a123's AMP20 LiFe cell is the perfect combination of high discharge, fast charge, low thermal load, high capacity, and long cycle/calendar life. They have have a very low IR, and are rated at 30c/600a (10 seconds) and 10c/200a continuous. a123 rates the AMP20 for 3,000 cycles to 100% DOD...