18650 Li-ion at $145 per KiloWatt Hour!

General Discussion about electric bicycles.
User avatar
liveforphysics   100 GW

100 GW
Posts: 14045
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by liveforphysics » May 20 2011 7:11pm

I don't know how many times I've gotta say it, but once more won't hurt I guess.

Ultrafire does NOT have a battery factory. Period.

They do not manufacture batteries. Period.


They buy lots of cheap cells (b-stock and/or QC fails) from people that do manufacture cells, and shrink-wrap them in Ultra-fire labels (and rip off tab welds and put little covers on the ends if needed to make it looks like a decent cell etc).

Totally fine for things like flashlights where nobody cares as long as it works.

Terrible idea for an EV pack, where you're only as strong as your weakest cell group, and a single failure can take down a whole cell group.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

oscaryu1   1 mW

1 mW
Posts: 18
Joined: Sep 12 2010 3:57pm

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by oscaryu1 » May 21 2011 8:49am

True true... but I've gone far to look back. Crapstock or not, the "new" cells actually do perform decently IMO. I had a 5P1S pack, 3.7v actually turn over a forklift motor without even raising the batteries a degree in temperature LOL.... that was surprising.

oscaryu1   1 mW

1 mW
Posts: 18
Joined: Sep 12 2010 3:57pm

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by oscaryu1 » May 29 2011 11:50am

Image

das sum boalshiz. First batch like that. Let's see how this ends out..

zombiess   100 MW

100 MW
Posts: 2868
Joined: Feb 01 2011 2:16am
Location: Ventura

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by zombiess » May 29 2011 1:38pm

How much time are you putting into this pack?

User avatar
neptronix   100 GW

100 GW
Posts: 13160
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by neptronix » May 29 2011 2:22pm

oscaryu1 wrote:das sum boalshiz. First batch like that. Let's see how this ends out..
Friends don't let friends buy ultrafires.. ;)
My first major build: 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w on a Turner O2 full suspension.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14045
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by liveforphysics » May 29 2011 3:50pm

I love how they are all different colors from random batches, and unprinted/unlabled because they failed QC and were culled before continuing on to the labeling machine. Lol

It's funny how random reject cells get labeled as higher capacity than the best in the world are capable of achieving.

Kai has a good sense of humor.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

oscaryu1   1 mW

1 mW
Posts: 18
Joined: Sep 12 2010 3:57pm

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by oscaryu1 » May 30 2011 6:05pm

Image

Image

Hillhater   100 GW

100 GW
Posts: 9459
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by Hillhater » May 30 2011 8:26pm

.. :shock: are those end caps just loose ??... held on only by the shrink wrap ? :o :lol: :lol: :lol:
Image
This forum owes its existence to Justin of ebikes.ca

999zip999   100 GW

100 GW
Posts: 8548
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by 999zip999 » May 30 2011 8:57pm

Got to love it. They looked better with the wrapper.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14045
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by liveforphysics » May 30 2011 9:16pm

Yep, the caps just sit on the end, touching the tiny high points from the residual spot welds that were ripped off.

Its ultrafire quality.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
beast775   100 kW

100 kW
Posts: 1205
Joined: Jul 05 2007 11:55am
Location: victoria british columbia

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by beast775 » May 30 2011 10:26pm

i use these for hobby apps that dont use tremendous draw and i find each battery has its own personality :) .i dont know if i would bundle a bunch for ebike battery.i hope it works!
2 FINGER SALUTE TO ESSO.no buying gasoline for 7 years now.
I spent all my money on bicycles women and beer the rest i just wasted.

User avatar
DrkAngel   100 GW

100 GW
Posts: 5028
Joined: Dec 15 2010 11:14am
Location: Upstate-Western-Southern Tier NY. USA

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by DrkAngel » May 31 2011 6:48am

oscaryu1 wrote:Image
Impressive work!
Would work nicely, as a "saddlebag" configuration.
Highly recommend-don't forget to, install a fuse, on each pack.

Also, I cover the sides of the pack with clear "boxing" tape. (after attaching balancing leads ... of course)
It will:
Add stability;
Protect from minor short dangers;
Still allow visual inspection.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - February 2019

EBike Toolbox - Bargains! $

Endless Sphere Wiki - Lost?

thomas.smith   1 µW

1 µW
Posts: 2
Joined: Dec 01 2011 12:56am

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by thomas.smith » Dec 01 2011 1:08am

For any interested... I recently picked up 50 of the UltraFire 3800mAh cells. I figured I would play with them to see what I could work out. First off... The ones that I got were not recapped and had no other signs of repackaging (only tore down a dozen, but got bored doing that). Second, I tested those dozen cells, and was getting pretty reliably around 3700mAh.
I sure am not gonna go saying that UltraFires are just fine, but from the sounds of it, they can be hit or miss...
I am working on a cheap reliable BMS now, and when that is done, I plan on really putting them through their paces.

P.S. I managed to pick mine up for $75 (about 11 cents per watt-hour)

User avatar
liveforphysics   100 GW

100 GW
Posts: 14045
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by liveforphysics » Dec 01 2011 1:10am

thomas.smith wrote:For any interested... I recently picked up 50 of the UltraFire 3800mAh cells. I figured I would play with them to see what I could work out. First off... The ones that I got were not recapped and had no other signs of repackaging (only tore down a dozen, but got bored doing that). Second, I tested those dozen cells, and was getting pretty reliably around 3700mAh.
I sure am not gonna go saying that UltraFires are just fine, but from the sounds of it, they can be hit or miss...
I am working on a cheap reliable BMS now, and when that is done, I plan on really putting them through their paces.

P.S. I managed to pick mine up for $75 (about 11 cents per watt-hour)

You do not have 3700mAh 18650 cells.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
neptronix   100 GW

100 GW
Posts: 13160
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by neptronix » Dec 01 2011 2:33am

:lol: yup...

Panasonic is not even up to that density in an 18650 cell yet. They're up to.. i think.. 3.4AH for the Tesla Model S?

Run it through a graphing RC charger or CBA-2/CBA-3 and you'll learn the ugly truth.
My first major build: 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w on a Turner O2 full suspension.

User avatar
Ypedal   100 GW

100 GW
Posts: 12521
Joined: Dec 27 2006 12:55pm
Location: Moncton NB, Canada
Contact:

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by Ypedal » Dec 01 2011 8:07am

thomas.smith wrote:For any interested... I recently picked up 50 of the UltraFire 3800mAh cells. I figured I would play with them to see what I could work out. First off... The ones that I got were not recapped and had no other signs of repackaging (only tore down a dozen, but got bored doing that). Second, I tested those dozen cells, and was getting pretty reliably around 3700mAh.
I sure am not gonna go saying that UltraFires are just fine, but from the sounds of it, they can be hit or miss...
I am working on a cheap reliable BMS now, and when that is done, I plan on really putting them through their paces.

P.S. I managed to pick mine up for $75 (about 11 cents per watt-hour)
Please do tell us more about how you tested the cells !!

we love pictures ! :P
ES site status page:
http://www.ypedal.com/ES/ES.htm
----------------
http://www.ypedal.com

User avatar
Ypedal   100 GW

100 GW
Posts: 12521
Joined: Dec 27 2006 12:55pm
Location: Moncton NB, Canada
Contact:

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by Ypedal » Dec 01 2011 8:15am

ES site status page:
http://www.ypedal.com/ES/ES.htm
----------------
http://www.ypedal.com

John in CR   100 GW

100 GW
Posts: 13578
Joined: May 20 2008 12:58am
Location: Paradise

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by John in CR » Dec 01 2011 8:53pm

I'd be content for now if I could get 1.5ah Sony US18650V cells for that same $1.50/ea . That's the kind of deal we need to be looking for instead of this stuff with a minuscule C rate that is just a fire waiting to happen.

thomas.smith   1 µW

1 µW
Posts: 2
Joined: Dec 01 2011 12:56am

Re: 18650 Li-ion at $145 per KiloWatt Hour!

Post by thomas.smith » Dec 29 2011 1:36pm

Ypedal wrote:
thomas.smith wrote: Please do tell us more about how you tested the cells !!

we love pictures ! :P
Sorry it took so long to respond, my actual job (and now lack thereof) has kept me pretty busy.

Well, I picked up a cheap digital/analog IO board, and wrote a quick voltage tracker. Then I rigged a 14w (1C) load, charged the cell, attached to load/voltage tracker (cut off at 2.9v); repeat. It was taking an average of around 52 minutes to drop to 2.9v. Admittedly, hardly what could be considered a really reliable rig.

After my new gig spins up, I am planning to pick up a CBA3 (like neptronix suggested) and run them through their paces again.

P.S. Not sure if I mentioned it, but the cells that I got have no signs of repacking after tearing them down (hehe, I do have a blister for my lack of patience in waiting to discharge it before hacking it up though).