Help w/changing "HighPower Phylion" charger t work w/LiFePO4

Batteries, Chargers, and Battery Management Systems.
Post Reply
sangesf   10 kW

10 kW
Posts: 862
Joined: Nov 14 2008 8:13pm

Help w/changing "HighPower Phylion" charger t work w/LiFePO4

Post by sangesf » Jan 13 2011 6:57pm

So I bought this charger and am able to use it for my lifepo4 battery (36v) however it's high end voltage is only 41.8.
For my 12s LiFePO4 that just won't do.
I did open it up and see three pots..
Anyone know if these can be used to change the output voltage and/or amperage?
Would like to be able to change it to 44.4 CV / ??CC

Model# is HP8204C

dnmun   100 GW

100 GW
Posts: 16190
Joined: Jun 09 2008 1:32pm
Location: portland, or and loveland, co

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by dnmun » Jan 13 2011 7:19pm

turn one of the pots until the voltage reaches the voltage you like. if that doesn't work, adjust another one, and if that doesn't work adjust the third one. if none of that works then you can post up a picture instead.

sangesf   10 kW

10 kW
Posts: 862
Joined: Nov 14 2008 8:13pm

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by sangesf » Jan 13 2011 8:59pm

I'm afraid of just turning pots, that why I asked if someone has tried that yet.
I'm unaware if turning one of them will damage the unit or not.
I can't upload a pic, because I only have an iPhone.
But there are 3 pots..
2 on one daughtercard and one on another one.

sangesf   10 kW

10 kW
Posts: 862
Joined: Nov 14 2008 8:13pm

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by sangesf » Jan 18 2011 12:05pm

Since obviously no one knows about these..
Does anyone have a phone number or email address that I can contact the manufacturer about the adjustability of their charger?

User avatar
Ypedal   100 GW

100 GW
Posts: 12528
Joined: Dec 27 2006 12:55pm
Location: Moncton NB, Canada
Contact:

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by Ypedal » Jan 18 2011 12:19pm

googled it.. http://elite-hk.diytrade.com/sdp/334944 ... 66082.html

those are quite common, the " Hi-Power " brand chargers....

If you touch the pots, mark them before you change anything so you can set them back to the original point.

One is likely amp limit, other high voltage cutoff, one could be the point at wich the unit goes into Constant Voltage stage... .. i have a few of them for nicad and the one that comes with the eZee phylion packs.... never messed with it tho.
ES site status page:
http://www.ypedal.com/ES/ES.htm
----------------
http://www.ypedal.com

User avatar
StudEbiker   1 MW

1 MW
Posts: 1999
Joined: Apr 13 2009 2:15pm
Location: Ashland, OR, USA

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by StudEbiker » Jan 18 2011 12:23pm

I would try dnum's advice. If turning the pots would damage the charger there probably wouldn't be pots there in the first place. Make very small adjustments and see what happens to the voltage and only change one thing at a time. Take a picture of what the pots look like before you change anything. I doubt that even if you were able to get a hold of the manufacturer they would tell you how to change the output.

User avatar
dogman dan   100 GW

100 GW
Posts: 35915
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by dogman dan » Jan 18 2011 2:59pm

I totally agree, put a voltmeter on it if it will output without a battery on it. Then turn 1 pot 1/2 turn. if nothing happens try another after putting the first pot back like it was. When you find one that adjusts voltage, then set to your liking.

sangesf   10 kW

10 kW
Posts: 862
Joined: Nov 14 2008 8:13pm

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by sangesf » Jan 22 2011 3:25pm

I actually played with one of the pots and got lucky that it's the voltage one.
Even if the CC/CV pots is at the same level as normal, it shouldn't hurt my batt/BMS.
it works perfectly.. My cells NOW balance to 3.65 each EXACTLY!

Thanks for the help guys!
(P.S. The afternoon after I finally changed that charger, my new LiFePo4 charger came in. LOL)

Anyone want to by a Phylion charger for 10s li-ion battery and a Phylion charger set for 12s LiFe?

stepfel   1 µW

1 µW
Posts: 1
Joined: Mar 08 2011 10:55am

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by stepfel » Mar 08 2011 10:57am

Hi,

i have the same problem i´ve changeg the f... LION with high impandance to
a real GOOD LIFEPO4 and want also to know:

WICH POTENTIOMETER DID YOU TURN????

Nice regards from Germany
Stefan

User avatar
thewmatusmoloki   10 kW

10 kW
Posts: 654
Joined: Sep 16 2008 9:07am
Location: Gold Coast Australia

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by thewmatusmoloki » Aug 10 2011 5:13pm

Sorry about the late response. I think there are plenty of these chargers around, I just found one in my shed down the back from years ago and thought I'd try to "up" the volts a bit as an opportunity charger for a friends 12s li-poly. Either that or chuck it out.
It's the bottom potentiometer Stefan, it was marked VR03. If you turn it to the left it turns the volts up, careful, cause its aweful sensitive.
bottom one.jpg
bottom one.jpg (52.35 KiB) Viewed 1165 times
fiddyvolts.jpg
fiddyvolts.jpg (55.47 KiB) Viewed 1165 times
Cheers.
Attachments
charger.jpg
charger.jpg (56.33 KiB) Viewed 1165 times

User avatar
jateureka   10 kW

10 kW
Posts: 824
Joined: Apr 06 2010 7:18pm
Location: Brisbane, QLD Australia

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by jateureka » Aug 15 2011 6:52pm

Great info on these popular chargers.
Some other discussion on repair and adjustments here:
http://endless-sphere.com/forums/viewto ... 14&t=16800 HP8204L3 36V 4A adjustment
http://endless-sphere.com/forums/viewto ... 14&t=18616 HP8204L 16S, 58.4VDC 3A repair
E-bikes: Bafang 8FUN; Mac; Ezee; FreeGo; Aprilia 7s LiPo; eLation V2; TerraTrike recumbent
E-motorbikes: ZEV 7100 LR scooter, 84V 60Ah LiFePO4.
ZERO 2011 S motorcycle, 51.8V 70Ah LiMno2, 2012 headlight, Kilovac EV-200 contactor
E-mower: EGO 56V mower & line trimmer

999zip999   100 GW

100 GW
Posts: 9997
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by 999zip999 » Aug 15 2011 7:48pm

when you are done turning the screws and get it right put a little glue on it to keep it from moving. No I don't know the best glue, but something that sets hard, but when you turn it it would brake off. And that will not melt. What potting glue ?

sangesf   10 kW

10 kW
Posts: 862
Joined: Nov 14 2008 8:13pm

Re: Help w/changing "HighPower Phylion" charger t work w/LiF

Post by sangesf » Jan 19 2012 12:18pm

Just a small update regarding this particular (36v) charger...
The left side POT changes the voltage from ~39.2v to ~44.2v.
That's what everyone knows..

The top right POT, I found out, varies the final CC/CV mode from 180mA (.18a) to 220mA (.22a).

Interestingly enough, The bottom right POT varies the max Amp out from 1.8a to 2.2a
(anyone else see, what I found to be interesting)?

User avatar
Ypedal   100 GW

100 GW
Posts: 12528
Joined: Dec 27 2006 12:55pm
Location: Moncton NB, Canada
Contact:

Re: Help w/changing "HighPower Phylion" charger t work w/LiFePO4

Post by Ypedal » May 02 2018 9:23pm

Ok, this is an antique thread but ended up here googling for adjusting the pots / potentiometers on a High Power High-Power HP8204C charger ( writing it like that for future google search results.. f'n creative name for a brand but annoying as hell when searching for tech info instead of sales leads.. )

So the 3 pots.. as described in the above post but only weird thing, i have a CA plugged in to monitor the charging of a few LiGo packs and the charger's output sweeps from 1.4 amps to 2.4 amps while in bulk charge phase... not exactly Constant Current huh.. not sure if this is be design, or because i foolishly played with the pots and did not mark them prior.

Gonna work just fine to charge the packs but throwing that out there if anyone happens to know more about these.