Li-PO no balancing, 48 V Electric Bike 4,000 mile experience

Get all your technical information about electric bikes here.
Post Reply
Boyntonstu   10 kW

10 kW
Posts: 549
Joined: Mar 07 2015 8:31pm
Location: Boynton Beach, Florida

Li-PO no balancing, 48 V Electric Bike 4,000 mile experience

Post by Boyntonstu » Jun 20 2017 12:51pm



The Hobby King 6s 5,200's are treated very well and they have lasted a long time without balancing, Slowly charge them with a Constant Voltage charger to just under 4.0 V and discharge to 3.8 V and everything is fine!

User avatar
Ypedal   100 GW

100 GW
Posts: 12528
Joined: Dec 27 2006 12:55pm
Location: Moncton NB, Canada
Contact:

Re: Li-PO no balancing, 48 V Electric Bike 4,000 mile experi

Post by Ypedal » Jun 20 2017 1:04pm

Nice !

I take mine up to 4.15v full average ( nothing over 4.20.. ever.. ) and down to 3.60v ( resting ) and have balance charge once a year at the start of the season ( fully charging to 4.20v with RC charger, all cells .. then go back to bulk charge )

You have to keep an eye on them, every charge cycle, and once one bad cell shows up, take action.. but otherwise, if you get good packs with no DUD cells from the start, they do fine for the super vigilant among us.