goatman said:wound up with 14 reverse polarity cells
5 at 0 volts
4 at 3.78v
73 at 0.1 volts
going to put tinfoil and magnets on each 1s18p pack and slowly charge to see if if they can be brought back to life
not corrosion, is vapor-deposition of the metal that used to be the cap leads.calab said:Very strange corrosion damage on those capacitors.