If a magnet sticks to it, its steel. Otherwise its aluminum.
If its steel, you might be able to slide a thick box section down the tube.
Then you can weld it without worrying about blowing holes through it.
You need to cut the folding mechanism off first.
Test the frame by jumping up and down...