Electric Motors and Controllers
-
BalorNG 1 kW

- Posts: 343
- Joined: Nov 10 2019 7:22pm
Post
by BalorNG » Nov 25 2021 9:10am
mxlemming wrote: ↑Nov 25 2021 8:43am
Phase amps is the correct way to rate a controller.
With 100 battery amps you can generate pretty much any amount of phase amps. Currently on my test bench I'm generating 270 phase amps from 17A battery at 24V.
Battery amps has no useful meaning.
Not exactly true if you are running very high phase resistance motors like typical ebike motors

But I agree that you should look at phase amps first and how long the controller can sustain THEM.
-
mxlemming 10 kW

- Posts: 866
- Joined: Jul 17 2020 7:56am
Post
by mxlemming » Nov 25 2021 11:18am
BalorNG wrote: ↑Nov 25 2021 9:10am
mxlemming wrote: ↑Nov 25 2021 8:43am
Phase amps is the correct way to rate a controller.
With 100 battery amps you can generate pretty much any amount of phase amps. Currently on my test bench I'm generating 270 phase amps from 17A battery at 24V.
Battery amps has no useful meaning.
Not exactly true if you are running very high phase resistance motors like typical ebike motors

But I agree that you should look at phase amps first and how long the controller can sustain THEM.
Ummm .. yes it really is true.
At very low speed you can equate power in to I^2R losses.
100A battery at 72V is 7.2kW
For a typical crappy hub motor, phase resistance is less than 100mohm; phase to phase 200mohm. That gives a current of about 190A.
But that's a hub motor that would melt with a small fraction of that power. Scale to a qs205 with 0.065 ohm phase to phase and you're at 330A... Scale that to the motor on my desk with 10mohm phase to phase and you got 850A and a fireball.
Hold my beer while I divide by zero

-
john61ct 100 GW

- Posts: 8438
- Joined: Dec 18 2018 2:06pm
Post
by john61ct » Nov 25 2021 11:29am
OP states the unit can handle 7000W?
My point is not that Flipsky "should not" give us at least a ballpark phase amps spec.
But so far they haven't,and that is the reality we need to deal with.
I am sure over time some range will be revealed by the tech-savvy early adopters
along with all the other IRL data points we'd like to see
and then those holding off purchasing due to insufficient information will feel more comfortable
-
BalorNG 1 kW

- Posts: 343
- Joined: Nov 10 2019 7:22pm
Post
by BalorNG » Nov 25 2021 12:00pm
john61ct wrote: ↑Nov 25 2021 11:29am
OP states the unit can handle 7000W?
My point is not that Flipsky "should not" give us at least a ballpark phase amps spec.
But so far they haven't,and that is the reality we need to deal with.
I am sure over time some range will be revealed by the tech-savvy early adopters
along with all the other IRL data points we'd like to see
and then those holding off purchasing due to insufficient information will feel more comfortable
...
They did, this is 120A and this is basically package limit an firware limit. Maybe you can hack it, but the legs will basically act as fuses

Not the worst that can happen, btw.
-
atkforever 10 W

- Posts: 83
- Joined: Sep 25 2019 2:17pm
Post
by atkforever » Nov 25 2021 12:05pm
But since we know the fets are 120amps package limited, max phase amps should be 120A or did I miss something?
Can we Say that Current flowing in phase A motor wise, is equal to current flowing between the legs of the mosfets ON related to phase A?
-
john61ct 100 GW

- Posts: 8438
- Joined: Dec 18 2018 2:06pm
Post
by john61ct » Nov 25 2021 1:47pm
BalorNG wrote:They did, this is 120A and this is basically package limit an firware limit.
Ah so I missed that.
100A battery maximum
120A phase maximum
Is that correct? At this point definitive as the vendor rating?
-
BalorNG 1 kW

- Posts: 343
- Joined: Nov 10 2019 7:22pm
Post
by BalorNG » Nov 25 2021 2:39pm
john61ct wrote: ↑Nov 25 2021 1:47pm
BalorNG wrote:They did, this is 120A and this is basically package limit an firware limit.
Ah so I missed that.
100A battery maximum
120A phase maximum
Is that correct? At this point definitive as the vendor rating?
YES, this IS vendor rating:
https://flipsky.net/collections/electro ... controller
-
MorbidlyObeseKoala 100 W

- Posts: 100
- Joined: Apr 06 2018 3:53pm
Post
by MorbidlyObeseKoala » Nov 29 2021 9:58am
Is there an agreement that an antispark switch needs to be used with one of these controllers as well?
Is that switch pre-charging the controller as well as limiting sparks at the connection?
I have a dc solar circuit breaker I was using as a main switch that was keeping sparks away from my connection at the battery. They seem a little expensive for simply spark reduction considering they have no other protections (no circuit breaking for high amps, no built in temperature protection, no reverse polarity protection)
-
Chito 10 mW

- Posts: 26
- Joined: Oct 18 2019 12:45pm
Post
by Chito » Dec 05 2021 11:08am
-
mxlemming 10 kW

- Posts: 866
- Joined: Jul 17 2020 7:56am
Post
by mxlemming » Dec 05 2021 11:44am
What happened at 3m30? Looks like the BMS cut out?
This seems like a lot of power for such a small box.
Hold my beer while I divide by zero

-
Chito 10 mW

- Posts: 26
- Joined: Oct 18 2019 12:45pm
Post
by Chito » Dec 05 2021 4:04pm
mxlemming wrote: ↑Dec 05 2021 11:44am
What happened at 3m30? Looks like the BMS cut out?
This seems like a lot of power for such a small box.
It is the bms that had it set to cut at 80a. then when i got home i turned it up to 95a
-
Woly 10 mW

- Posts: 32
- Joined: Nov 16 2020 10:32pm
Post
by Woly » Dec 05 2021 4:49pm
And if its the motor temp is correct, running at 80+ too much will kill the magnets.
-
afzal 10 W

- Posts: 74
- Joined: Jun 13 2021 7:55am
- Location: Kerala, India
Post
by afzal » Dec 06 2021 5:05am
john61ct wrote: ↑Dec 05 2021 4:32pm
Negative motor temp?
Probably temp sensor is not connected to VESC
-
Chito 10 mW

- Posts: 26
- Joined: Oct 18 2019 12:45pm
Post
by Chito » Dec 06 2021 11:11am
afzal wrote: ↑Dec 06 2021 5:05am
john61ct wrote: ↑Dec 05 2021 4:32pm
Negative motor temp?
Probably temp sensor is not connected to VESC
exact, sensor is not connected
-
atkforever 10 W

- Posts: 83
- Joined: Sep 25 2019 2:17pm
Post
by atkforever » Dec 06 2021 5:23pm
I like the way fets cool from 70degrees to 50 within few seconds. May I Ask you where you live?
What's the limit regarding temp ?
It looks like 120A Can be held for almost a minute, I'm pretty amazed about this little box. Definitely killing kt controllers or any "cheap" ebike controller.
-
Chito 10 mW

- Posts: 26
- Joined: Oct 18 2019 12:45pm
Post
by Chito » Dec 09 2021 1:33am
Spain.
Cools fast because it has an improved heat sink
-
zombiess 1 GW

- Posts: 3046
- Joined: Feb 01 2011 2:16am
- Location: Ventura
Post
by zombiess » Dec 09 2021 3:59am
I wonder how much safety margin is available at 98% duty cycle. What is the switching frequency set to? The time to switch on / off can vary quite a bit under real world conditions cycle to cycle and change at different operating temperatures and vary between parts. It's pretty easy to get runt pulses or get some shoot through due to not enough dead time. The amount required also varies with the switching frequency since the time needed is fixed. Lower switching frequencies can allow for more power delivery, but they also stress the caps more.
I dislike the misleading spec of stating it will do 100A continuous even though it only has 12 guage leads. I managed to desolder some 8 gauge XT150 connectors at 100A sustained for only 20 mins, the wire was toasty. Also, XT150 connectors being rated for 150 Amps...LOL... NO!
Fundamentals United, Inc.
CISSP Certified
-
msim 1 µW

- Posts: 4
- Joined: Jul 18 2019 3:06pm
Post
by msim » Dec 09 2021 8:28pm
I am new to Vesc as well and I am having a tough time getting mine to run correctly. It does well under no load but as soon as I encounter a hill it comes to a dead stop as if no current. Flipsky has not been much help so far they say it looks like a current roll off but have not suggested a fix. I have battery amps set to 50 and motor amps to 65. The motor is an HM CX72v4500w dual phase wires. I am running it at 16s on a 50a bms. I understand that some motors present problems for the vesc. But I am wondering if there is something I am missing that may resolve this issue. I used Vest tool 3.0 for mac to program the flipsky. Vesc tool 3.1 would not launch the ADC wizard for connecting the throttle. I understand the firmware is not supposed to be updated is there anything I can do or is this a motor compatibility issue . Thanks in advance
-
john61ct 100 GW

- Posts: 8438
- Joined: Dec 18 2018 2:06pm
Post
by john61ct » Dec 09 2021 9:21pm
likely the battery, not enough oomph
-
juancargarcia84 1 µW

- Posts: 2
- Joined: Dec 09 2021 4:25am
Post
by juancargarcia84 » Dec 13 2021 5:30pm
Hello. I have bought this same controller for my son's 1600w electric motorcycle. In previous projects he had used brushed motor controllers, in which with a simple switch it was turned off and on without problems.
Now I see that you are talking about non-sparking switches, and I do not understand why you have to use them. From what I read I deduce that these vesc-based controllers cannot be turned off if it is not by cutting the power from the battery, and that is where sparks are produced. Is that correct?
If someone can clarify that I would appreciate it.
Thanks
-
atkforever 10 W

- Posts: 83
- Joined: Sep 25 2019 2:17pm
Post
by atkforever » Dec 13 2021 6:19pm
There are capacitors inside the controller and when you plug it to the battery the caps charge quickly Hence a high current in the connector for few millisecondes which results in sparks.
For "tiny" controllers such as this one an antispark Switch (which basically precharges the circuit via a resistor) is optionnal as it won't Fry the circuit, but for bigger controllers it's mandatory since they have bigger caps.
I have a Kelly controller, 72v 130amps, and I was quite worried about not using a Switch because it was required on the wiring diagram so I wrote to the technical service they replied it's okay without it'll just wear the connector over time.
I've Never Heard about vesc beeing killed when plugging the battery...
Correct me if I'm wrong.
-
mxlemming 10 kW

- Posts: 866
- Joined: Jul 17 2020 7:56am
Post
by mxlemming » Dec 14 2021 7:45am
It's quite possible to get substantial overshoot on the Vbus rail of the board when you first plug in due to the inductive nature of the cables.
The extent to which this is a problem depends on a number of things
1) length and loop area of the cables
2) Resistance of cables
3) nature of the input capacitors (big problem if only ceramics, the series resistance of electrolytic caps danois the effect)
Whether it damages the system is another question. Normally the MOS will survive since they're all off at turn on time and so the Vbus withstand is 2x the MOS rating.
The DCDC converters can be much more sensitive.
I've killed some lm5017 100Vdcdc converters by hot swapping 65V on a board with only ceramics. Scoping the input voltage at plug in showed a substantial overshoot.
With 1500uF of electrolytic caps the effect was much diminished, but the connector starts to take a beating.
This is quite application specific. Your mileage may vary.
Another tip... If you're going to hot swap connectors, make the ground connect first, battery+ after. When braking the connection do the opposite. This avoids dumping the inrush through whatever else is connected and partially grounded or not.
Hold my beer while I divide by zero

-
juancargarcia84 1 µW

- Posts: 2
- Joined: Dec 09 2021 4:25am
Post
by juancargarcia84 » Dec 14 2021 5:24pm
Thanks for the help. These types of drivers are new to me.
Although there is one thing that I still do not understand. Once you connect them to the battery, the only way to turn them off is to disconnect them?
If it is not going to be used for a week for example, what should I do? I can put a switch on the adc signal wire to avoid accidental acceleration, but will the controller still draw some current?
-
mxlemming 10 kW

- Posts: 866
- Joined: Jul 17 2020 7:56am
Post
by mxlemming » Dec 14 2021 6:50pm
My VESC controllers draw about 1.2W at idle, so do the math for how long that'll last with your battery.
My guess is leaving it plugged in for a week isn't desirable.
Hold my beer while I divide by zero