Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 10 2022 7:26pm

leesafur wrote:
tylerwatts wrote:
Jan 04 2022 6:16am
Agniusm that looks like energy storage though, not high current. Would 2 8p modules in parallel be comfortable with 400A output? I am wondering about a pack similar size also.

cheers
Tyler
Hi Tyler, The answer to your question is it depends. It depends on what battery and BMS you are using. The above picture of the green batteries is mine and I was surprised to see it when it showed up in a google search lol. What you see there is 9-15s8p 63v batteries. Soon to be 15 batteries.. I paused building them last year as it was just to hot on the boat coming into summer (I'm a fulltime liveaboard) to keep printing them. Each battery has its own 40 amp BMS that's tied to a huge busbar that you cant see. Each 18650 cell that I'm using has a standard discharge rating of 0.2c which works out to be 590mA. That works out to be .59amps X 8=4.72amps X the 9 batteries = 42.48amps standard discharge. That's 2,676 watts of power without anything breaking a sweat. The maximum output is a totally different story! Maximum discharge current is (2c 5900mA) 5.9amps X 8=47.2amps X 9=424.8amps X 60volts =25,488 watts! The most my system has peaked is 414amps and the BMS's will peak to 540amps for 5s. The system is fully automatic and will simply start the generator if we are pulling more than 5,000 watts for more than 2 minutes. So... yeah.. I guess you could call it both, a energy storage system with high current. Short of spending 10 times as much and buying Battle Born Batteries this was the safest solution for me. The N.E.S.E system is a sound product that has changed everything todo with boating for us.
Lee
Hi Lee
Thanks for the background and fascinating use case. I was actually asking about the rating of the NESE hardware over the cells. I.e. if I built 8-10-12p modules of high output cells what max current could the NESE hardware handle comfortably before melting housings or seeing significant voltage drop. Particularly I'm considering how scalable the modules are for say building large motorcycle or small car packs of 20-30kwh and 100kw continuous or higher 5min rated outputs. And would I have to run a 400v system @250A to keep current down or could I run 160v say demanding 625A and possibly 30s bursts to 800A. Therefore rather than cells being the max discharge bottleneck would the NESE hardware start to be a concern?

I am aware that the hardware was improved not too long ago and rated to handle higher currents so I guess what is real world experience now showing? Does having lots of uncooled cells with potentially high current output in a densely packed battery assembly present a significant problem for the NESE system? And has anybody found a practical way for cooling potentially? Air channels in the modules or even interconnected water galleries that lock together when you stack modules maybe?

I apologise, I'm thinking aloud about the practicalities and challenges I'm likely to face on my desired builds, hypothetically.

cheers
Tyler


User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Jan 11 2022 3:09am

Tyler, its not viable to build a cooled pack out of NESE. I would not even consider such big packs as there are car batteries you could use for quiet cheaper.
So for passive pack you would want to go with as many cells as is needed to keep the pack from overheating. Cells themselved dictate so NESE modules would not melt. If they melt, your cells are at over 70C and that is far from good for your cells. I melted mine while testing modules loaded with 6 sony vtc5a at over 200A reaching ~90C.
Modules are scalable as in you parallel them. I would test my cells were they are at, at desired load in terms of heating up, then size the pack accordingly.
Last edited by agniusm on Jan 11 2022 1:08pm, edited 2 times in total.

john61ct   100 GW

100 GW
Posts: 8441
Joined: Dec 18 2018 2:06pm

Re: N.E.S.E. the no solder module

Post by john61ct » Jan 11 2022 7:56am


agniusm wrote:Tyler, its not viable to build a colled pack out of NESE.
Sorry what is meant by "colled" there?


999zip999   100 GW

100 GW
Posts: 10522
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: N.E.S.E. the no solder module

Post by 999zip999 » Jan 13 2022 11:19pm

Tyler wants a high current water cooled pack. I think.

User avatar
tylerwatts   100 W

100 W
Posts: 200
Joined: Sep 14 2012 3:10am

Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 16 2022 8:45am

Well not water cooled, wondering what the limit of an uncooled pack might be, as Agnasium said, need a bigger battery with low current draw to mitigate high heat build up, in summary.

cheers
Tyler


john61ct   100 GW

100 GW
Posts: 8441
Joined: Dec 18 2018 2:06pm

Re: N.E.S.E. the no solder module

Post by john61ct » Jan 16 2022 4:13pm

Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Jan 16 2022 9:15pm

john61ct wrote:
Jan 16 2022 4:13pm
Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs
How have your NESE kits worked out?
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
tylerwatts   100 W

100 W
Posts: 200
Joined: Sep 14 2012 3:10am

Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 21 2022 5:38am

john61ct wrote:Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs
Of course, but the weight and volume are then the problem and as I mentioned motorcycles it's then not feasible.

cheers
Tyler


User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Jan 21 2022 7:14am

tylerwatts wrote:
Jan 21 2022 5:38am
john61ct wrote:Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs
Of course, but the weight and volume are then the problem and as I mentioned motorcycles it's then not feasible.

cheers
Tyler
Not completely true. If you would compare Nissan leaf module which quiet often is used in motorcycle conversions you will notice the difference. Here is my comparison:
Nissan leaf module is 2365cm³ in volume, holds 474Wh of energy and weighs 3800g.
NESE 8P module is 246cm³ in volume, holds 86wh of energy and weighs 506g (122g module and 384g cells).
If we take 6 modules, it will take up 246x6=1476cm³ in volume, hold 86x6=516Wh of energy and weigh 506x6=3036g
So the fair comparison is
NESE 516Wh vs 474Wh LEAF - NESE stores 9% more energy
NESE 3036g vs 3800g LEAF - NESE is 20% lighter
NESE 1476cm³ vs 2365cm³ LEAF - NESE takes up 40% less space

User avatar
tylerwatts   100 W

100 W
Posts: 200
Joined: Sep 14 2012 3:10am

Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 21 2022 8:27am

agniusm wrote:
tylerwatts wrote:
Jan 21 2022 5:38am
john61ct wrote:Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs
Of course, but the weight and volume are then the problem and as I mentioned motorcycles it's then not feasible.

cheers
Tyler
Not completely true. If you would compare Nissan leaf module which quiet often is used in motorcycle conversions you will notice the difference. Here is my comparison:
Nissan leaf module is 2365cm³ in volume, holds 474Wh of energy and weighs 3800g.
NESE 8P module is 246cm³ in volume, holds 86wh of energy and weighs 506g (122g module and 384g cells).
If we take 6 modules, it will take up 246x6=1476cm³ in volume, hold 86x6=516Wh of energy and weigh 506x6=3036g
So the fair comparison is
NESE 516Wh vs 474Wh LEAF - NESE stores 9% more energy
NESE 3036g vs 3800g LEAF - NESE is 20% lighter
NESE 1476cm³ vs 2365cm³ LEAF - NESE takes up 40% less space
That is correct but it does not consider power requirements, therefore related to heat. So we said before we are forced to have higher capacity/storage to lower C output levels and reduce IR heat generation. If I want a smaller ~5-10kWh pack but capable of 5-10C peaks/short term output then cooling is likely required or temperature monitoring to protect battery from thermal runaway etc which will surely limit output after a short time.

@agniusm this is certainly no criticism of your product, it is fantastic. I want to be clear I fully support and endorse the N.E.S.E. modules.

This is rather a design constraint for the target solution. Tesla would not require battery cooling if they limited power outputs but their design requirements stipulated cooling was required to achieve performance targets.

Let's not spoil this thread with further discussion on this, not for my benefits at least.

cheers
Tyler


User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Jan 21 2022 8:44am

tylerwatts wrote:
Jan 21 2022 8:27am
That is correct but it does not consider power requirements, therefore related to heat. So we said before we are forced to have higher capacity/storage to lower C output levels and reduce IR heat generation.

If I want a smaller ~5-10kWh pack but capable of 5-10C peaks/short term output then cooling is likely required or temperature monitoring to protect battery from thermal runaway etc which will surely limit output after a short time.

@agniusm this is certainly no criticism of your product, it is fantastic. I want to be clear I fully support and endorse the N.E.S.E. modules.

This is rather a design constraint for the target solution. Tesla would not require battery cooling if they limited power outputs but their design requirements stipulated cooling was required to achieve performance targets.

Let's not spoil this thread with further discussion on this, not for my benefits at least.

cheers
Tyler
Not spoiling for sure. Its good info and I haven't done a comparison myself.
In regards to power, it would be on par with leaf module at 300A roughly (3 modules in parallel or 72ah). This estimate covers for the heating.

I have done calculations with sony vtc6. 3000mah cell @ 48g per piece. These are 30A rated cells so they would stay cool enough. Total of them would be capable of 720A(24P)

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Jan 21 2022 11:20pm

Never mind. JCT (Hans)has no skin in the game. Just blather from a virtual “expert”with zero experience with most of the bits commented on.
tylerwatts wrote:
Jan 21 2022 5:38am
john61ct wrote:Yes, preventing heat from being generated internally in the first place, if practical is far far better than needing cooling solutions.

Lower C-rates and capacity utilisation can extend also lifespan by 3x 5x or more

drastically lowering annual running costs
Of course, but the weight and volume are then the problem and as I mentioned motorcycles it's then not feasible.

cheers
Tyler
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
tylerwatts   100 W

100 W
Posts: 200
Joined: Sep 14 2012 3:10am

Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 23 2022 5:38pm

agniusm wrote:
tylerwatts wrote:
Jan 21 2022 8:27am
That is correct but it does not consider power requirements, therefore related to heat. So we said before we are forced to have higher capacity/storage to lower C output levels and reduce IR heat generation. If I want a smaller ~5-10kWh pack but capable of 5-10C peaks/short term output then cooling is likely required or temperature monitoring to protect battery from thermal runaway etc which will surely limit output after a short time.

@agniusm this is certainly no criticism of your product, it is fantastic. I want to be clear I fully support and endorse the N.E.S.E. modules.

This is rather a design constraint for the target solution. Tesla would not require battery cooling if they limited power outputs but their design requirements stipulated cooling was required to achieve performance targets.

Let's not spoil this thread with further discussion on this, not for my benefits at least.

cheers
Tyler
Not spoinling for sure. Its good info and i haven't done comparison myself.
In regards to power, it would be on par with leaf module at 300A roughly(3 modules in parallel or 72ah). This estimate covers for the heating. I have done calculations with sony vtc6. 3000mah cell @ 48g per piece. These are 30A rated cells so they would stay cool enough. Total of them would be capable of 720A(24P)
Thank you Agniusm ImageImage

cheers
Tyler


mozolis   1 µW

1 µW
Posts: 1
Joined: Feb 04 2022 6:20am

Re: N.E.S.E. the no solder module

Post by mozolis » Feb 08 2022 5:44am

agniusm wrote:
Feb 27 2021 6:20am
Forgot to mention, 21700 tabs are redone and now have larger area

Image
where to buy?

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Feb 08 2022 2:45pm

mozolis wrote:
Feb 08 2022 5:44am
agniusm wrote:
Feb 27 2021 6:20am
Forgot to mention, 21700 tabs are redone and now have larger area

Image
where to buy?

www.18650.lt
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Feb 09 2022 9:00am

Anyone knows what happened with vruzend? I see all the threads are deleted/removed?

john61ct   100 GW

100 GW
Posts: 8441
Joined: Dec 18 2018 2:06pm

Re: N.E.S.E. the no solder module

Post by john61ct » Feb 09 2022 6:24pm


eMark   10 kW

10 kW
Posts: 738
Joined: Nov 02 2019 11:53am

Re: N.E.S.E. the no solder module

Post by eMark » May 09 2022 2:01pm

agniusm wrote:
Feb 09 2022 9:00am
Anyone knows what happened with vruzend? I see all the threads are deleted/removed?
The V2.1 kit is still available AFAIK. I've emailed Micah a couple times (2020 and recently), but he never replies. My recent email was encouraging him to offer a 10s3p 21700 V2.2 kit.

I've been using a V2.1 kit for my 2020 experimental 10s3p 30Q build. I had to replace nine of the 30Q '141' cells because of high self-discharge with '6T' cells. So far have 250+ cycles on twenty-one '141' cells and 125+ cycles on nine '6T' cells. My take away so far is that IMR unknowingly shipped me both Grade A & B '141' cells. Hopefully all 9 of the replaced '6T' cells are Grade A (won't know for sure until disassembling pack and testing all the cells again in November), but so far AOK.

The great advantage of the Vruzend V 2.1 kit is for eperimenting (ease of assembly and disassembly). Also excellent for a beginner to wrap their mind around parallel, series, current flow, attaching balance leads, etc. I can split my 10s3p into 5s6p for bulk charging with my RC 2s-6s Balance Charger with p-group voltage readouts during charging as well as checking IR of each p-group. Use JST-XH 5s Y-cable (p-group voltage readouts) and 5s Deans Y-cable (2amp charge).

The Vruzend V.2 kit would serve as a great high school science teaching/learning build project for gals as much as guys (the dos and don'ts as well as answering all the - WHYs). The kit had it's drawbacks, but definitely served a useful niche; especially for beginners.

Think Micah got his fill of those that belittled his kit as "crap". Thus a 21700 kit may not be a top priority ... as much as i would be one of the first to buy one if in the pipeline.

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » May 10 2022 8:14am

An all new vruzend design will be released, soon I think. Covid was a business crushing event everywhere.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.