Hello everyone!
I am here to assess the need for the welder I made.
I developed it for the production of our batteries and it has proven itself so far. I made it because I couldn’t find a similar one anywhere at an affordable price. Our machine is an everlast EX210, but it can be used with practically any machine with advanced digital control.
You can see the test welding in the attached pictures. 100% of the welds are perfect, there is no such thing as spot welding to be visually okay, but poor adhesion.
Used regularly for spot welding of 0.2 - 0.4mm copper plate.
Specifications:
- gas-cooled head
- up to 150A continuous welding current
- 1.6mm tungsten
- 3m gas and power cable
- weldable copper thickness up to 1 mm with a current of 150A
- can be used by hand, pressing on the surface of the copper
- can be clamped in an industrial robot (this is how we use it) and in an XY coordinate machine.
Contents of the package:
- A piece of TIG torch
- 3m gas and power cable
- 1.6mm tungsten suitable for copper
The package does not include:
- electrical and gas connections (all machines are different)
Price: 200 € + delivery and VAT
Thanks.
---------------------------------------------------------
Reference pictures below
![Screenshot 2021-06-24 at 0.39.29.jpg Screenshot 2021-06-24 at 0.39.29.jpg](https://endless-sphere.com/sphere/data/attachments/167/167819-33c5d1cba9ce81f129bfb0e670b73d6d.jpg)
![Screenshot 2021-06-24 at 0.39.06.jpg Screenshot 2021-06-24 at 0.39.06.jpg](https://endless-sphere.com/sphere/data/attachments/167/167821-c20763ba6913d97bf0ad6dc9e0658842.jpg)
![Screenshot 2021-06-24 at 0.39.18.png Screenshot 2021-06-24 at 0.39.18.png](https://endless-sphere.com/sphere/data/attachments/167/167818-bafc3ad3e307ebd20dd1da49bd36511d.jpg)
![Screenshot 2021-06-24 at 0.39.44.jpg Screenshot 2021-06-24 at 0.39.44.jpg](https://endless-sphere.com/sphere/data/attachments/167/167820-a08247e3e42cfbf84bdca3060e51334d.jpg)
---------------------------------------------------------
I am here to assess the need for the welder I made.
I developed it for the production of our batteries and it has proven itself so far. I made it because I couldn’t find a similar one anywhere at an affordable price. Our machine is an everlast EX210, but it can be used with practically any machine with advanced digital control.
You can see the test welding in the attached pictures. 100% of the welds are perfect, there is no such thing as spot welding to be visually okay, but poor adhesion.
Used regularly for spot welding of 0.2 - 0.4mm copper plate.
Specifications:
- gas-cooled head
- up to 150A continuous welding current
- 1.6mm tungsten
- 3m gas and power cable
- weldable copper thickness up to 1 mm with a current of 150A
- can be used by hand, pressing on the surface of the copper
- can be clamped in an industrial robot (this is how we use it) and in an XY coordinate machine.
Contents of the package:
- A piece of TIG torch
- 3m gas and power cable
- 1.6mm tungsten suitable for copper
The package does not include:
- electrical and gas connections (all machines are different)
Price: 200 € + delivery and VAT
Thanks.
---------------------------------------------------------
Reference pictures below
![Screenshot 2021-06-24 at 0.39.29.jpg Screenshot 2021-06-24 at 0.39.29.jpg](https://endless-sphere.com/sphere/data/attachments/167/167819-33c5d1cba9ce81f129bfb0e670b73d6d.jpg)
![Screenshot 2021-06-24 at 0.39.06.jpg Screenshot 2021-06-24 at 0.39.06.jpg](https://endless-sphere.com/sphere/data/attachments/167/167821-c20763ba6913d97bf0ad6dc9e0658842.jpg)
![Screenshot 2021-06-24 at 0.39.18.png Screenshot 2021-06-24 at 0.39.18.png](https://endless-sphere.com/sphere/data/attachments/167/167818-bafc3ad3e307ebd20dd1da49bd36511d.jpg)
![Screenshot 2021-06-24 at 0.39.44.jpg Screenshot 2021-06-24 at 0.39.44.jpg](https://endless-sphere.com/sphere/data/attachments/167/167820-a08247e3e42cfbf84bdca3060e51334d.jpg)
---------------------------------------------------------