A peak of 23A per cell with a continuous 6A per cell can easily be handled by 0.10mm copper, which has the same conductivity as 0.40mm nickel without the high resistance.
I am curious about any results you could post about settings for 0.15mm copper, and if you do that, I would gladly paypal you the cost of buying the copper for the test.