Hey everyone! I have around 200 Panasonic NCR18650BD cells that I have salvaged from electric scooter batteries. They are rated at 3100 mAh as new and I’ve tested them all with no batteries below 3000mAh and most of them sitting at around the 3100mAh mark, using a Liitokala-Lii500.
I’m based in southern Sweden but I can ship them to anywhere in Europe aswell as to the US. I’m asking for 2.5€ each but for large orders(>35 cells) I’m willing to go down in price.
Here is an imgur link with some pictures of the cells:
https://imgur.com/gallery/UEPaUQV
If you want me to add more pictures/information feel free to tell me in the thread.
Cheers
Noak