1 Turnigy multistar 6s 16,000mah $65usd each + shipping

PeeHell

100 W
Joined
Jul 30, 2011
Messages
184
Location
Montreal
1/15 batteries remaining. See details below

I have 1 Turnigy multistar 6s 16,000mah battery packs.They were bought $127usd each on Hobbyking. The internal resistance ranges below have been measured with a SkyRC Imax B6 v2 charger. Series and parallel connectors can be included for free upon request.

  • 1 Turnigy multistar 6s 16,000mah battery packs available
  • Internal resistance within 2 mOhms
  • 13 charging/discharging cycles
  • $65usd per battery + shipping cost from Canada

Battery cycles Gui.jpg

I also have a brand new Turnigy 6s 16,000mah battery pack selling for $100USD + shipping. PM if interested and/or any questions.
Pierre-Luc
 

Attachments

  • PXL_20220406_185035490.jpg
    PXL_20220406_185035490.jpg
    2.3 MB · Views: 1,033
Hi,

These can be assemble into a bigger battery pack, right? And 6 of these will be 390 CAD?

I am assuming 6 of these will give me 66.6 V and 32 AH.

I have a brother-in-law in Ottawa. He can ship it to me (Chennai, India).

Let me have a word with him and I will let you know.

Thank you.

SHAILENDRA SHANKAR
 
Shailendra Shankar said:
Hi,

These can be assemble into a bigger battery pack, right? And 6 of these will be 390 CAD?
I am assuming 6 of these will give me 66.6 V and 32 AH.
I have a brother-in-law in Ottawa. He can ship it to me (Chennai, India).
Let me have a word with him and I will let you know.
Thank you.

SHAILENDRA SHANKAR

Sent you a PM :thumb:
 
Is the new one still available? Either way I’d like to buy a few of them. What is the c rating? I think most are between 10c-20c on those lines
 
RichBlac said:
Is the new one still available? Either way I’d like to buy a few of them. What is the c rating? I think most are between 10c-20c on those lines

PM sent
 
Back
Top