I've just ordered one. I'll follow up again once I get it, should be the end of December. In my research I found the exact same frame is used by a number of western resellers, retailing at 2-3 times the price.
So far, I've found Dengfu to be surprisingly communicative and pleasant to work with. They made some tweaks to the components for whatever reasons, upgraded the rear shock to a RS Deluxe.
With that all said, I'm not walking into this blind. I used paypal with an Amex card. I've not had a lot of fun in the past making claims through paypal but vendors are usually shit scared if you mention contacting them, they don't want to get shut down. Amex on the other hand will refund a claim in days with the right paperwork.
My biggest concern next is the shipping, I'm pretty sure the packaging is going to be sub-standard. I went with sea, it was another $150 for air and I'm not in a rush. This is the build out I went with
Item Description Quantity Unit price(usd) Amount(usd)
1 E06 20" in UD matt finish, 12*197mm rear space (rear thru axle included) 1 $2,999.00 $2,999.00
2 Neco headset for E06 1
3 BAFANG M620 G510 1000W 48V 1
4 DENGFU Lithium-ion 48V 14Ah 672Wh 1
5 Suspension fork, air, 120mm travel, 1 1/8"-1 1/2" steer tube, 135x9 QR 1
6 RS DLX R 185X50 DB 2T MM TS B1 1
7 SRAM RD-SX EAGLE/ SRAM CS-PG-1210 EAGLE 11-50T 12S/ SRAM DB LVL/ SRAM SL-SX EAGLE TRIGGER/ BAFANG EB11 170mm 40T/ SRAM CN-SX EAGLE 12S/ 180mm disc 1
8 Aluminum Alloy, 80mm wide, fat hubs, 6-bolt, 135x9 front, 197x12 rear, DT spokes, 32/32 holes, all black (INNOVA 26er*4.0 tire) 1
9 ZOOM, suspension seat post, 31.6mm diameter, 100mm drop 1
10 HB006 handlebar 720mm in 3k matt finish 1
11 aluminum stem 1
12 normal black saddle 1
13 postage to USA by sea 1 $500.00 $500.00