ULtra Compact 1800W charger + Eltek programming

Batteries, Chargers, and Battery Management Systems.
dakoal   100 µW

100 µW
Posts: 8
Joined: Nov 04 2016 2:42am

Re: ULtra Compact 1800W charger + Eltek programming

Post by dakoal » Oct 10 2018 12:10am

jean0 wrote:
Jun 09 2018 9:17am
Ian, You're great! The bigger is NCP1015 switcher, the smaller is BC817 transistor.
I replace them, hope it will solve my problem...
Thanks a lot, buddy.
Hi,

I have 4 dead Flatpacks, not opened yet.
jean0, did you ever bring the Flatpack2 back to life with the 2 parts?

Best regards
Bernhard

grumble & grunt   1 µW

1 µW
Posts: 1
Joined: Oct 06 2018 2:14pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by grumble & grunt » Oct 10 2018 12:09pm

Hi,
Just want to say a massive thanks to all who contributed in getting these gizmos running.
Remmie... you're a demi-god.

First time I've loaded code into anything and I've got a programmable, grunty supply for my battery bank.

Grassy arse.

Camon   1 mW

1 mW
Posts: 10
Joined: Nov 18 2017 6:31pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by Camon » Oct 14 2018 9:12am

Hello again. today I tried again to program the voltage. I have put 122 ohm in can h and can l of arduino leonardo and another r of 122ohm in pcb of eltek. the amber led lights but the voltage does not rise

pm_dawn   100 W

100 W
Posts: 164
Joined: Jan 17 2009 3:36pm
Location: Östersund, Sweden

Re: ULtra Compact 1800W charger + Eltek programming

Post by pm_dawn » Oct 15 2018 12:22am

Hi !
Try to measure the resistance over the bus when both the leonardo and eltek is powered off.

It should be about 60ohms.

If if is lower than that remove the 120 at the Eltek Side.

I only have a resistor at my CAN2USB tool when communicating with the Eltek.


Give that a try.

Regards
/Per

Hayds13   100 mW

100 mW
Posts: 40
Joined: Dec 25 2014 12:48pm
Location: Sydney, Australia
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Hayds13 » Oct 15 2018 12:33am

Hello Camon,
I can see from previous posts you've checked the serial number is in your code...excellent.
Have you tried some basic code that will just get the status from the canbus via Arduino? ie...is it talking? (There are some examples in this thread...but if you need me to repost, let me know).
My PCB breakout board came incorrectly labelled on the canbus pins. you might want to check yours.
My Arduino Leonardo will talk to the flatpack with the terminator connected or disconnected...So I don't think it's that critical.
I have a few flatpacks. All of them (except one) set the voltage correctly. The one that doesn't goes over the set voltage by about 1.7v from memory. So if I set it to maximum, I think it gets upset goes to default. You might want to try and set a lower voltage and see if it works?

pm_dawn   100 W

100 W
Posts: 164
Joined: Jan 17 2009 3:36pm
Location: Östersund, Sweden

Re: ULtra Compact 1800W charger + Eltek programming

Post by pm_dawn » Oct 15 2018 1:31am

Hi Camon !

As Hayds13 says if you have my 60A board for the 3kw units the CAN connection port is labelled wrong.

I have set fixed voltage on a number of units now.
About 15-20 units.
I have had one unit behaving a bit strange.
But I think that it was mostly just that the unit was off in calibration and also had a slow walk in progress.

Are you trying to use fixed setting or continues CAN setting?

Best Regards
/Per

Camon   1 mW

1 mW
Posts: 10
Joined: Nov 18 2017 6:31pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by Camon » Oct 16 2018 10:47am

[/quote]
Hello everyone, thanks for your answers.
pm_dawn wrote:
Oct 15 2018 1:31am
Hi Camon !

As Hayds13 says if you have my 60A board for the 3kw units the CAN connection port is labelled wrong.

Are you trying to use fixed setting or continues CAN setting?

Best Regards
/Per
Currently I do not have any pcb to connect, I connect two wires directly on the ELTEK pcb.
What do you think whit fixed setting or continues can setting? I use these code.

Code: Select all

// Eltek Flatpack Permanent Voltage changer, Code By RHO


#include <mcp_can.h>
#include <mcp_can_dfs.h>
#include <SPI.h>

const int SPI_CS_PIN = 17;                                                          // Set CS pin to pin 17
MCP_CAN CAN(SPI_CS_PIN);                                                            // Set CS pin for CANBUS shield

void setup()                                                                        // Initialisation routine
{
  pinMode(23, OUTPUT);                                                                // Set pin 9 to output (backlight of the LCD)
  digitalWrite(23, HIGH);                                                            // LED on
  delay(250);
  digitalWrite(23, LOW);

START_INIT:

    if(CAN_OK == CAN.begin(CAN_125KBPS))                                            // init can bus : baudrate = 125k !!
    {
    }
    else
    {
    delay(100);
    goto START_INIT;
    }
    unsigned char login[8] = {0x14, 0x49, 0x72, 0x00, 0x31, 0x66, 0x00, 0x00};     //this is the serial number of the Flatpack + 2 [quote=Hayds13 post_id=1418753 time=1539581632 user_id=41294]
Hello Camon,
I can see from previous posts you've checked the serial number is in your code...excellent.
Have you tried some basic code that will just get the status from the canbus via Arduino? ie...is it talking? (There are some examples in this thread...but if you need me to repost, let me know).
My PCB breakout board came incorrectly labelled on the canbus pins. you might want to check yours.
My Arduino Leonardo will talk to the flatpack with the terminator connected or disconnected...So I don't think it's that critical.
I have a few flatpacks. All of them (except one) set the voltage correctly. The one that doesn't goes over the set voltage by about 1.7v from memory. So if I set it to maximum, I think it gets upset goes to default. You might want to try and set a lower voltage and see if it works?
[/quote]added bytes of 00 each)
    CAN.sendMsgBuf(0x05004804, 1, 8, login);                                       //send message to log in and assign ID=1 (last 04 means ID=1, for ID=2 use 05004808 ) 

    unsigned char setdefaultvolt[5] = {0x2B, 0x15, 0x00, 0x44, 0x16};              //this is the command for setting the default output voltage (Last two bytes, LSB first). 16 80 is the maximum voltage of 57.6 V
    CAN.sendMsgBuf(0x05009C02, 1, 5, setdefaultvolt);                              //send message to set ouput voltage to all Flatpacks connected to the CAN-bus
digitalWrite(23, HIGH); 
}

void loop()                                                                        // main program (LOOP)
{                                                                                  // nothing to do :)
}

I tested only with the two 100ohm and 22ohm resistors (I bought 120ohm resistors and I wait it)
Hayds13 wrote:
Oct 15 2018 12:33am

My Arduino Leonardo will talk to the flatpack with the terminator connected or disconnected...So I don't think it's that critical.
I only see the amber LED light up when I have the jumper connected
Hayds13 wrote:
Oct 15 2018 12:33am
You might want to try and set a lower voltage and see if it works?
Hi I try to change the value of voltage to 57Volts 1644HEX and nothing
Hayds13 wrote:
Oct 15 2018 12:33am
Hello Camon,

Have you tried some basic code that will just get the status from the canbus via Arduino? ie...is it talking? (There are some examples in this thread...but if you need me to repost, let me know).
I don't have any idea to get the status can you help me?
pm_dawn wrote:
Oct 15 2018 12:22am
Hi !
Try to measure the resistance over the bus when both the leonardo and eltek is powered off.

It should be about 60ohms.

If if is lower than that remove the 120 at the Eltek Side.

I only have a resistor at my CAN2USB tool when communicating with the Eltek.


Give that a try.

Regards
/Per
I measure with the polymeter in the terminals of the aruino leonardo and I measure 60,56 ohm

Hayds13   100 mW

100 mW
Posts: 40
Joined: Dec 25 2014 12:48pm
Location: Sydney, Australia
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Hayds13 » Oct 16 2018 11:29pm

Hi Camon,

I've edited your code example with commands I used to set to 50.2v. When I try to set my flatpack to 57v in code, it actually goes to over-volt protection shuts down because it goes much higher.

Code: Select all

#include <mcp_can.h>
#include <mcp_can_dfs.h>
#include <SPI.h>

const int SPI_CS_PIN = 17;                                                          // Set CS pin to pin 17
MCP_CAN CAN(SPI_CS_PIN);                                                            // Set CS pin for CANBUS shield

void setup()                                                                        // Initialisation routine
{
  pinMode(23, OUTPUT);                                                                // Set pin 9 to output (backlight of the LCD)
  digitalWrite(23, HIGH);                                                            // LED on
  delay(250);
  digitalWrite(23, LOW);

START_INIT:

    if(CAN_OK == CAN.begin(CAN_125KBPS))                                            // init can bus : baudrate = 125k !!
    {
    }
    else
    {
    delay(100);
    goto START_INIT;
    }
//  unsigned char login[8] = {0x14, 0x49, 0x72, 0x00, 0x31, 0x66, 0x00, 0x00};     //CAMON this is the serial number of the Flatpack + 2 added bytes of 00 each)
    unsigned char login[8] = {0x15, 0x44, 0x71, 0x02, 0x11, 0x66, 0x00, 0x00};     //HB this is the serial number of the Flatpack + 2 added bytes of 00 each)
    CAN.sendMsgBuf(0x05004804, 1, 8, login);                                       //send message to log in and assign ID=1 (last 04 means ID=1, for ID=2 use 05004808 ) 

//  unsigned char setdefaultvolt[5] = {0x2B, 0x15, 0x00, 0x44, 0x16};               //???? INCORRECT ??? this is the command for setting the default output voltage (Last two bytes, LSB first). 16 80 is the maximum voltage of 57.6 V
    unsigned char setdefaultvolt[5] = {0x29, 0x15, 0x00, 0x9C, 0x13};               // 50.2V
//  CAN.sendMsgBuf(0x05009C02, 1, 5, setdefaultvolt);                               //???? WRONG COMMAND ???? send message to set ouput voltage to all Flatpacks connected to the CAN-bus
    CAN.sendMsgBuf(0x05019C00, 1, 5, setdefaultvolt);                               //send message to set ouput voltage to all Flatpacks connected to the CAN-bus

digitalWrite(23, HIGH); 
}

void loop()                                                                        // main program (LOOP)
{                                                                                  // nothing to do :)
}

Hayds13   100 mW

100 mW
Posts: 40
Joined: Dec 25 2014 12:48pm
Location: Sydney, Australia
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Hayds13 » Oct 16 2018 11:38pm

Hi Camon,

This code should set your flatpack temporarily to 50.2v and 14a. You need to change the serial numbers in two places. Upload to Arduino Leonardo and power the Arduino off/on. Then use the serial monitor to see status

Example
04 1A 00 00 A3 13 F1 00 2C
Temperature = 26
Current = 0.00
OutputVoltage = 50.27
OutputPower = 0.00
InputVoltage = 241


Your flatpack will only have green led n, when this is running.

Code: Select all

#include <mcp_can.h>
#include <mcp_can_dfs.h>
#include <SPI.h>

const int SPI_CS_PIN = 17;
MCP_CAN CAN(SPI_CS_PIN);                                                              // Set CS pin for CANBUS shield
#define INT32U unsigned char
void setup()                                                                          // Initialisation routine
{
    Serial.begin(115200);                                                             // Sets the data rate in bits per second (baud) for serial data transmission to PC.
    delay(1000); 
START_INIT:

    if(CAN_OK == CAN.begin(CAN_125KBPS))                                              // init can bus : baudrate = 125k !!
    {
        Serial.println("CAN BUS Shield init ok!");
    }
    else
    {
        Serial.println("CAN BUS Shield init fail");
        Serial.println("Init CAN BUS Shield again");
        delay(100);
        goto START_INIT;
    }
     unsigned char stmp3[8] = {0x15, 0x44, 0x71, 0x02, 0x11, 0x66, 0x00, 0x00};       // ***** Serial number
       CAN.sendMsgBuf(0x05004804, 1, 8, stmp3);                                       //send message to log in
       delay(10);   
       unsigned char stmp4[8] = {0x14, 0x00, 0x9C, 0x13, 0x9C, 0x13, 0x3E, 0x17};     //this is the command for changing the output voltage 50.2v 14A
       CAN.sendMsgBuf(0x05FF4004, 1, 8, stmp4);                                       //send message to set ouput voltage to all chargers connected to the CAN-bus
      Serial.print("Output Voltage set to : ");
      Serial.println(stmp4[3]*256*0.01+stmp4[2]*0.01);
     
}

void loop()                                                                           // main program (LOOP)
{
    unsigned char len = 0;
    unsigned char buf[8] ;
    if(CAN_MSGAVAIL == CAN.checkReceive())                                            // check if data coming
    {

        CAN.readMsgBuf(&len, buf);                                                    // read data,  len: data length, buf: data buf
          INT32U canId = CAN.getCanId();                                              // read the CAN Id
          Serial.print("0");                                                          // leading zero 
          Serial.print(canId,HEX);                                                    // output CAN Id to serial monitor
          Serial.print("\t");                                                         // send Tab
        for(int i = 0; i<len; i++)                                                    // print the data
        {
            if( buf[i] < 0x10){ Serial.print("0");} Serial.print(buf[i],HEX);         // send a leading zero if only one digit
            Serial.print(" ");                                                        // space to seperate bytes
        }
       Serial.println();
       Serial.print("Temperature = ");
       Serial.println(buf[0]);                                                        //first byte is temperature in celcius
       Serial.print("Current = ");
       Serial.println(buf[2]*256*0.1+buf[1]*0.1);                                     // third (msb) and second byte are current in 0.1A (deciamp) calculated to show directly in Amps
       Serial.print("OutputVoltage = ");
       Serial.println(buf[4]*256*0.01+buf[3]*0.01);                                   // fifth (msb) and fourth byte are voltage in 0.01V (centivolt) calculated to show directly in Volts dc
       Serial.print("OutputPower = ");
       Serial.println((buf[4]*256*0.01+buf[3]*0.01)*(buf[2]*256*0.1+buf[1]*0.1));     // Power is calculated from output voltage and current. Output is in Watts
       Serial.print("InputVoltage = ");          
       Serial.println(buf[5]);                                                        // sixth byte is input voltage in volts ac/dc
//send request for new update

       unsigned char stmp3[8] = {0x15, 0x44, 0x71, 0x02, 0x11, 0x66, 0x00, 0x00};     // *** this is the serial number of the unit
       CAN.sendMsgBuf(0x05004804, 1, 8, stmp3);                                       //send message to request updated figures and keep being 'logged in' or the charger defaults to 53.5 V
       

    }
 

}

/*********************************************************************************************************
  END FILE
*********************************************************************************************************/

Camon   1 mW

1 mW
Posts: 10
Joined: Nov 18 2017 6:31pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by Camon » Oct 17 2018 7:35am

Image
Hayds13 wrote:
Oct 16 2018 11:29pm
Hi Camon,

I've edited your code example with commands I used to set to 50.2v. When I try to set my flatpack to 57v in code, it actually goes to over-volt protection shuts down because it goes much higher.

}[/code]
It works¡¡¡¡¡ wow amazing first I programed to 50.2v and works :O before I programed to maximun value 1680 and it works.
Thank you, thank you so much finally I can do a 4kw charger for mi zero DS.
What is the diference between your code and mine?

Hayds13   100 mW

100 mW
Posts: 40
Joined: Dec 25 2014 12:48pm
Location: Sydney, Australia
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Hayds13 » Oct 17 2018 3:57pm

Awesome Camon! Glad to hear you got it working.

Here are the main difference in code:

unsigned char setdefaultvolt[5] = {0x2B, 0x15, 0x00, 0x44, 0x16}; // (Old) setting the default output voltage
unsigned char setdefaultvolt[5] = {0x29, 0x15, 0x00, 0x9C, 0x13}; // (New) 50.2V
CAN.sendMsgBuf(0x05009C02, 1, 5, setdefaultvolt); // (Old) send message to set output voltage to the CAN-bus
CAN.sendMsgBuf(0x05019C00, 1, 5, setdefaultvolt); // (New) send message to set output voltage to the CAN-bus

User avatar
multifrag   100 W

100 W
Posts: 143
Joined: Feb 19 2016 5:44am
Location: London, UK

Re: ULtra Compact 1800W charger + Eltek programming

Post by multifrag » Oct 21 2018 7:55am

I'm trying to figure out which of the 4 pins on the flatpack S are can L and H. I have flatpack HE working and used this image for pinout, but for flatpack S I can't find a similar image. Closest I could find is this and it looks like Can L and H are suppose to be pins 3 and 4. Just wanted to check if my assumptions are correct.


Edit: Finished soldering it up and yep, my guess was correct. Just need to fit the oled and esp32 inside.

User avatar
eee291   100 kW

100 kW
Posts: 1149
Joined: Nov 05 2015 4:35pm
Location: Austria, Burgenland

Re: ULtra Compact 1800W charger + Eltek programming

Post by eee291 » Oct 26 2018 4:08pm

I found this floating around and thought someone might want this as some kind of documentation at least.
:arrow:
Attachments
Eltek CANbus Protocol.pdf
(114.2 KiB) Downloaded 356 times

pm_dawn   100 W

100 W
Posts: 164
Joined: Jan 17 2009 3:36pm
Location: Östersund, Sweden

Re: ULtra Compact 1800W charger + Eltek programming

Post by pm_dawn » Oct 29 2018 1:53am

Hi eee291 !

That documentation does not apply to the Flatpack2 HE recitfiers but for the EV chargers.
They can be found here:
https://evolveelectrics.com/collections/chargers

The IP21 look very similar to the Flatpack2HE but they have totally different CAN- protocol.

Best REgards
/Per

jean0   1 mW

1 mW
Posts: 10
Joined: May 21 2018 1:24pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by jean0 » Nov 28 2018 7:54am

dakoal wrote:
Oct 10 2018 12:10am
jean0 wrote:
Jun 09 2018 9:17am
Ian, You're great! The bigger is NCP1015 switcher, the smaller is BC817 transistor.
I replace them, hope it will solve my problem...
Thanks a lot, buddy.
Hi,

I have 4 dead Flatpacks, not opened yet.
jean0, did you ever bring the Flatpack2 back to life with the 2 parts?

Best regards
Bernhard

Hi Bernhard,

Sorry for late answer.
I have 2 dead Flatpacks, I couldn't repair the first one, more parts are damaged, so the device is a big short-circuit.
I bought one more FP, but it is crashed/damaged on its way to me, so its semiconductor parts are good, but the transformers are broken. I'd like to make one FP from the two, but hadn't time to complete yet...

Best Regards,
Je@n

jean0   1 mW

1 mW
Posts: 10
Joined: May 21 2018 1:24pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by jean0 » Dec 29 2018 7:37am

Hi,

I've just finished the repair of my one of the 2 FPs.
Now the fan is spinned up, but the red LED is on beside the green and no output voltage.
I can't check the CAN traffic now, but I'm not sure, the CAN connection is necessary for working?
From the manual:
Alarms: Red LED 'on' -> Low mains shutdown, High and low temperature shutdown, Rectifier Failure, Overvoltage
shutdown on output, Fan failure, Low voltage alarm, CAN bus failure

The red LED can be ON for several cases, so I don't know what still the problem...

Best Regards,
Je@n
Last edited by jean0 on Jan 07 2019 7:42am, edited 1 time in total.

jean0   1 mW

1 mW
Posts: 10
Joined: May 21 2018 1:24pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by jean0 » Jan 07 2019 7:41am

Hi,

I could check just now the CAN traffic of the repaired FP2.
Although the output voltage is only 0.36V, the CAN interface is working.
After I logged in, I get this status: 1E 00 00 F6 FE EC 00 1E
The output voltage word seems to be interesting...
FE F6 is incorrect...

If I try to set any voltage, have no success...
:-(

Je@n

Hayds13   100 mW

100 mW
Posts: 40
Joined: Dec 25 2014 12:48pm
Location: Sydney, Australia
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Hayds13 » Jan 07 2019 11:50pm

Hi jean0,
You're getting 0.36v as the DC output? For a 48v unit you should be getting 53.5v as default when connecting AC (with CAN disconnected). Alternately, the unit could be programmed for another default voltage within 43-5v-57.6v.

Some units don't calibrate well, so if the voltage is programmed to the maximum, it may go into over-voltage protection and get the result you've got(?). You could try re-programming the default voltage to something lower.

Sounds like your flatpack is unhappy. Might be easier to buy another...
Best of luck!
Hayden

jean0   1 mW

1 mW
Posts: 10
Joined: May 21 2018 1:24pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by jean0 » Jan 17 2019 2:22am

Hi Hayden,

Unfortunately, every attempt to change the voltage is unsuccesful. :-(
The green and red LED are lit, but interesting, if FP automatically logs out after timeout, the yellow LED also becomes on...
So I don't know if it's software problem or hardware...

Regards,
Je@n

john61ct   100 GW

100 GW
Posts: 8439
Joined: Dec 18 2018 2:06pm

Re: ULtra Compact 1800W charger

Post by john61ct » Apr 09 2019 8:51pm

pm_dawn wrote:
Sep 19 2016 9:39am
I have done a small breakout board for the Flatpack2 and Flatpack2HE
Hi Per.

Have you received your new order yet?

Do they fit in the Flatpack S version too?

pm_dawn   100 W

100 W
Posts: 164
Joined: Jan 17 2009 3:36pm
Location: Östersund, Sweden

Re: ULtra Compact 1800W charger

Post by pm_dawn » Apr 10 2019 1:49am

john61ct wrote:
Apr 09 2019 8:51pm
pm_dawn wrote:
Sep 19 2016 9:39am
I have done a small breakout board for the Flatpack2 and Flatpack2HE
Hi Per.

Have you received your new order yet?

Do they fit in the Flatpack S version too?
Hi !
Yes new boards are in.
50pcs ready for you.

Yes they fit the FP2 S version also.
I programmed a FP2 S unit with the board yesterday.

regards
/Per

User avatar
Doctorbass   100 GW

100 GW
Posts: 7490
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: ULtra Compact 1800W charger + Eltek programming

Post by Doctorbass » Apr 15 2019 1:00am

Remmie,

Any instructions for the Flatpack 2 HE 2000W 110-125Vdc model like on electricmotorcycleforum ?

I tried couple serial number and voltage commands like published here for the 48v models here but i can't get it to change voltage output. I want 116.5Vdc output on one unit of model 125Vdc 2000W HE

Image

I use the IXXAT USB to CAN compact v1.6 with galvanic isolation.

I just want the correct commands lines that can be sent to permanently change the output voltage.

http://electricmotorcycleforum.com/boar ... ic=7407.30

Thanks alot!!
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

J_haggerty   100 mW

100 mW
Posts: 38
Joined: Dec 04 2018 4:41pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by J_haggerty » Apr 23 2019 1:37am

EDIT: Per I don't mean to step on your toes with boards here. As an FYI I ordered a board from Per and it was very good quality and I would recommend them highly. I chose to redesign and tighten up the footprint because the housing pictured below was quite constrained. END EDIT

Would any of you be interested in PCBs for the 1800W Flatpack 2 regular model (not HE)? Not sure if the dimensions are the same but I can post them.

They look like this and can be shipped with or without connectors (for the price of the connectors). AC/CAN Eurostyle headers with a surface mount pad for CAN termination resistor. DC is a 76amp screw terminal by TE Connectivity. I'm ordering our first run and want to gauge interest. Had to reduce the footprint of the board from the guy I originally bought one from (and add connectors).

These boards are spec'd for 240V at full amperage input and output (11A AC in/31A DC Out) This is assuming you're stacking two chargers for a higher DC output.
Screen Shot 2019-04-23 at 2.29.36 AM.png
Screen Shot 2019-04-23 at 2.29.36 AM.png (62.35 KiB) Viewed 2893 times
Screen Shot 2019-04-23 at 2.30.18 AM.png
Screen Shot 2019-04-23 at 2.30.18 AM.png (67.85 KiB) Viewed 2893 times
Additionally, I may be looking to sell enclosures for the flatpack 2 that hold these boards and have a 20 amp C-19 inlet and molex CAN connection like so:
Screen Shot 2019-04-23 at 2.35.06 AM.jpg
Screen Shot 2019-04-23 at 2.35.06 AM.jpg (103.42 KiB) Viewed 2893 times
These are still in prototype and will likely have to be green. Let me know if there's any interest! You all have been a great help.

john61ct   100 GW

100 GW
Posts: 8439
Joined: Dec 18 2018 2:06pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by john61ct » Apr 23 2019 2:00am

yes interested, also for the S

side by side low profile in my case

Able to accommodate the Smartpack where that's desired would be ideal

And always allowing individual per-rectifier AC inputs from separate circuits where limited options are available like campgrounds or friends' houses

J_haggerty   100 mW

100 mW
Posts: 38
Joined: Dec 04 2018 4:41pm

Re: ULtra Compact 1800W charger + Eltek programming

Post by J_haggerty » Apr 23 2019 8:13pm

If you give me dimensions for the smartpack and the S I could probably work something out. The difficulty there will be extra open space around the units. The side by side is definitely doable as are the separate input circuits. The design was originally for two C13 plugs, so 10 amp max per plug and standard equipment for most power supplies and i could swap it back.