Hello everybody,
A couple of months ago I bough a DIY spotwelder from keenlab.de.
After creating a suitable power supply I have to say: This is the best product I have ever bought.
You can set the amount of energy (in Joule) you want to put into the weld. It has an automatic mode and
a...