I received 3 LiFePO4 38120 cell of 3.2V 8.0Ah.
I will test those 3 identicals cells with my lab equipment soon and will post some true specs. I asked 3 for having better and realistic results acuraccy.
Here are some spec from Headway:
Oem specs
3.2V
8.0Ah
300g = 85.3Wh/kg
25.6Wh/cell
80A continuous
160 peak
2.8mohm