I am building my first pack. It is a 14S6P pack that needs to output 30A, but I would like to be able to output 60A, for future proofing. I'm using Molicel P42A cells.

Unfortunately I had to deviate from the usual square shape, to fit the battery below the top tube. Will the wiring layout I designed work?

Please see attachments for details. I would appreciate any advice you have.

Key:
Red - 10AWG bare wire (acting as busbar)
Blue - 0.15mm x 15mm pure nickel strips
 

Attachments

  • battery bottom.png
    battery bottom.png
    634.9 KB · Views: 133
  • top battery.png
    top battery.png
    622.7 KB · Views: 133
  • 20210526_151750.jpg
    20210526_151750.jpg
    333.9 KB · Views: 133