When calculating internal resistance of my 14S10P Sanyo GA pack based on voltage drop it is around 90-95mOhm.
I read that the internal resistance of one GA cell should be <38mOhms, so I expected the internal resistance to be 14/10*38mOhm + 5mOhm (wire resistance) = <58mOhm.
Are the 35mOhms caused by the connections inside the pack? Or does it have a higher internal resistance on the first cycles?
Weather was cold, but the bike+battery was inside before.
I read that the internal resistance of one GA cell should be <38mOhms, so I expected the internal resistance to be 14/10*38mOhm + 5mOhm (wire resistance) = <58mOhm.
Are the 35mOhms caused by the connections inside the pack? Or does it have a higher internal resistance on the first cycles?
Weather was cold, but the bike+battery was inside before.