batteryGOLD
100 W
Today I was around onewhell or onehell !
veicule XR symptoms: no nothing!
cause: baterry LiFePO4 16S at zero volts! long time no charge..
test solution #1: inject some controlled charge into pack.
results: OK revive, but maybe only 50% capacity now.. no more radical
check picture.
https://ibb.co/HGCffF9
veicule XR symptoms: no nothing!
cause: baterry LiFePO4 16S at zero volts! long time no charge..
test solution #1: inject some controlled charge into pack.
results: OK revive, but maybe only 50% capacity now.. no more radical
check picture.