104 BCD
Made of 2mm stainless steel.

Because having 5 pieces milled was not much more expensive than just one :D

I cut the shim/guide to make it fit (I cut the chainguide part of so it's only a shim now). The shim is on the right side and the spider is on the left (with the original setup the other way around)

I'm using this 36T chainring.
https://nl.aliexpress.com/item/32833995257.html?spm=a2g0o.order_list.0.0.21ef79d2EnOcwm&gatewayAdapt=glo2nld

I have 3 more for sale.
€35 each excl. shipping from the Netherlands Europe.

So nice to stay warm when pedaling in winter at 60+ km/h :bigthumb: