Voltage: 36v (Max voltage - 42v Min voltage - 30v)
Capacity: 21000mAh 756wH
Discharge rate: 60a continuous 90a peak
Wattage output: 750w continuous 1050w peak
Charge rate: 6 amp max
Charge voltage: 42v
Charge time: 4 hours
Condition: Lightly used, less than 30 times (tested with capacity tester)
Manufacturer: SCUD
Enclosure: Hardened epoxy resin sheets, shrink wrap. No plastic enclosure
Weight: 7.4 lb.
Dimensions: 13 inch x 4.8 inch x 1.6 inch
Cell holders: SCUD 12 cell module with integrated core rods for rigidity.
Connector: xt60 + charging port
BMS: 30A with low voltage cut-off overcharge protection, temperature management, current output and short circuit protection, power equalization output.
Cycle life: ~800-1200 full charge and discharge cycles (gentle use) or 500-800 cycles if used regularly
Amount of cells: 60
Configuration: 10 series and 6 parallels
Cell manufacturer: LG
Cell model: inr18650mj1
Cell size: 18650
Cell chemistry: Lithium Ion
Cell capacity: 3500
Cell connection: 0.2mm pure nickel strips
Storage temperature: -15 ~ +35 ℃, humidity: 45-75%,
Operating temperature: Discharging 0-60 ℃; Charging 0-45 ℃;

Additional details:
Does not come with a charger.