / MXUS 3kW Dual sus. bike

    i have been looking at leaf motors for the last couple of weeks for my new build, I am so happy you did this thread thanks!! but do you really run a 12 fet at 70 amps? hell my 12 fet has never seen more than 35..time to get thr programming cable out ...
  9. L

    Cooling fans inside Hub motors

    so surely keep the copper cool, keep the magnets cool?
  10. L

    Bafang BPM code 11

    I run a code 10 36 volt 500 watt at 50 volt 25 amps, its done 3k kilometres now
  11. L

    Putting small heat sink on outside of controller?Worth it?

    Hello brumbrum, did you get around to ordering the mac 12t and controller? if so did you also order the programe cable? brilliant lil piece of kit, reprogrammed my controller today set the lvc up and now it cuts of at a perfect 3.7 volts, its the 6 fet 25 amp so i took it down from 25 amps to...
  12. L

    Re: Street LEGAL Custom Bomber build! :-)

    thats a stunning build hopefully its still going strong! are you still using the brooks seat? im thinking of buying one as my ass is on fire after 60k
  13. L

    Putting small heat sink on outside of controller?Worth it?

    I run a 25 amp infineon at 50 volts, it was situated at the back of the down tube i turned it around 180 degrees and the difference in cooling was unbelivable, here it gets to 40 c in summer n it was so hot i couldnt touch it some days its the really small changes that can make the big...
  14. L

    Anyone running mac motor over 60v without failure?

    Ahh thanks for clearing that up, mine does the weird stuttering thing if im too gentle with the throttle, i just like with it or get going then hit the throttle
  15. L

    New Q8 48V1Kw Rear Driving Hub Motor

    I am thinking about one of these motors on this frame EEB Full Suspension eBike, but i dont know enough about them yet..i dont want to blow 4k on a bike and have a motor that sucks!
  16. L

    My series parralel changer

    That is very true but i was refering to the how to wire up the balance leads, i have seen a few posts using serial connectors but never an explanation as to how but your diagrams helped me a great deal in understanding it, tommorow im off work and will be in the workshop doing just that!
  17. L

    Fun Commuter eBike? Bafang750W or Bomber eBike?

    I am currently debating on the exact same thing, i have a nice comuter but i want something with a lot more capacity and speed so ive started to think about the EEB Full Suspension eBike with a HS 4080 @ 75 volts 40 amps ran with those new fandangaled 6s 16 amp 10c lipos from hobby king, 4 packs...
  18. L

    Anyone running mac motor over 60v without failure?

    What does a jerking take-off usually signify? I have the same problem on my bpm the take off is jerky but not always..No idea as too why
  19. L

    My series parralel changer

    Oh man thanks for making this post i have looked for exactly this for 6 months on the web!!
  20. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    I just reread your post, I forgot to say never connect the balance wires in parallel when the mains are connected in series
  21. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    I never have them connected unless they are on the charger then i use a balance board, avoid discharging your packs to less than 3.8 and dont charge over 4.15 and the packs will live a lot longer, they will go out of balance until you get some cycles on them after that providing all the cells...
  22. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    I also looked at those packs you will have to let us know what you think of them but yes I run mine in series and then parallel charge with no problems apart from pulling them apart for charging is a pain in the ass, don't let your wife lend them to a neighbour for his lawn mower....
  23. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    Yep I know exactly what that is now i have logview i had completly forgotten about it as the pc the program and files where on had the hard drive fail i should graph this pack for a chuckle
  24. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    So mystery solved! this pack was lent out to a neighbour whilst i was at work and returned some days later, he ran his lawn mower with it and totally drained the pack and then recharged it with a nicad charger...safe to say the pack is retired
  25. L

    RC Lipo pack inspection, series/parallel charging, and lifespan/safety tips

    I am sorry to be so ignorant but what do you mean?