Frequenly we need to make a battery by connecting a bunch of smaller batteries together.
If you want a higher voltage, the batteries are connected in SERIES. This means they are connected + to - between cells. The voltage of the individual cells add in this case, but the capacity (amp-hours) stays the same. The maximum current for the string is the same as a single cell also.