Does anyone here build these in the US?
M momo 100 W Joined Jan 14, 2008 Messages 109 Mar 17, 2022 #1 Does anyone here build these in the US? Attachments 20220317_151446.jpg 7.2 MB · Views: 426 20220317_151509.jpg 7.6 MB · Views: 426 20220317_151435.jpg 6.8 MB · Views: 426 20220317_151454.jpg 7.2 MB · Views: 426
C calab 1 MW Joined Dec 10, 2013 Messages 2,063 Mar 17, 2022 #2 Have you checked out https://ebikes.ca/shop/electric-bicycle-parts/battery-accessories.html To see if anythings even close?
Have you checked out https://ebikes.ca/shop/electric-bicycle-parts/battery-accessories.html To see if anythings even close?
M momo 100 W Joined Jan 14, 2008 Messages 109 Mar 21, 2022 #3 Here's a cheap method I found and very simple. Pickup brackets from lowes or home depo. Attachments Screenshot_20220320-163632_eBay.jpg 718.5 KB · Views: 376
jimmyhackers 10 kW Joined May 11, 2015 Messages 602 Mar 21, 2022 #4 yep, local diy or plumbing store, metal tube mounts or pipe clamps. cheaper and stronger. you can even paint them black or other fancy colours with a spray can
yep, local diy or plumbing store, metal tube mounts or pipe clamps. cheaper and stronger. you can even paint them black or other fancy colours with a spray can