DIY Toroidal Axial Flux PM
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
DIY Toroidal Axial Flux PM
Hello ES community,
I have lurked this site here and there, but really got hooked reading APL's DIY axial flux bike motor build, and it inspired me to make my own post.
viewtopic.php?f=30&t=97860
It's a hell of a thread and I learned a lot and about motors and the community while reading through it all. It's clear that there are people out there in this world with a similar passion to mine, and luckily it sounds like you guys are all way smarter than I. So I welcome the discussion and ideas. While I proceed down a similar journey to APL's
Let me start with some background. I am a software engineer, with background in computer technology. Physics and math were always an interest of mine, but I was not proficient in either. I find that I learn best by doing and getting my hands dirty. I also am fascinated by magnets and their potential application throughout advanced technologies. Another interest of mine is renewable energy, which is where the fascination with the motors piqued.
I love the idea of combining renewable technologies, and in a northern US climate, solar is only so viable. have read a bunch of articles and papers on turbines, and the axial flux diy-er community. Which is what led me to try to make a light weight generator that could be cheaply manufactured, and the neat thing about these generators, is that they are motors too! Therefore I decided a side project of mine would to to electrify my Honda PCX 125.
Now that seems like a lofty goal. It's a 8.5KW ICE engine. Obviously it wouldn't need that kind of power if it was fully electric, and I will need to start smaller, but I felt that it was attainable with enough effort. Especially if a hub motor was a reality, and I could put one on each wheel.
I have been working at this project for a bit over a year, with slow-ish progress with life getting in the way through out. When I had started, I was living in an apartment with very little space, and I didn't have any real tools. I had comprised a very rudimentary rig using K'nex, superglue, and some time. After a while I felt like I had a decent grasp on how this whole induction thing worked, so I bought a 3d printer and started learning a 3d modeling. My thought was that it was the most versatile tool and great for rapid prototyping. I made a few coil cores and toroidal stators, but it wasn't long and my wife didn't like all the room I was taking up soooo, I bought a house.
I would like to dump some photos with out making this initial post too long, but I have so much I would like to talk about from litz wire winding machine that I created to the benefits of FOC type ESCs and how they may work with a coreless toroidal form factor.
Anyway, look forward to more posts!
My YouTube Channel
https://www.youtube.com/channel/UCQk0Ck ... QvpGxj4kxw
the Genesis a CD with a bunch of magnets superglued to it. Super safe!
Made it a bit nicer with some aluminum sheets and amore coils. Also a 3d printed rotor that a buddy of mine made before I had my printer. That's when it got a bit more real: Until I felt good about it: But that was really just a heater. So I tried again. this one spun! I was on to something. so I took my learnings and made a bigger "better" one. And then it blew up. Wish I recorded that it was pretty wild. I never found some of the chunks of the rotor. They seem to have disintegrated. this I believe was due to only one rotor half being on. (for a test), but what I didn't think about is that the KV was at least double that of a dual rotor, also the two halves helped support each other, but with one on it is much more susceptible to vibration. it was a bad idea, lets just leave it at that. I then made a nicer version of that same one that I don't seem to have photos of, but I have a video of it here (details in description of video):
I have lurked this site here and there, but really got hooked reading APL's DIY axial flux bike motor build, and it inspired me to make my own post.
viewtopic.php?f=30&t=97860
It's a hell of a thread and I learned a lot and about motors and the community while reading through it all. It's clear that there are people out there in this world with a similar passion to mine, and luckily it sounds like you guys are all way smarter than I. So I welcome the discussion and ideas. While I proceed down a similar journey to APL's
Let me start with some background. I am a software engineer, with background in computer technology. Physics and math were always an interest of mine, but I was not proficient in either. I find that I learn best by doing and getting my hands dirty. I also am fascinated by magnets and their potential application throughout advanced technologies. Another interest of mine is renewable energy, which is where the fascination with the motors piqued.
I love the idea of combining renewable technologies, and in a northern US climate, solar is only so viable. have read a bunch of articles and papers on turbines, and the axial flux diy-er community. Which is what led me to try to make a light weight generator that could be cheaply manufactured, and the neat thing about these generators, is that they are motors too! Therefore I decided a side project of mine would to to electrify my Honda PCX 125.
Now that seems like a lofty goal. It's a 8.5KW ICE engine. Obviously it wouldn't need that kind of power if it was fully electric, and I will need to start smaller, but I felt that it was attainable with enough effort. Especially if a hub motor was a reality, and I could put one on each wheel.
I have been working at this project for a bit over a year, with slow-ish progress with life getting in the way through out. When I had started, I was living in an apartment with very little space, and I didn't have any real tools. I had comprised a very rudimentary rig using K'nex, superglue, and some time. After a while I felt like I had a decent grasp on how this whole induction thing worked, so I bought a 3d printer and started learning a 3d modeling. My thought was that it was the most versatile tool and great for rapid prototyping. I made a few coil cores and toroidal stators, but it wasn't long and my wife didn't like all the room I was taking up soooo, I bought a house.
I would like to dump some photos with out making this initial post too long, but I have so much I would like to talk about from litz wire winding machine that I created to the benefits of FOC type ESCs and how they may work with a coreless toroidal form factor.
Anyway, look forward to more posts!
My YouTube Channel
https://www.youtube.com/channel/UCQk0Ck ... QvpGxj4kxw
the Genesis a CD with a bunch of magnets superglued to it. Super safe!
Made it a bit nicer with some aluminum sheets and amore coils. Also a 3d printed rotor that a buddy of mine made before I had my printer. That's when it got a bit more real: Until I felt good about it: But that was really just a heater. So I tried again. this one spun! I was on to something. so I took my learnings and made a bigger "better" one. And then it blew up. Wish I recorded that it was pretty wild. I never found some of the chunks of the rotor. They seem to have disintegrated. this I believe was due to only one rotor half being on. (for a test), but what I didn't think about is that the KV was at least double that of a dual rotor, also the two halves helped support each other, but with one on it is much more susceptible to vibration. it was a bad idea, lets just leave it at that. I then made a nicer version of that same one that I don't seem to have photos of, but I have a video of it here (details in description of video):
Last edited by HalbachHero on Apr 13 2021 1:25pm, edited 1 time in total.
Re: DIY Toroidal Axial Flux PM
This is brilliant. I love it.
How much scope is there for flattening the stator while keeping the same amount of copper? If you can get the magnets close enough to have the flux linking between them i think the mag field gets stronger and better aligned.
Wondering how much torque you can get out of it... Whether it's mountable on an ebikes.
If you've read APL's thread, try Lebowski axial flux, he did coreless as well, and it appeared it worked fairly well.
I love that this packages so neatly.
The obvious hassle of adding iron to the core is that suddenly your magnets want to stick to the core and everything has to be much much stronger to resist the magnets pull.
How much scope is there for flattening the stator while keeping the same amount of copper? If you can get the magnets close enough to have the flux linking between them i think the mag field gets stronger and better aligned.
Wondering how much torque you can get out of it... Whether it's mountable on an ebikes.
If you've read APL's thread, try Lebowski axial flux, he did coreless as well, and it appeared it worked fairly well.
I love that this packages so neatly.
The obvious hassle of adding iron to the core is that suddenly your magnets want to stick to the core and everything has to be much much stronger to resist the magnets pull.
Hold my beer while I divide by zero 

- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Thank you for your interest. I think it packages nicely as well, and it's fairly simple to print 5 pieces in total. The version in the video is pretty thin as there are only 4 turns per slot, but the more turns the thicker it needs to be due to the wires crossing over, therefore the newer version is about 25mm thick. The difference in the pull of the magnets from rotor to rotor is significant. I can tell that its much weaker now that its further apart.
This is the conundrum I have been facing, and seems like the tradeoff, either get stronger, heavier, bigger magnets or make the stator thinner. I cannot find a clever way of adding turns but keeping it thin without adding significantly to end turns and ultimately the diameter of everything.
I worry that adding iron to the core has a greater impact than cogging and tolerance issues though. I fear that the form factor will not work the same as currently induction is direct to the coil where as with iron, my understanding is that its to guide the flux into a path where it can be optimally inducted. My concern given the stator shape is that the flux would be pulled into multiple phases at once.
Thoughts?
This is the conundrum I have been facing, and seems like the tradeoff, either get stronger, heavier, bigger magnets or make the stator thinner. I cannot find a clever way of adding turns but keeping it thin without adding significantly to end turns and ultimately the diameter of everything.
I worry that adding iron to the core has a greater impact than cogging and tolerance issues though. I fear that the form factor will not work the same as currently induction is direct to the coil where as with iron, my understanding is that its to guide the flux into a path where it can be optimally inducted. My concern given the stator shape is that the flux would be pulled into multiple phases at once.
Thoughts?
Re: DIY Toroidal Axial Flux PM
Super awesome thread HalbachHero! My hat goes off to your tenacity and ingenuity,.. which is what it takes to do this
DIY stuff. Lots of sleepless nights, he, he...
Now I can see what your up to, great pics, and I can see that the trail of tears has been long and hard. I love the 3D
printing aspect of you're build, and we haven't really explored that too much here on the ES. I can see a lot of potential
there, and it can only get better with the advent of newer materials coming all the time.
From what I've seen so far on core-less axial's, is the gaps between magnets seem to hoover around 13mm or so,
(memory), but it's dependent on strength like you say, and adding steel will only get us more axial problems, with the
'pay off' ratio still being reletivly unknown. Ive always wondered about the hybrid aspect, half coreless, half cored.
A thinner stator comes down to materials strength, and bigger magnets add weight and expense which are unnecessary if
the stator is thinner. Lots of conundrums with motors,.. bigger diameter amplifies the torque, but also amplifies the
strength problems.
Well, thats what were here for, to thread the needle and find a solution. I see that your using lots of Litz type wire in your
experiments, which is very nice stuff, but have you thought about single strand as a way to maybe get a thinner stator?
How much current/voltage are you using these days?
DIY stuff. Lots of sleepless nights, he, he...

Now I can see what your up to, great pics, and I can see that the trail of tears has been long and hard. I love the 3D
printing aspect of you're build, and we haven't really explored that too much here on the ES. I can see a lot of potential
there, and it can only get better with the advent of newer materials coming all the time.

From what I've seen so far on core-less axial's, is the gaps between magnets seem to hoover around 13mm or so,
(memory), but it's dependent on strength like you say, and adding steel will only get us more axial problems, with the
'pay off' ratio still being reletivly unknown. Ive always wondered about the hybrid aspect, half coreless, half cored.
A thinner stator comes down to materials strength, and bigger magnets add weight and expense which are unnecessary if
the stator is thinner. Lots of conundrums with motors,.. bigger diameter amplifies the torque, but also amplifies the
strength problems.
Well, thats what were here for, to thread the needle and find a solution. I see that your using lots of Litz type wire in your
experiments, which is very nice stuff, but have you thought about single strand as a way to maybe get a thinner stator?
How much current/voltage are you using these days?
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Thanks APL,
The rotors I have constructed are using halbach arrays. In that photo you can see that there are thin magnets placed on their side to prevent some flux leakage, while minimizing extra weight. However, their is still a decent amount of flux leaking through the back of the rotor. I am considering including a iron backing with a halbach. though that might not be the best power to weight choice.
Weirder is that the axial facing magnets are N52 1/2" x 1/4" x 1/8" and the ones on their side are N50 1/2" x 1/8" 1/16". which probably has something to do with flux leakage.
The litz wire is homebrew. I have created a winding machine with a combination of K'nex and 3D printed parts. Here's a video of it in action.
The rotors I have constructed are using halbach arrays. In that photo you can see that there are thin magnets placed on their side to prevent some flux leakage, while minimizing extra weight. However, their is still a decent amount of flux leaking through the back of the rotor. I am considering including a iron backing with a halbach. though that might not be the best power to weight choice.
Weirder is that the axial facing magnets are N52 1/2" x 1/4" x 1/8" and the ones on their side are N50 1/2" x 1/8" 1/16". which probably has something to do with flux leakage.
The litz wire is homebrew. I have created a winding machine with a combination of K'nex and 3D printed parts. Here's a video of it in action.
Re: DIY Toroidal Axial Flux PM
To have the halbach array work properly your would probably need shaped magnets. The gaps will leak a lot of flux. See the FEA done in this thread: viewtopic.php?f=30&t=46476&hilit=Axial+flux
Wire can take a lot more current than those charts say. That's based on very conservative values for wiring up machines etc where voltage drops are important, for your motor the heating effect is the only real limit so you can probably pass far more current.
I'd just flatten the ends of as much as possible. I'm not even sure half the plastic is needed in your last stator.
Wire can take a lot more current than those charts say. That's based on very conservative values for wiring up machines etc where voltage drops are important, for your motor the heating effect is the only real limit so you can probably pass far more current.
I'd just flatten the ends of as much as possible. I'm not even sure half the plastic is needed in your last stator.
Last edited by mxlemming on Apr 15 2021 5:38pm, edited 1 time in total.
Hold my beer while I divide by zero 

Re: DIY Toroidal Axial Flux PM
Possibly your halbach magnets should be much wider, try to keep the gap between the rotor less than the gaps between the magnets?
Love the knex winding machine.
Love the knex winding machine.
Hold my beer while I divide by zero 

- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
I want to also go into a little more detail of what I have tried so far. Initially I was using PLA just to really simply test things. Not only was I new to making motors, but also 3d printing. So I had no real idea of what tolerances were possible especially with the printer I bought, a hobbyist level printer. I was also new to 3D modeling, so the ramp up process was slow as there was just a lot to take in.
Anyway, eventually I made some of the stators that were in the previous photos, I tried using angled stator legs and straight, and I tried angling the magnets and straight magnets. While angling the magnets I think makes for complicated flux paths, it also makes it so you cant fit as many magnets and not have overlap as they pass over each phase. Therefore, I just went with straight.
This worked well, so I experimented with iron backing. I understood enough to know that I was going to direct the flux but I would have to give up structural integrity, and would produce some eddy currents. This actually worked quite well in my "Mk1" motor. it had horribly tolerances, but I just went for it anyway because I was excited, and it got hot enough that it fused itself together because the plastic melted.
So I sort of abandoned the iron backing and tried the halbach array and immediately had success, and could feel the difference on the sides of the rotors, so I knew it was doing something, and while I never calculated the weight savings (other parameters changed since then too), I imagine it was reasonable given the rest of it was mostly plastic and copper.
Once I had the pretty much the tightest possible arrangement of magnets given the 12 pole pair count I wanted (24 poles, 48 individual magnets due to halbach), I only made some changes to support a ring in the middle instead of standoffs attached to one rotor and a groove for the ring to sit in on each rotor half. This helps seat the ring. There are still 2mm standoffs at 5 points where its "keyed" just to have a solid way to transfer rotational energy without shifting.
Once I was happy with the rotors, I moved to the stator and tried to optimize that. The format I went with was 3 Phase 12 "Teeth"
per phase so 36 in total. I practiced winding on stators with small amounts of purchased litz wire since it was expensive. and found that the amount of twist in the wire is important to prevent it from getting loose as you go. This proved to be exhausting on the hands to do more than one phase at a time (at first it took like 20 minutes per phase). Holding the wire tightly and having to twist it over and over sucked.
Thus spawned the litz wire machine. I figured I could just spin a bunch of spools. of course, it was a bit more complex. and I ended up with a few iterations of that before I have what I have now, but now it nicely twists 20 strands into a small 3d printed spool. Which is small enough to fit through the center of the stator, and has enough wire for at least 1 phase. ( you can fit 2 but its tight, and theres no real point that I can see). Great, now I am drowning in litz
I tried twisting strands of litz together, 2 and 4 strands of 20/32 on different attempts, The downside to this is having to cut the litz to length, twist it up then solder the ends together. That proved to be a pain in the butt (before I had my solder pot). After that I tried just doing laps. I would do one phase at a time. This is what I have found to be the most pain free. The Mk1 had two strands of litz wired simultaneously. (Ill add it goes on neater this way, but the soldering after it messier, and a pain (without that solder pot, see what im getting at?)). The Mk2 had 4 laps of a single litz wire strand. and so did Mk3.
Mk2 and 3 were great super thin, the whole motor is like 13mm thick, and weighs 300g or something close. Mk2 exploded because im dumb and spun it with one rotor half with the same voltage, and it didn't last long. Like only a few couple seconds long. Mk3 was a replica, and survived a few stress tests. in the "hardest" stress test I ran it at 100W load for 10 minutes continuously and it survived, the temperature on the coils was 38C after. Albeit, it has a propeller on it that may have cooled it a bit, but eventually on another test, it got too warm, and a magnet was pulled out of place, and the stator started to drag on it.
And that brings us to now. I then decided to go bigger with the stator. I wanted 10 laps, or turns. so I made it a bit thicker to 15mm, after a many small tweaks and reprints I got something I liked. So I wound it up and put it on the rotor halves. but there was an issue. I didn't compensate for the height change in the stator in regard to the hub. Damn... its already epoxied together. No worries, I modified the rotor design and added a stand off on the shaft collar. for the stator to sit on. This was actually a blessing in disguise, because it also solved another issue, which was a very weak shaft collar on the rotor, due to plastic and what-not. I added some braces and it seems to have helped. Also fixing an issue with the printer resolved some layer adhesion issues I was facing. Great now it fit, but theres another issue with the printer. Because it was printing like crap, I messed up all the settings, so when I fixed it (New bowden tube, new hot end, new nozzle, replaced corroded wiring, etc). I was printing with different tolerances. I was over extruding. So nothing fit. Well I'm impatient so I thought Ill just smack it with this hammer till it goes in. Its tight but cant be that tight (I've had to hammer in the stator some iterations). Anyway, it was too tight, and everything broke. So. I needed to beef up the stator now.
The stator was held to the hub by 12 little 2mm nubs. this was working (sorta) for a while. But they did break or print badly quite a few times. So they had to go. I ended up going with a new design that I have yet to play with much, but it should receive up to 12 M2 screws. which will go into threaded heat insets in the stator hub. this way I can replace those two parts independently, and its a bit thicker, so hopefully it can take a bit more abuse. I think I need to make more litz wire, but I have enough for at least 2 phases, so I can see how winding goes with the new form factor. But I'm also waiting on some M2 screws and heat set inserts to show up in the mail, so that I can test fit the stator to the new hub design.
Let me know what you all think!
Anyway, eventually I made some of the stators that were in the previous photos, I tried using angled stator legs and straight, and I tried angling the magnets and straight magnets. While angling the magnets I think makes for complicated flux paths, it also makes it so you cant fit as many magnets and not have overlap as they pass over each phase. Therefore, I just went with straight.
This worked well, so I experimented with iron backing. I understood enough to know that I was going to direct the flux but I would have to give up structural integrity, and would produce some eddy currents. This actually worked quite well in my "Mk1" motor. it had horribly tolerances, but I just went for it anyway because I was excited, and it got hot enough that it fused itself together because the plastic melted.
So I sort of abandoned the iron backing and tried the halbach array and immediately had success, and could feel the difference on the sides of the rotors, so I knew it was doing something, and while I never calculated the weight savings (other parameters changed since then too), I imagine it was reasonable given the rest of it was mostly plastic and copper.
Once I had the pretty much the tightest possible arrangement of magnets given the 12 pole pair count I wanted (24 poles, 48 individual magnets due to halbach), I only made some changes to support a ring in the middle instead of standoffs attached to one rotor and a groove for the ring to sit in on each rotor half. This helps seat the ring. There are still 2mm standoffs at 5 points where its "keyed" just to have a solid way to transfer rotational energy without shifting.
Once I was happy with the rotors, I moved to the stator and tried to optimize that. The format I went with was 3 Phase 12 "Teeth"
per phase so 36 in total. I practiced winding on stators with small amounts of purchased litz wire since it was expensive. and found that the amount of twist in the wire is important to prevent it from getting loose as you go. This proved to be exhausting on the hands to do more than one phase at a time (at first it took like 20 minutes per phase). Holding the wire tightly and having to twist it over and over sucked.
Thus spawned the litz wire machine. I figured I could just spin a bunch of spools. of course, it was a bit more complex. and I ended up with a few iterations of that before I have what I have now, but now it nicely twists 20 strands into a small 3d printed spool. Which is small enough to fit through the center of the stator, and has enough wire for at least 1 phase. ( you can fit 2 but its tight, and theres no real point that I can see). Great, now I am drowning in litz
I tried twisting strands of litz together, 2 and 4 strands of 20/32 on different attempts, The downside to this is having to cut the litz to length, twist it up then solder the ends together. That proved to be a pain in the butt (before I had my solder pot). After that I tried just doing laps. I would do one phase at a time. This is what I have found to be the most pain free. The Mk1 had two strands of litz wired simultaneously. (Ill add it goes on neater this way, but the soldering after it messier, and a pain (without that solder pot, see what im getting at?)). The Mk2 had 4 laps of a single litz wire strand. and so did Mk3.
Mk2 and 3 were great super thin, the whole motor is like 13mm thick, and weighs 300g or something close. Mk2 exploded because im dumb and spun it with one rotor half with the same voltage, and it didn't last long. Like only a few couple seconds long. Mk3 was a replica, and survived a few stress tests. in the "hardest" stress test I ran it at 100W load for 10 minutes continuously and it survived, the temperature on the coils was 38C after. Albeit, it has a propeller on it that may have cooled it a bit, but eventually on another test, it got too warm, and a magnet was pulled out of place, and the stator started to drag on it.
And that brings us to now. I then decided to go bigger with the stator. I wanted 10 laps, or turns. so I made it a bit thicker to 15mm, after a many small tweaks and reprints I got something I liked. So I wound it up and put it on the rotor halves. but there was an issue. I didn't compensate for the height change in the stator in regard to the hub. Damn... its already epoxied together. No worries, I modified the rotor design and added a stand off on the shaft collar. for the stator to sit on. This was actually a blessing in disguise, because it also solved another issue, which was a very weak shaft collar on the rotor, due to plastic and what-not. I added some braces and it seems to have helped. Also fixing an issue with the printer resolved some layer adhesion issues I was facing. Great now it fit, but theres another issue with the printer. Because it was printing like crap, I messed up all the settings, so when I fixed it (New bowden tube, new hot end, new nozzle, replaced corroded wiring, etc). I was printing with different tolerances. I was over extruding. So nothing fit. Well I'm impatient so I thought Ill just smack it with this hammer till it goes in. Its tight but cant be that tight (I've had to hammer in the stator some iterations). Anyway, it was too tight, and everything broke. So. I needed to beef up the stator now.
The stator was held to the hub by 12 little 2mm nubs. this was working (sorta) for a while. But they did break or print badly quite a few times. So they had to go. I ended up going with a new design that I have yet to play with much, but it should receive up to 12 M2 screws. which will go into threaded heat insets in the stator hub. this way I can replace those two parts independently, and its a bit thicker, so hopefully it can take a bit more abuse. I think I need to make more litz wire, but I have enough for at least 2 phases, so I can see how winding goes with the new form factor. But I'm also waiting on some M2 screws and heat set inserts to show up in the mail, so that I can test fit the stator to the new hub design.
Let me know what you all think!
Re: DIY Toroidal Axial Flux PM
I would
1) consider doing an inrunner, then the screws could be on the outside where side is less constrained
2) make the wire guides as thin as possible, then you can make them lower for the same wire fill.
3) if the ends start to get large, you can always cut a channel in the rotor?
What are you modeling in? CAD wise? Your shapes are moderately advanced for any of the open source CAD packages.
1) consider doing an inrunner, then the screws could be on the outside where side is less constrained
2) make the wire guides as thin as possible, then you can make them lower for the same wire fill.
3) if the ends start to get large, you can always cut a channel in the rotor?
What are you modeling in? CAD wise? Your shapes are moderately advanced for any of the open source CAD packages.
Hold my beer while I divide by zero 

-
- Posts: 86
- Joined: Dec 07 2016 7:01am
Re: DIY Toroidal Axial Flux PM
Your corelless statosr are looking really good !
Happy to see someone else inspired by Ben katz axial flux build, I've been following APL's build also for quite some time and find it really inpiring.
Since you presented yourself I might do the same : I did mechanical engineering studies and started working as an electrotechnical engineer 5 month ago (I was just a lot in electromechanical stuff at the time last year reading all the posts in the Motor Technology section).
Since I'm also working on coreless axial design I will be happy to share my understanding and advancement on your thread if possible or start my own thread if needed too.
I've build a really small test motor some month ago to validate my findings, here are some pictures of it :

Happy to see someone else inspired by Ben katz axial flux build, I've been following APL's build also for quite some time and find it really inpiring.
Since you presented yourself I might do the same : I did mechanical engineering studies and started working as an electrotechnical engineer 5 month ago (I was just a lot in electromechanical stuff at the time last year reading all the posts in the Motor Technology section).
Since I'm also working on coreless axial design I will be happy to share my understanding and advancement on your thread if possible or start my own thread if needed too.
I've build a really small test motor some month ago to validate my findings, here are some pictures of it :
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
mxlemming,
Great thoughts. Here are just some counter thoughts as these have crossed my mind already.
Thecoco974,
Thanks for sharing. It's awesome to know there are others like myself out in the world, and I'm certainly getting some Ben Katz vibes from your motor there. Looks very nice, and seems to spin up and down nicely. Looks like a pretty high Kv assuming that was an RPM readout in your video. What is the diameter of your full size version. It looks very close to mine (120mm). Do you know what you are designing for yet? I'd love to see where it ends up. I would encourage you to post about your endeavor. It's fun.
Also, that video you shared. I'm the third comment from the top haha. I watched that video several times, and modeled my motor quite closely after his.
Can I also assume the airgap you mention is rotor to rotor, and not rotor to stator?
Also can you elaborate on what you mean by winding it straight. I am using litz specifically for its benefits in reducing eddy currents at high frequencies, and with a 36 slot stator, I thought that was enough to merit the use of litz. but also there is the added benefit of being pretty easy to work with.
Thanks for the thoughts!
Great thoughts. Here are just some counter thoughts as these have crossed my mind already.
I could do an in runner. However, I had thought that I could swap the ring out for a something that included mounting to have a direct drive attached directly to the motor. But the in runner concept is looking more and more attractive as I deal with very small parts on the inner diameter.1) consider doing an inrunner, then the screws could be on the outside where side is less constrained
currently the guides coincide with the magnet width quite nicely, and as soon as I make the grooves flat, the subsequent laps of wire are difficult to hold into position. With the current architecture, I can pull the wire as hard as I want and it just tightens up, I haven't broken a stator once that way yet, which is a nice feature for getting things nice and tight.2) make the wire guides as thin as possible, then you can make them lower for the same wire fill.
This I had not thought of, but I'm not sure of it's feasibility, as the overhang is already quite flexible on one rotor, and making that any bigger is asking for clipping under load. I am dealing with millimeter tolerances pretty much everywhere at this point.3) if the ends start to get large, you can always cut a channel in the rotor?
Thecoco974,
Thanks for sharing. It's awesome to know there are others like myself out in the world, and I'm certainly getting some Ben Katz vibes from your motor there. Looks very nice, and seems to spin up and down nicely. Looks like a pretty high Kv assuming that was an RPM readout in your video. What is the diameter of your full size version. It looks very close to mine (120mm). Do you know what you are designing for yet? I'd love to see where it ends up. I would encourage you to post about your endeavor. It's fun.
Also, that video you shared. I'm the third comment from the top haha. I watched that video several times, and modeled my motor quite closely after his.
Can I also assume the airgap you mention is rotor to rotor, and not rotor to stator?
Also can you elaborate on what you mean by winding it straight. I am using litz specifically for its benefits in reducing eddy currents at high frequencies, and with a 36 slot stator, I thought that was enough to merit the use of litz. but also there is the added benefit of being pretty easy to work with.
Thanks for the thoughts!
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Thecoco974,
Perhaps its minor, and/or a complete misunderstanding but does back EMF not find its way into the back iron?Why do you think rotor back iron add eddy current ? To my understanding eddy current are created when a conductive material is exposed to variating magnetic flux, in the case of the rotor back iron magnet flux is fixed and coil field is also fixed in the rotor frame, am i missing something ?
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Also mxlemming,
I am using Fusion 360What are you modeling in? CAD wise? Your shapes are moderately advanced for any of the open source CAD packages
-
- Posts: 86
- Joined: Dec 07 2016 7:01am
Re: DIY Toroidal Axial Flux PM
I see why you're doing that, winding is quite a pain, but i agree with mxlemming on this, spreading the winding over the full electric revolution decrease KV because all turns will not contibute the same (I think thay might contribute sinusoidally) but the flux increase will more than make up for. Should be interesting to model it.HalbachHero wrote: ↑Apr 13 2021 6:35pmcurrently the guides coincide with the magnet width quite nicely, and as soon as I make the grooves flat, the subsequent laps of wire are difficult to hold into position. With the current architecture, I can pull the wire as hard as I want and it just tightens up, I haven't broken a stator once that way yet, which is a nice feature for getting things nice and tight.
Yes it is rpm. The KV is really high because of the thin and weak magnets and the increase airgap I got. Full scale stator to magnet clearance was supposed to be 1mm, scaling 4 times down mean 0.25 mm, not really dooable with my craftings skills. Also the full scale one is design to spin fast at 8-9Krpm at 55V, scalling down the diameter means also dividing by 4 the BEMF (linear with magnet speed) and multiplying by 4 the KV also.HalbachHero wrote: ↑Apr 13 2021 6:35pmLooks like a pretty high Kv assuming that was an RPM readout in your video. What is the diameter of your full size version. It looks very close to mine (120mm). Do you know what you are designing for yet? I'd love to see where it ends up. I would encourage you to post about your endeavor. It's fun.
I still need to check if my sims results where correct though ...
The full scale version have changed since then, I'm now looking for a three stator inrunner with a 167.5mm magnet end to magnet end rotor diameter (so since going inrunner the motor diameter will be 195mm). I'm really ambitious about it but i'm looking for 5kw continuous and 10kW for 1min. I might start a thread about it in the next few days.
Just saw your commentHalbachHero wrote: ↑Apr 13 2021 6:35pmAlso, that video you shared. I'm the third comment from the top haha. I watched that video several times, and modeled my motor quite closely after his.


So have you done some FEM simulation of you're motor design ? I'm interested by the flux in the airgap you're achieving with the hallback array.
Yes of course rotor to rotor ! being aircored everything betwen magnets is airgap for me.HalbachHero wrote: ↑Apr 13 2021 6:35pmCan I also assume the airgap you mention is rotor to rotor, and not rotor to stator?
Winding the litzwire without twisting it first, I know it's not litwire anymore but for our use case (reducing eddy current on the winding) the twisting isn't needed. winding it straight will also marginally reduce the turn length and resistance. I think we only need the multiple strand enamebled small diameter copper wire part of the litz wire, not the fancy twisting (for my build i'm planning 700 strands of 0.1mm parralleled per turn).HalbachHero wrote: ↑Apr 13 2021 6:35pmAlso can you elaborate on what you mean by winding it straight. I am using litz specifically for its benefits in reducing eddy currents at high frequencies, and with a 36 slot stator, I thought that was enough to merit the use of litz. but also there is the added benefit of being pretty easy to work with.
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
That's the beauty of these axial flux motors, lots of power in a small package. I'd love to see how it turns out.I'm really ambitious about it but i'm looking for 5kw continuous and 10kW for 1min
No I haven't I haven't spent the time to learn that yet. Though I feel it could be really helpful with understanding the complex flux lines, it's something I will have to put some time into. But, likewise. I am very curious what this sort of halbach array looks like in FEMMSo have you done some FEM simulation of you're motor design ? I'm interested by the flux in the airgap you're achieving with the hallback array.
The twisted litz wire is certainly easier to manage and turn, but I get what you two are saying now. I will already have some twisted litz, but I have just about run out. For the next spools I wind, I'll not twist it up.
I'll make two stators and compare how many turns I can fit on the two given the same stator and assuming I can fit more turns. I'll modify the stator design to be much thinner with thinner wire guides.
I suspect I will need to find a creative way to hold the wires flat in their place while I wind each phase. Maybe I can make a jig.
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Okay, well I think you guys were right. I decided to just try the untwisted litz just to see if I could fit more. I have to say its a nicer looking coil in the end. Much neater, and thin, and clean on the outer diameter of everything. But it was a pain in the butt to wind. I'm going to need to make a jig to help with that.
But dang doesn't that look sexy? The issues I see now are, since I beefed up the supports in the middle they kind of get in the way of winding the phase that touches it. Also, keeping the wire in its slot while winding is a bit more of a challenge. Thinking of making a modification to the stator design to facilitate that. But also the wire is going to overlap the other phases. I make the whole stator shorter, that will be less of an issue but still a bit of a problem. Might need to find a way to wind all 3 phases at once....
The photos make it clear too that there is more room between those teeth. I stopped at 10 turns which is what my last one was with the twisted litz. I think I can fit a few more. I will keep playing with that and see what's possible.
But dang doesn't that look sexy? The issues I see now are, since I beefed up the supports in the middle they kind of get in the way of winding the phase that touches it. Also, keeping the wire in its slot while winding is a bit more of a challenge. Thinking of making a modification to the stator design to facilitate that. But also the wire is going to overlap the other phases. I make the whole stator shorter, that will be less of an issue but still a bit of a problem. Might need to find a way to wind all 3 phases at once....
The photos make it clear too that there is more room between those teeth. I stopped at 10 turns which is what my last one was with the twisted litz. I think I can fit a few more. I will keep playing with that and see what's possible.
Re: DIY Toroidal Axial Flux PM
Thanks for sharing your builds here.
I have been looking at axial style motors for a ebike build that's churring away in my head and this is all amazing info.
A questions regarding size/weight to power. The motor I want needs to put out about 300w nominal and I'd like to pair it with a cycloidal drive for it's reduction. Battery would be 52V. Do you a rough idea on the size / weight of this style axial motor that would hit this 300w 5k RPM 52V spec?
I have been looking at axial style motors for a ebike build that's churring away in my head and this is all amazing info.
A questions regarding size/weight to power. The motor I want needs to put out about 300w nominal and I'd like to pair it with a cycloidal drive for it's reduction. Battery would be 52V. Do you a rough idea on the size / weight of this style axial motor that would hit this 300w 5k RPM 52V spec?
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Shirk,
It's difficult to say without some real thought. But a 52V @ 5k RPM will give you a Kv of ~96. 300W @ 52V is only 6A without losses. This means you could get away with pretty small conductors, and likely small magnets in a pretty small form factor. But the power to weight ratio is really achieved through very small tolerances and minimization of losses. The ability to fabricate one is also really important. You can only make things so small, and so close together. Another important thing to consider is materials. Composites and some metals like titanium are great for strength to weight, but are difficult to source or just expensive. Cheaper materials come at the price of weight and size. Everything is a balance.
Also, specifically axial flux motors benefit from having a large diameter, as they can produce exponentially more torque the further away from the center of the hub. This can mean big power. 300W is not a LOT of power, and there are many very lightweight brushless outrunners that can achieve 300W and are very cheap and widely available. I feel that axial flux really shows its worth in high power applications.
Now if you're talking about a 3Kw motor, that may be a better application for a geared down axial flux hub motor
It's difficult to say without some real thought. But a 52V @ 5k RPM will give you a Kv of ~96. 300W @ 52V is only 6A without losses. This means you could get away with pretty small conductors, and likely small magnets in a pretty small form factor. But the power to weight ratio is really achieved through very small tolerances and minimization of losses. The ability to fabricate one is also really important. You can only make things so small, and so close together. Another important thing to consider is materials. Composites and some metals like titanium are great for strength to weight, but are difficult to source or just expensive. Cheaper materials come at the price of weight and size. Everything is a balance.
Also, specifically axial flux motors benefit from having a large diameter, as they can produce exponentially more torque the further away from the center of the hub. This can mean big power. 300W is not a LOT of power, and there are many very lightweight brushless outrunners that can achieve 300W and are very cheap and widely available. I feel that axial flux really shows its worth in high power applications.
Now if you're talking about a 3Kw motor, that may be a better application for a geared down axial flux hub motor
Last edited by HalbachHero on Apr 15 2021 6:56am, edited 2 times in total.
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
I was able to get 12 wraps around the same stator slot without it becoming a huge pain. I worry what its going to take to wind the next version as things get thinner and more fragile. I have started redesigning the stator. The connections on the inner diameter are no longer sufficient, There is now very little material to grab on to, and the copper will want to take that up. Hmmm, looks like an inrunner going forward.
I really liked the outrunner, it was clean, but so be it if it works better.
I squished everything to 9mm and changed the shape of the slot to better facilitate winding. but I will likely need to make that a bit thicker. I have leaned on the suggestion of 11mm air gap assuming I will be able to have 1mm tolerances between the rotor and stator.
The cool thing is, at 9mm I am back to the thickness of my Mk2 which only had 4 turns. So thats cool (if this works).
I would love to bring the Kv down in a linear fashion given the number of turns, and I think that's only possible if I keep the thickness and airgap the same.
Any suggestions on how to mount this stator on the outside? I do worry the copper is going to be difficult to work around with it this thin.

I squished everything to 9mm and changed the shape of the slot to better facilitate winding. but I will likely need to make that a bit thicker. I have leaned on the suggestion of 11mm air gap assuming I will be able to have 1mm tolerances between the rotor and stator.
The cool thing is, at 9mm I am back to the thickness of my Mk2 which only had 4 turns. So thats cool (if this works).
I would love to bring the Kv down in a linear fashion given the number of turns, and I think that's only possible if I keep the thickness and airgap the same.
Any suggestions on how to mount this stator on the outside? I do worry the copper is going to be difficult to work around with it this thin.
-
- Posts: 86
- Joined: Dec 07 2016 7:01am
Re: DIY Toroidal Axial Flux PM
I just did some quick sims of the arrangment you use layed flat as others did for axial FEM analysis :HalbachHero wrote: ↑Apr 14 2021 7:48amNo I haven't I haven't spent the time to learn that yet. Though I feel it could be really helpful with understanding the complex flux lines, it's something I will have to put some time into. But, likewise. I am very curious what this sort of halbach array looks like in FEMM
Flux line results : here is the flux at the midline : I Thought there were too much leakage flux so i did the same without insert magnet : and with back iron for base line evaluation of hallback efficiency at redirecting flux on one side : So I think the insert magnet may be to thin and add litle to the flux (if my sims are correct). Plus side if I am you might decrease the KV working on that too.
Holy shit youre fast working on this ! And it look really good for sure

If you're keeping the wire on its spool can you make one turn by one turn all phase at once like you said ? might be a pain and need a holder of some sort.HalbachHero wrote: ↑Apr 14 2021 10:55amBut also the wire is going to overlap the other phases. I make the whole stator shorter, that will be less of an issue but still a bit of a problem. Might need to find a way to wind all 3 phases at once....
HalbachHero wrote: ↑Apr 14 2021 2:37pmI was able to get 12 wraps around the same stator slot without it becoming a huge pain.

I d'ont know if you're reusing wire for each evolution, but the simpler thing to do (not the cleanest for sure) might be to epoxy a center mounting ring directly to the inner winding like i did in my small scale build.HalbachHero wrote: ↑Apr 14 2021 2:37pmThere is now very little material to grab on to, and the copper will want to take that up. Hmmm, looks like an inrunner going forward. I really liked the outrunner, it was clean, but so be it if it works better.
Yes it's the best way, I think you'll need to sacrifice copper section for KV.HalbachHero wrote: ↑Apr 14 2021 2:37pmI would love to bring the Kv down in a linear fashion given the number of turns, and I think that's only possible if I keep the thickness and airgap the same.
It's more dificult to deal with because of end turn (tha's another reason why i'm folowing Ben Katz on the no end turn winding), but if going outrunner you can make it wider on the outside without making the rotor weaker (since it's already floating) and it might give you more mounting optionsHalbachHero wrote: ↑Apr 14 2021 2:37pmAny suggestions on how to mount this stator on the outside? I do worry the copper is going to be difficult to work around with it this thin.
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
Thecoco974,
Woah! thank you so much for doing that. That is very helpful. Now I am very curious how close it would have to be to prevent flux leaking, and seeing the difference between the back iron and not is cool, though it complicates how to make this with a printer a bit. I also wonder if on the inner diameter since its basically touching, if flux isn't leaked. Also, what airgap did you use in your simulation? was that with the 11mm?
Wonder if I can jam more magnets in there if I get rid of the halbach ones.... food for thought
I might be able to turn all three phases at once, but I think its going to prove to be a challenge, without a good groove or twisted wires, its wants to go everywhere. I printed a test stator based on my model change and wound 2 laps. While the trough (that's what I'm gonna call the female side of the wire guide thing.) is nearly the same cross sectional area that the other stator, due to the larger width the wires have more of a chance to run at an angle, which takes up some precious extra space. Will keep going with this test to see how many laps I can fit.
Also I made a tool, which I think could be helpful.
Woah! thank you so much for doing that. That is very helpful. Now I am very curious how close it would have to be to prevent flux leaking, and seeing the difference between the back iron and not is cool, though it complicates how to make this with a printer a bit. I also wonder if on the inner diameter since its basically touching, if flux isn't leaked. Also, what airgap did you use in your simulation? was that with the 11mm?
Wonder if I can jam more magnets in there if I get rid of the halbach ones.... food for thought
I might be able to turn all three phases at once, but I think its going to prove to be a challenge, without a good groove or twisted wires, its wants to go everywhere. I printed a test stator based on my model change and wound 2 laps. While the trough (that's what I'm gonna call the female side of the wire guide thing.) is nearly the same cross sectional area that the other stator, due to the larger width the wires have more of a chance to run at an angle, which takes up some precious extra space. Will keep going with this test to see how many laps I can fit.
Also I made a tool, which I think could be helpful.
I have a concern with material strength if I make the stator a larger diameter. Since one of the rotors have no support on the inner diameter. The 6mm of plastic likes to flex already. My goal is to keep this as this as possible, so I don't really want to add any more overhang or thickness if I don't have to. If it makes more sense to go in runner. I will, but it won't look at good I don't thinkIt's more dificult to deal with because of end turn (tha's another reason why i'm folowing Ben Katz on the no end turn winding), but if going outrunner you can make it wider on the outside without making the rotor weaker (since it's already floating) and it might give you more mounting options
Re: DIY Toroidal Axial Flux PM
I think for this you should get higher power density with an inrunner, since the outer shell takes up a lot of volume, being on the outside and all... the middle is generally pretty empty so you have a lot of space for bearings, flanges and whatnot.
Getting tabs to add screws on the outside of the stator should be far far easier than the tabs you previously put in the middle, again because the circumference increases, so there is just generally more space on the outside.
You could use a solid steel disc for your magnet backing, just drill a single hole (exactly...) in the middle. or, if you are really cheaping it/bodging away, I just checked my bike disc brake rotors and found they are made from highly magnetic steel. That's a circle that can sustain a lot of force and RPM.
This is looking pretty cool! I can really get behind this, since the costs involved are super low, I have a 3d printer and piles of ESCs to energise it with
I also have a solidworks licence, so I can model away.
Any idea what the BEMF profile of it looks like? You have an oscilloscope?
Getting tabs to add screws on the outside of the stator should be far far easier than the tabs you previously put in the middle, again because the circumference increases, so there is just generally more space on the outside.
You could use a solid steel disc for your magnet backing, just drill a single hole (exactly...) in the middle. or, if you are really cheaping it/bodging away, I just checked my bike disc brake rotors and found they are made from highly magnetic steel. That's a circle that can sustain a lot of force and RPM.

This is looking pretty cool! I can really get behind this, since the costs involved are super low, I have a 3d printer and piles of ESCs to energise it with

Any idea what the BEMF profile of it looks like? You have an oscilloscope?
What are you doing this FEA with? Is it some open source thing I can play with? Or is it some mega expensive thing you get through work/uni/...?Thecoco974 wrote: ↑Apr 15 2021 2:25pmI just did some quick sims of the arrangment you use layed flat as others did for axial FEM analysis :
Hold my beer while I divide by zero 

Re: DIY Toroidal Axial Flux PM
You guys must drink a lot of coffee,.. I have trouble just keeping up with this thread!
I guess I'm not really sure what your having trouble with, on the wire moving or not staying put, but it's common for
motors to use string to help hold coils together. Theres a fabric fishing line thats supper strong and mega-thin that
wouldn't take any space,.. might work well for that, and it super glues well. Just a thought.

I guess I'm not really sure what your having trouble with, on the wire moving or not staying put, but it's common for
motors to use string to help hold coils together. Theres a fabric fishing line thats supper strong and mega-thin that
wouldn't take any space,.. might work well for that, and it super glues well. Just a thought.
- amberwolf 100 GW
- Posts: 33669
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: DIY Toroidal Axial Flux PM
If you found this advice helpful, supporting contributions are accepted here.
Beginning of a New Life
Give a listen to my music!
(More here, including experimental).
Beginning of a New Life
Give a listen to my music!
(More here, including experimental).
- HalbachHero 100 W
- Posts: 209
- Joined: Apr 05 2021 8:35pm
Re: DIY Toroidal Axial Flux PM
mxlemming,
Thanks!
I will keep playing with the stator a bit more to see what I can fit, but you're totally right bring the mass to the middle as much as possible. If you can move the mounting points to the middle as well, then you isolate the mass that is on the outside to only what needs to be there.
I am considering making the same style supports I had on the inner diameter since it allows for support on the top and bottom but still allowing for easy winding.
I bought some large diameter washers initially, which ended up in the Mk1, but were working with a larger diameter now. I worry about making my own, because they will have to be very well balanced. But will definitely give it a shot when I get there.
I believe strongly in renewable technology and would love for others to be able to use this as a generator in a wind turbine. I will definitely make the STLs available once the design is solid. (or now if someone wants them)
I do not have an oscilloscope. That would be really helpful to visualize the waveform.
FEMM is a free program for Windows. I think it runs in Wine too
https://www.femm.info/wiki/Download
Amberwolf,
Thanks for sharing, that is a handy resource. Bookmarked!
Thanks!
I will keep playing with the stator a bit more to see what I can fit, but you're totally right bring the mass to the middle as much as possible. If you can move the mounting points to the middle as well, then you isolate the mass that is on the outside to only what needs to be there.
I am considering making the same style supports I had on the inner diameter since it allows for support on the top and bottom but still allowing for easy winding.
I bought some large diameter washers initially, which ended up in the Mk1, but were working with a larger diameter now. I worry about making my own, because they will have to be very well balanced. But will definitely give it a shot when I get there.
I believe strongly in renewable technology and would love for others to be able to use this as a generator in a wind turbine. I will definitely make the STLs available once the design is solid. (or now if someone wants them)
I do not have an oscilloscope. That would be really helpful to visualize the waveform.
FEMM is a free program for Windows. I think it runs in Wine too
https://www.femm.info/wiki/Download
The issue with this is that I am doing laps around the whole toroid with a single phase. So I wouldn't be able to tie it until I was done all the laps. And it wants to fall apart in the process of winding it. I just have to pull everything super tight, and the thinner this gets the more difficult that becomes. However a change to the stator again may help allow for tying it at the end. But I may rather go with a high heat epoxy to keep everything solid at the end, which would likely make tying things unnecessary. We will have to find out what works best.I guess I'm not really sure what your having trouble with, on the wire moving or not staying put, but it's common for
motors to use string to help hold coils together. Theres a fabric fishing line thats supper strong and mega-thin that
wouldn't take any space,.. might work well for that, and it super glues well. Just a thought.
Amberwolf,