TrotterBob
100 W
- Joined
- May 10, 2016
- Messages
- 219
Oh dayum. That does not look like fun.
ridethelightning said:ace man! that looks like good stuff. how did you get .3mm,? link is 0.15mm i saw
I posted it so that others might give it a try too, but yeah...I'll be posting if I can spot weld it or not.john61ct said:key issue is, if the plating is thick enough to increase the copper's resistance enough
Please let us know!
Are you using Kweld with caps or lipo or? Optimizing the joules output might be critical
john61ct said:Great stuff.
Best to also post this setup description with your results if successful to the main KWELD thread for reference there.
Using the kcap units in effect insulates the main unit from batteries that have too high/fast power output, is that correct?
ridethelightning said:id be keen to see if you manage to weld the nickel plated copper.
i tried plating my own but the power of the weld pulse for copper just flashed off the nickel when i tried to weld it.
if i can find some tin it may prove to be better.
i dont know how the power tool packs are done, many use plated copper. i may try welding some of the strips from them onto cells.
Any way for those that don't FB?spinningmagnets said:From Ian M Molina on facebook. 0.20mm copper sheet, 0.15mm nickel, kWeld at 60J
https://www.facebook.com/100000645165546/videos/pcb.908101586417740/229170929021460