N.E.S.E. the no solder module

Place for dealers to post items for sale.
User avatar
ZeroEm   10 MW

10 MW
Posts: 2335
Joined: May 03 2019 11:53am
Location: San Antonio, TX

Re: N.E.S.E. the no solder module

Post by ZeroEm » Nov 09 2021 10:26am

I like it and it's not for everyone. Keep finding uses for your modules and show them to people. Think you have a bright future.
Would like to build my next battery from your modules but it's so big the cost is more than the rest. I'm thinking for the smaller projects they would be a great fit. Have rechargeable bike lights and solar lights in the yard that need battery replacements. Were are talking about 1p so a dual cell module made to be water resistant (not water proof) would be great. I like small rechargeable's but the cells are to small and always need to damage them to access the battery.
2019 Performer E-Trike
2013 Nissan Leaf S 7 bars 331.5w/KM

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Nov 09 2021 12:32pm

Brilliant for sure!
You've proved to be the most reliable method, with none of the caveates other designs exhibit.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

pomah   10 W

10 W
Posts: 67
Joined: Jan 02 2016 3:09pm
Location: Gothenburg, Sweden

Re: N.E.S.E. the no solder module

Post by pomah » Nov 20 2021 10:28am

Hi, looking into making my next battery using this design, but a few questions that I have not found an answer for:

1) On thingverse the 21700 module has a "normal" and a v2 design, what is the difference?
2) On your webpage when ordering the tabs, you can order "normal" and "shallow" once again what is the difference?
3) when building a 13s3p (21700) battery, when ordering tabs on your website, if I add text that it is a 3p and order 13 sets of the tabs, that should be enough for the whole pack?

Thank you for your time and your great work.

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Nov 20 2021 1:16pm

pomah wrote:
Nov 20 2021 10:28am
Hi, looking into making my next battery using this design, but a few questions that I have not found an answer for:

1) On thingverse the 21700 module has a "normal" and a v2 design, what is the difference?
2) On your webpage when ordering the tabs, you can order "normal" and "shallow" once again what is the difference?
3) when building a 13s3p (21700) battery, when ordering tabs on your website, if I add text that it is a 3p and order 13 sets of the tabs, that should be enough for the whole pack?

Thank you for your time and your great work.
Hi,
1. V2 is most recent design. You can get it here: https://cults3d.com/en/users/18650/creations
2. Normal and shallow reffers to bolts and how much they stick out off enclosure. For exact numbers check Resources on the website. Normal is hex bolt with phillips, spring and flat washers attached, shallow is allen type with serrated washer. See attached photo.
3. 13 sets can build you 2 batteries, 3P and 5P. Tabs are 8P, double ended. You can make 13S out of 7 tab sets but you need to order 6 more fixing sets.
Fljoy6j.jpg
Fljoy6j.jpg (71.35 KiB) Viewed 978 times

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Nov 24 2021 2:59am

Starting 2021.12.01 until 2022.01.04
sale.jpg
sale.jpg (2.58 MiB) Viewed 936 times

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Nov 25 2021 8:15pm

Cool. Time for another kit or two.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Nov 26 2021 9:00am

tomjasz wrote:
Nov 25 2021 8:15pm
Cool. Time for another kit or two.
Do you have one built? How long and any photos you shared?

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Nov 26 2021 1:49pm

PM sent
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

pomah   10 W

10 W
Posts: 67
Joined: Jan 02 2016 3:09pm
Location: Gothenburg, Sweden

Re: N.E.S.E. the no solder module

Post by pomah » Nov 26 2021 2:17pm

agniusm wrote:
Nov 20 2021 1:16pm
pomah wrote:
Nov 20 2021 10:28am
Hi, looking into making my next battery using this design, but a few questions that I have not found an answer for:

1) On thingverse the 21700 module has a "normal" and a v2 design, what is the difference?
2) On your webpage when ordering the tabs, you can order "normal" and "shallow" once again what is the difference?
3) when building a 13s3p (21700) battery, when ordering tabs on your website, if I add text that it is a 3p and order 13 sets of the tabs, that should be enough for the whole pack?

Thank you for your time and your great work.
Hi,
1. V2 is most recent design. You can get it here: https://cults3d.com/en/users/18650/creations
2. Normal and shallow reffers to bolts and how much they stick out off enclosure. For exact numbers check Resources on the website. Normal is hex bolt with phillips, spring and flat washers attached, shallow is allen type with serrated washer. See attached photo.
3. 13 sets can build you 2 batteries, 3P and 5P. Tabs are 8P, double ended. You can make 13S out of 7 tab sets but you need to order 6 more fixing sets.

Fljoy6j.jpg
Thank you, had to read the answer to 3 a few times before I got it, had to look at the pictures on your website :)
I'll make an order while they will be on sale, so happy to finally jump on this, have been waiting for my current battery to "die" on me so I could motivate the investment into this.

Thank you for your answers

pomah   10 W

10 W
Posts: 67
Joined: Jan 02 2016 3:09pm
Location: Gothenburg, Sweden

Re: N.E.S.E. the no solder module

Post by pomah » Dec 07 2021 8:42am

Hi, I have some issues printing these modules on a Ender v3 using the "Cura" slicer.

Current settings I use are attached to this post.

I am gratefull for all suggestion from someone with more experience printing these
Attachments
1.png
1.png (35.62 KiB) Viewed 788 times
2.png
2.png (35.89 KiB) Viewed 788 times

pomah   10 W

10 W
Posts: 67
Joined: Jan 02 2016 3:09pm
Location: Gothenburg, Sweden

Re: N.E.S.E. the no solder module

Post by pomah » Dec 10 2021 3:16pm

For anyone wondering, the issue seems to have been with the "white" plastic, same settings worked like a charm on a black PETG role but still wont work for two different types of white PETG. Not sure why, I just read that other people have issues with "white" PETG.

One module is printed and assembled looking forward to finishing my 13s pack :)

User avatar
neptronix   100 GW

100 GW
Posts: 16351
Joined: Jun 15 2010 5:56pm
Location: Utah, USA
Contact:

Re: N.E.S.E. the no solder module

Post by neptronix » Dec 10 2021 3:21pm

Are there any good 26650's out there to use the 26650 kit with at this point?

I always liked the idea of using big honkin' cells and think that this would be a great setup with them.
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500 MTB.
Monster MTB: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: Cannondale semi recumbent - under construction.
Blue Dream: Maxaraya FS semi recumbent and high efficiency mid-drive - under construction.

john61ct   100 GW

100 GW
Posts: 8441
Joined: Dec 18 2018 2:06pm

Re: N.E.S.E. the no solder module

Post by john61ct » Dec 10 2021 4:28pm

For LFP

A123 / Lithium Werks

ANR26650M1B

Apparently Liitokala / VariCore not shabby

justlooking808   100 W

100 W
Posts: 102
Joined: Sep 01 2021 7:05pm

Re: N.E.S.E. the no solder module

Post by justlooking808 » Dec 10 2021 5:03pm

tomjasz wrote:
Nov 26 2021 1:49pm
PM sent
hi, im interested in pictures also. thinking or seeing if i should try this venture for those 60v speed days.
Current Ebike = Custom ride1up Core5 ST Older, Nicer Version. 8) (got totaled :( )
Current Project = Qualisport Beluga that took a swim in the ocean :shock:

User avatar
tomjasz   10 GW

10 GW
Posts: 4663
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: N.E.S.E. the no solder module

Post by tomjasz » Dec 10 2021 8:24pm

john61ct wrote:
Dec 10 2021 4:28pm
For LFP

A123 / Lithium Werks

ANR26650M1B

Apparently Liitokala / VariCore not shabby
Are you using the NESE kit or just trolling this thread too.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Dec 11 2021 2:24am

neptronix wrote:
Dec 10 2021 3:21pm
Are there any good 26650's out there to use the 26650 kit with at this point?

I always liked the idea of using big honkin' cells and think that this would be a great setup with them.

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Dec 11 2021 2:25am

neptronix wrote:
Dec 10 2021 3:21pm
Are there any good 26650's out there to use the 26650 kit with at this point?

I always liked the idea of using big honkin' cells and think that this would be a great setup with them.
Not many 26650 cells. There are few 4.2V cells but i have no idea how they perform. One of them is 15A Keeppower IMR26650, 5500mAh.

alexayala.ut   1 mW

1 mW
Posts: 11
Joined: May 07 2020 2:22pm
Location: Florida

Re: N.E.S.E. the no solder module

Post by alexayala.ut » Dec 11 2021 6:18pm

I originally bought some of these last year because I was looking at the cost of these vs a kWeld, and the total cost would have been similar. I already had a 3d printer, and had bought 10kg of PETG for $100 a while back, so those were sunk costs. Each roll printed about 11-12 8p cases.

I'm so glad I went with these because they are so adjustable. I currently have a 13s8p primary pack with that I use for my recumbent, and a second 16s8p pack for my cargo bike that'll I'll also split down to 4x4s8p to get a 12v battery for my trolling motor when I get out on the water. My recumbent is also my commuter, and I commute 18 miles each way, so I've run quite a bit of power through the pack over the past year.

The flexibility also lets me easily try different things. I have a heated 12V jacket that is normally plugged into a vehicle 12V system. I took four of my 8p packs, slipped them into a clipboard case, and had a portable power source I could slide into my backpack. I don't need a dedicated battery for something like that, but it's easy to grab a few packs and reconfigure for a weekend project with this system. Afterwards, I could return the packs to my ebike.

The 8p height fits perfectly in the metal 0.50 caliber ammo cans, and you can fit 13s in a single column, or 21s in 3 rows of 7, or whatever you want. I also experimented with the 4x4 vinyl fenceposts, and 4p packs fit into those pretty nicely. 3d print the end caps, and you can make nice compact booster packs that you can slot into your bike if you're going on a longer ride.

My controllers can take up to 21s, so the NESE system let me try different voltages for a while, and easily adjust if it was too much or not enough voltage without having to tear apart the entire battery.

I'm very much a Grin fan, and I think agniusm's battery system is an excellent complement to all the Grin hardware. Both just work, they're not something you have to worry about. However, I think agniusm's system is how Grin should have built their LiGo packs (1s8p instead of 10s1p), because it's just so flexible. Especially when compared to the LiGo system, NESE modules that cost around $10 plus batteries (new would be ~$3/cell, reclaimed ~$1/cell) are an amazing bargain.

I picked up more batteries over the course of this year with the hope the winter sale would return (I'm in the US, so the sale basically gives me free shipping). Time to order more!

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Dec 12 2021 2:58am

alexayala.ut wrote:
Dec 11 2021 6:18pm
I originally bought some of these last year because I was looking at the cost of these vs a kWeld, and the total cost would have been similar. I already had a 3d printer, and had bought 10kg of PETG for $100 a while back, so those were sunk costs. Each roll printed about 11-12 8p cases.

I'm so glad I went with these because they are so adjustable. I currently have a 13s8p primary pack with that I use for my recumbent, and a second 16s8p pack for my cargo bike that'll I'll also split down to 4x4s8p to get a 12v battery for my trolling motor when I get out on the water. My recumbent is also my commuter, and I commute 18 miles each way, so I've run quite a bit of power through the pack over the past year.

The flexibility also lets me easily try different things. I have a heated 12V jacket that is normally plugged into a vehicle 12V system. I took four of my 8p packs, slipped them into a clipboard case, and had a portable power source I could slide into my backpack. I don't need a dedicated battery for something like that, but it's easy to grab a few packs and reconfigure for a weekend project with this system. Afterwards, I could return the packs to my ebike.

The 8p height fits perfectly in the metal 0.50 caliber ammo cans, and you can fit 13s in a single column, or 21s in 3 rows of 7, or whatever you want. I also experimented with the 4x4 vinyl fenceposts, and 4p packs fit into those pretty nicely. 3d print the end caps, and you can make nice compact booster packs that you can slot into your bike if you're going on a longer ride.

My controllers can take up to 21s, so the NESE system let me try different voltages for a while, and easily adjust if it was too much or not enough voltage without having to tear apart the entire battery.

I'm very much a Grin fan, and I think agniusm's battery system is an excellent complement to all the Grin hardware. Both just work, they're not something you have to worry about. However, I think agniusm's system is how Grin should have built their LiGo packs (1s8p instead of 10s1p), because it's just so flexible. Especially when compared to the LiGo system, NESE modules that cost around $10 plus batteries (new would be ~$3/cell, reclaimed ~$1/cell) are an amazing bargain.

I picked up more batteries over the course of this year with the hope the winter sale would return (I'm in the US, so the sale basically gives me free shipping). Time to order more!
Thank you very much for taking time and sharing your experience. Really helps. Hopefully more people will get to experience battery builds that are quick and enjoyable and if you have 3D printer, accidentally damaged parts are few hours away :)

pomah   10 W

10 W
Posts: 67
Joined: Jan 02 2016 3:09pm
Location: Gothenburg, Sweden

Re: N.E.S.E. the no solder module

Post by pomah » Dec 25 2021 12:09pm

Finished my 13s build using the N.E.S.E modules. I am very happy with the result, seller is great to deal with, answers email and gave support before my purchase on what to order.

The final result is a bit larger than my older welded pack, but this is my last pack that I need to build and I can just rebuild it if something issues would occur with time.

Image
Battery built
Image
BMS wires attached
Image
Test install in custom bike electronics box

All in all I am very happy with choosing the system, the issues I had was with printing the modules (my own fault due to being novice with a 3d printer). With that in hind sight I would just order the complete set through AMtech, the totalt cost is mostly negligible and you know that you will get good printed modules you can start building with.

Wimbi39   10 mW

10 mW
Posts: 32
Joined: Oct 29 2021 2:27pm

Re: N.E.S.E. the no solder module

Post by Wimbi39 » Dec 25 2021 3:36pm

Has anyone ever made a "bigger" Pack using these modules? I am planning a 20s16p pack and would like to use the nese system, I am not sure if they will be able to handle the current I will be needing though (200a continuous, 400a max)

User avatar
agniusm   100 MW

100 MW
Posts: 2551
Joined: Apr 16 2011 3:06pm
Location: Lithuania, Zarasai
Contact:

Re: N.E.S.E. the no solder module

Post by agniusm » Dec 27 2021 12:15pm

Wimbi39 wrote:
Dec 25 2021 3:36pm
Has anyone ever made a "bigger" Pack using these modules? I am planning a 20s16p pack and would like to use the nese system, I am not sure if they will be able to handle the current I will be needing though (200a continuous, 400a max)
There are some big packs in the wild :)
IMG_3649.JPEG
IMG_3649.JPEG (2.8 MiB) Viewed 478 times

User avatar
tylerwatts   100 W

100 W
Posts: 200
Joined: Sep 14 2012 3:10am

Re: N.E.S.E. the no solder module

Post by tylerwatts » Jan 04 2022 6:16am

Agniusm that looks like energy storage though, not high current. Would 2 8p modules in parallel be comfortable with 400A output? I am wondering about a pack similar size also.

cheers
Tyler


leesafur   1 µW

1 µW
Posts: 2
Joined: Feb 10 2021 2:05pm

Re: N.E.S.E. the no solder module

Post by leesafur » Jan 04 2022 9:42pm

tylerwatts wrote:
Jan 04 2022 6:16am
Agniusm that looks like energy storage though, not high current. Would 2 8p modules in parallel be comfortable with 400A output? I am wondering about a pack similar size also.

cheers
Tyler
Hi Tyler, The answer to your question is it depends. It depends on what battery and BMS you are using. The above picture of the green batteries is mine and I was surprised to see it when it showed up in a google search lol. What you see there is 9-15s8p 63v batteries. Soon to be 15 batteries.. I paused building them last year as it was just to hot on the boat coming into summer (I'm a fulltime liveaboard) to keep printing them. Each battery has its own 40 amp BMS that's tied to a huge busbar that you cant see. Each 18650 cell that I'm using has a standard discharge rating of 0.2c which works out to be 590mA. That works out to be .59amps X 8=4.72amps X the 9 batteries = 42.48amps standard discharge. That's 2,676 watts of power without anything breaking a sweat. The maximum output is a totally different story! Maximum discharge current is (2c 5900mA) 5.9amps X 8=47.2amps X 9=424.8amps X 60volts =25,488 watts! The most my system has peaked is 414amps and the BMS's will peak to 540amps for 5s. The system is fully automatic and will simply start the generator if we are pulling more than 5,000 watts for more than 2 minutes. So... yeah.. I guess you could call it both, a energy storage system with high current. Short of spending 10 times as much and buying Battle Born Batteries this was the safest solution for me. The N.E.S.E system is a sound product that has changed everything todo with boating for us.
Lee

leesafur   1 µW

1 µW
Posts: 2
Joined: Feb 10 2021 2:05pm

Re: N.E.S.E. the no solder module

Post by leesafur » Jan 04 2022 9:47pm

agniusm wrote:
Dec 27 2021 12:15pm
Wimbi39 wrote:
Dec 25 2021 3:36pm
Has anyone ever made a "bigger" Pack using these modules? I am planning a 20s16p pack and would like to use the nese system, I am not sure if they will be able to handle the current I will be needing though (200a continuous, 400a max)
There are some big packs in the wild :)

IMG_3649.JPEG
And its getting bigger! The print time is now down to 3hrs per module 8)

Post Reply