I have 2 questions.
First is, from most of my reading, it is recommended to only charge the battery to 80%. The battery maker (em3ev) says to charge to 90% for longer battery life and lower Cut Off to be 43v (52v 23 AH). Is one better then the other and why.
The second is watt/hours & amp hours. I can figure out the total watt hours & amp hours for the battery but how can I figure out what is available to me with a 43v LVC.
Thanks, Tom