Assembled Hi-Power LiPo battery packs - any interest?

Place for dealers to post items for sale.
Rube   100 W

100 W
Posts: 255
Joined: Jun 25 2016 10:18pm
Location: Brisbane, Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Rube » Nov 07 2018 4:54am

Congratulations Chris, really cool is a huge understatement. I've followed your work, and the research and development to produce this as a viable product deserves its own paper. Massive respect for pushing the envelope to adapt LiPo to such an unforgiving Australian climate. I can only imagine the hours of research and development it took to deliver such an elegant solution. Super cool :es: :lowbatt: :bigthumb:
Might see you this weekend. :D

Toby82   100 mW

100 mW
Posts: 38
Joined: Oct 13 2010 5:26am
Location: Newcastle, Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Toby82 » Nov 07 2018 5:47am

Hey Chris,

New liquid cooled packs look great.

What's even better is the dimensions are perfect for my build.😁

Be great if I was not on the other side of the continent so I could drop past for a chat and to check out your work.

Cheers

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Nov 07 2018 6:17am

Toby - we can compromise - come to Brisbane for the AEVA conference and Expo! Brisbane is just up the road (in West Australian terms) :mrgreen:

User avatar
Doctorbass   100 GW

100 GW
Posts: 7442
Joined: Apr 08 2007 2:24am
Location: Quebec, Canada East
Contact:

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Doctorbass » Nov 07 2018 1:44pm

Hmm I see power here!!!

Properly installed/used copper buss, excellent current share, great thermal management, well protected cells, AWSOME WORK :wink:

Doc
CURRENT PROJECT: 2WD duo MXUS/Max-E ebike 32kW
http://endless-sphere.com/forums/viewto ... =3&t=65764
-Fastest speed record 117 km/h on flat
-Fastest 1/4 mile@ 114km/h on flat and 16.316 sec
-Succeded to haul a 19200 pounds schoolbus!
113kmh Gianthttp://www.evalbum.com/3406
Mongoosehttp://www.evalbum.com/1947
YOUTUBE---https://m.youtube.com/user/Doctorbasss
http://twitter.com/DocbassMelancon
I speak FRENCH and english

User avatar
Samd   1.21 GW

1.21 GW
Posts: 3750
Joined: Jun 28 2011 11:08pm
Location: Ballarat, AU
Contact:

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Samd » Nov 07 2018 8:36pm

Awesome work Jonesy.
http://ballaratebikes.com/

ImageImageImage
"Knowledge is knowing that a tomato is a fruit. Wisdom is knowing that a 165mm rear shock can't deliver 220mm of rear swingarm travel." - Oprah Winfrey.

User avatar
Danny Mayes   1 kW

1 kW
Posts: 320
Joined: Feb 16 2011 10:17pm
Location: Perth, Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Danny Mayes » Nov 25 2018 3:40am

Very ambitious battery Chris. I love it.

Cool to see the cells glued in with thermal epoxy and the cooling base looks rad.

D

Frank   100 W

100 W
Posts: 227
Joined: Dec 10 2007 11:57am
Location: Maine/Nova Scotia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Frank » Nov 25 2018 1:06pm

Nice looking pack Chris. Very nice. Have you had a chance to grab any Delta-T under-load data yet ? i.e. top of pouch versus heat sink? My limited experience with pre-heating indicates the cell innards conduct heat fairly well. Great idea BTW, you could also circulate warmed coolant on chilly days. :thumb:
Frank

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Nov 25 2018 7:57pm

Frank - hope to get that data this week. I've been busy with other stuff, but hope to get some numbers soon.
I have a test rig where I measure inlet and outlet temperatures, as well as cell top temperatures. The thermal conductivity in that plane is very good (it's like 50% copper and aluminium through there).

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Dec 08 2018 7:11am

Just some pictures of the Prelude battery coming together:
4 done and a spare.jpg
4 done and a spare.jpg (220.67 KiB) Viewed 3716 times

Volts   10 W

10 W
Posts: 68
Joined: Feb 12 2013 8:13am

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Volts » Dec 27 2018 10:54am

These things are works of art dude good job, my only thing is why the hell would you do all that work only to run lipos with a 5c rating when there are single cells out there with 50c rating?

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Dec 30 2018 7:24am

Volts wrote:
Dec 27 2018 10:54am
These things are works of art dude good job, my only thing is why the hell would you do all that work only to run lipos with a 5c rating when there are single cells out there with 50c rating?
Specific energy. These 5C cells are over 208 Wh/kg at 1C, so using 18650 testing regimes they are well over 220 Wh/kg.
This gives a vehicle which will never exceed 2C discharge a range of about 160 km on the highway, and probably 190 km around town.

The 30C/60C cells I have for the race bike are only about 158 Wh/kg at 1C. So it's all about range.

User avatar
Arlo1   100 GW

100 GW
Posts: 8401
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Arlo1 » Dec 30 2018 12:11pm

jonescg wrote:
Dec 08 2018 7:11am
Just some pictures of the Prelude battery coming together:
4 done and a spare.jpg
Very nice man, Did you cycle each cell to weed out the duds?
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Dec 30 2018 7:59pm

Hey Arlin,
I didn't cycle each one, but I do check voltage and DCIR. If a cell was below 3.80 volts I left it out, and likewise if the DCIR was above 15 mOhm I put it aside. Most of them fell a few milliohms either side of 8 mOhm.
I hope to finally get around to thermal testing it this week, but the car itself has been keeping me busy. Just cut the back seat divots out of the car yesterday and will be welding up the subframe today.

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Dec 31 2018 3:50am

So I decided to set up the test rig for measuring heat removal with the liquid cooling plate.
I borrowed a few parts from work, including the PC cooling pump and radiator. However, the thermocouples are not giving satisfactory readings through the multimeters, so unfortunately I will have to borrow the datalogger from work too.
Cooling system test rig.jpg
All set up to deliver a 150 amp (6.6 kW) discharge. In the car, this would equate to about 53 kW, which is pretty close to maximum power from the inverter, but we might be surprised.

At least the datalogger can manage 8 separate thermocouple channels so I will put a few on the top side of the battery as well.

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Dec 31 2018 6:23am



Hehe, so it turns out it's a 330 amp discharge, which is almost 5C. Considering how they don't sag a huge amount, I reckon that's pretty good. At worst this pack will see 2C continuous, for about 2 minutes or so.

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Jan 10 2019 9:04pm

I finally got around to testing the cooling system on this battery module. To be honest I'm disappointed, but it's not all bad. Let me explain.

First up, this is a 4.4 C discharge on a cell which is nominally 1-2 C and 5 C burst - so I'm fairly hammering it. At 330 amps, the busbar linking the two half modules is not rated for this sort of continuous rate (neither are the cells, but that's not what I was testing).

Secondly, the cells were still warm from the day - they have a specific heat capacity of about 2000 J/kg.K so they retain heat fairly well. The cooling loop was bringing them down to ambient slowly before I started the run, hence the higher starting temperatures for the cells.

Finally, the thermal epoxy application on this particular module was poor - the cells to the rear of the module have very little contact with the potting material, while the ones at the front were OK. This is evident in the difference in temperatures of the two probes I had in the pack. I applied the thermal material with a spatula, rather than squeezing beads out with a gun like I did for the others. So there would definitely be better contact and heat transfer in the later modules.

Still, the delta T on the inlet and outlet was at best 0.6 'C with a flow rate of 3 litres per minute.
temp plot.JPG
temp plot.JPG (48.3 KiB) Viewed 3442 times
So at the point where the cells are as hot as they can be, the water in the cooling loop was removing heat at a rate of about 120 W. At this point the cells are generating about 1000 W of waste heat, so they get hot fast. They cooled down once the load was removed at a rate which was OK, but when I turned the pumps off for the night and went to bed, the rate of cooling was not much slower.

I might try to cool the busbars above with airflow as they are in direct contact with the core of the cells. It may end up being as effective as the liquid cooling :confused:

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Jan 11 2019 9:28am

How I make them.



Enjoy!

Frank   100 W

100 W
Posts: 227
Joined: Dec 10 2007 11:57am
Location: Maine/Nova Scotia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Frank » Jan 11 2019 12:54pm

Fun video - what is that, a couple of hours in real time?

Cooling busbars makes sense, would it be hard to try now? It sounds like you've already got some temp sensors embedded in the pack. :thumb:
Frank

User avatar
Arlo1   100 GW

100 GW
Posts: 8401
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Arlo1 » Jan 11 2019 1:17pm

Guys I read a paper showing how cooling the Tabs is the most important thing to do in cooling pouch cells.
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Jan 11 2019 7:56pm

Tab cooling is the most effective way to cool a pack but other than air convection you're limited to low thermal conductivity polymers stuck to the battery terminals. Not only that you cant seal a battery completely from the elements when you aircool. This is the perpetual dillemma. Base cooling is the best compromise here given the constraints.

User avatar
Arlo1   100 GW

100 GW
Posts: 8401
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by Arlo1 » Jan 12 2019 2:15am

jonescg wrote:
Jan 11 2019 7:56pm
Tab cooling is the most effective way to cool a pack but other than air convection you're limited to low thermal conductivity polymers stuck to the battery terminals. Not only that you cant seal a battery completely from the elements when you aircool. This is the perpetual dillemma. Base cooling is the best compromise here given the constraints.
That's where some fancy potting comes in ;)
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Feb 02 2019 6:13am

Just finished up a 28s8p battery pack (100 V, 40 Ah, 4 kWh) for another electric motorbike using the 30C continuous cells. It's built as a 24s8p pack, and a small 4s8p pack which is placed somewhere else in order to fit.
20190202_141129.jpg
20190202_141129.jpg (196.89 KiB) Viewed 3247 times
EV-Power BMS, polycarb enclosure. The cells should be good for over 1000 A continuous, but the buslinks are only 35 mm2 solid copper so probably only 200 A continuous. Not that it matters - even at 200 A the pack is flat in 12 minutes.

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Mar 18 2019 1:25am

I figure it's about time I shared the Prelude battery pack.

This battery pack sits in the fuel tank space and has six 12s10p liquid-cooled modules in series. The conversion needs two more modules up the front to make a standard 355 V nominal pack with 24 kWh of useful energy. This rear battery stored 19 kWh as it is.
released.jpg
A bit of patching, sealing and some black paint to hide my sins...
cover painted.jpg
cover painted.jpg (228.54 KiB) Viewed 2938 times
It makes for a neat fit:
HV cable routing.jpg
HV cable routing.jpg (185.31 KiB) Viewed 2938 times
I used that aluminium honeycomb sandwich material with epoxy resin potting. It's good, and very space and weight efficient, but in another life I would put some additional fixings in tension in the middle of the pack. It will be fine for this job though - only 125 kg being supported by 26 high tensile M6 bolts.

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » Apr 05 2019 1:34am

Finally shipped off this 24s10p battery where it will be going into an electric cruiser motorcycle. BMS by EV Power as before, this time with a full 12-cell read out per screen.
Splash screen 2.jpg
Splash screen 2.jpg (262 KiB) Viewed 2837 times
4.4 kWh, and will be paired up with a Motenergy and Sevcon combination (50 kW). I think it will look good when painted black (of course) :)
Pauls bike.jpg
Pauls bike.jpg (264.04 KiB) Viewed 2837 times

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3952
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Assembled Hi-Power LiPo battery packs - any interest?

Post by jonescg » May 16 2019 1:36am

Guess who's not going to have a weekend or evening free for the next month...
IMG_1150.jpg

Post Reply