As the title says its a test and review of 100 cells from batteryhookup.com. I wanted cells for my E Chopper build and these fit the bill well. Paid $1.50 a cell and avg mah was over 2600. More details are in the description as well. Results are at 4:43 time line.
[youtube]cMIOPPhby6w[/youtube]
https://youtu.be/cMIOPPhby6w