j bjork said:I think it would be interesting to hear if people had problems without statoraid too.
https://endless-sphere.com/forums/viewtopic.php?p=1551213#p1541839
j bjork said:I think it would be interesting to hear if people had problems without statoraid too.
amberwolf said:j bjork said:I think it would be interesting to hear if people had problems without statoraid too.
https://endless-sphere.com/forums/viewtopic.php?p=1551213#p1541839
hias9 said:Do you guys also have rust at the bearings when using Statorade?
This is the Chinese bearing (left side) after a bit over a year with Statorade. Technically it was still ok.
The bearing (right side) in the background is a FAG bearing after less than 2 months with Statorade.
I seal the cover plates using a high temperature silicone motor sealant.
hias9 said:What you see on the pictures are the interior sides of the bearings.
On the exterior sides there was only very little rust even after 1.5 years of use.
My side covers are sealed so the only way for moisture to get insid