recycling opening 18650 could U get $1 from dead cell?

But it is not Nickel !
It is steel ( sometimes rarely, aluminium)
You will get a much longer strip by pealing down a steel soup/food can.
...( really a good length if you can get hold of those catering size food cans) ! :bigthumb:
 