Sorry could not find a thread about this motor so created a new one.
I think that this new mxus 3000 motor could be a serious competitor to the Crystalyte 40xx series. People call it Mini Cro
-------------------------------------------------------
Just look at the spec for V1
Nominal: 3000W
Peak: 6500w
Stator/Magnets with: 45mm
4 turn
Stamped steel stator
0.5mm Laminations
Weight: 8Kg Stamped steel stator(8.3Kg with aluminium stator)
135mm dropouts
13AWG phase wires
v2 differences compared to v1:
4Tx16 windings;
Al stator base;
0,35mm laminations;
+300g to weight resulting in 10kg total for motor laced in 26" P35D meety rim with 10G spokes.
------------------------------------------------------------------------------------------------------------------
Added from "teslanv"
Here is some more Hard data for the EE folks:
MXUS XF40-45H (3000W) DD Hub motors...
21X3T Winding
Phase resistance = 0.072 Ohms
RPM at 50.2V = 597, 11.89 Kv
1.78A/89.4 Watts No Load
16X4T Winding
Phase resistance = 0.110 Ohms
RPM at 50.2V = 448.2, 8.93 Kv
1.08A/54.2 Watts No Load
12X5T Winding
Phase resistance = 0.163 Ohms
RPM at 50.2V = 359, 7.15 Kv
0.84A/42.2 Watts No Load
10X6T Winding
Phase resistance = 0.225 Ohms
RPM at 50.2V = 299.4, 5.96 Kv
0.64A/32.1 Watts No Load
All bare hub motors weigh in at right around 9.14 Kg.
These are the motors I sent to Justin for Dyno Testing.
No Load Current was measured with my Fluke 77 iii RMS Digital Multimeter, so it should be pretty darn accurate.
-----------------------------------------------------------------------------------------------------------------------------------------
Mxus V2 4t@13kW 160A DC/400A phase
Stock phase wires: