This is the data of the battery I bought.
Baterie is no Lifepo4
Baterie ist LiCoxNiyMnzO2
Here are the most important technical data:
Voltage: 72V
Capacity: 40Ah
Energy: 2880Wh
CE certified
LiCoxNiyMnzO2 / battery
18650 lithium ion single cells
Weight: 16kg
BMS battery management system...
Hello guys
I need help. I replaced the acid battery of 72 volts 20 amps with 72 volts 40 amps lithium polymer battery. Here comes the question about the controller settings.
1. Overvoltage - I realized that it can not be less than 86 volts because it turns off the controller.
2. Undervoltage -...
Votol EM 100 mit 2,3 KW Motor, 60 Volt 80 Ah
I tried everything but the speed remains 25-30 km.
Is there a possibility that the problem is in the electric motor?
Za is designed so that I can be manipulated by the controller.
Hello guys.
These are the original settings of my controller.
I have unchecked the speed limit.
I removed the double voltage check mark.
I will also change the percentages in the speed tree
But I'm worried about values like 5000 High Flux Weakening.
The only speed I have when turning on is...
Hi Guys.
I will show you how my VOTOL EM50M controller works.
In the film you can see how you can easily switch the controller to speed mode with the help of the brake, the throttle and the button, which you can toggle while moving.
1. Turn the throttle grip while depressing the brake. Hold it...
Pin 15 + 12V = sport gear farbe white
pin 4 +12V = 1 bis 3 gear farbe white/brown
I understand that you do not have a display for this, with the programming you will make all the settings
There are two options.
One is: with a button and each time you press you change gears from 1 to 3.
The other is: programmatic each time the Bosch key is turned on.
It is programmatic: You turn the throttle handle together with the brake and hold them. You turn the ignition key and by means of...
Hello
If I decide to buy a controller, what would you recommend?
Who can set up with a program?
I will have to limit it to 45km in first gear but when I want to remove any restrictions.
I'm happy with Votol, but I bought 150 amps before but there were some bugs in the programming. Now I see...
Thanks for the reply.
In this case, the distance is important to me. I have reduced the consumption to save battery but actually 50 amps is enough for me. The bike accelerates well, but it is a scooter and the maximum speed allowed in Germany is 45 km. If they take more pictures of me, they will...
I have one more question.
I am currently using a 72V 20Amp battery
I am considering buying 72v 40amp lithium batteries.
Can you tell me what will change with the new battery.
My controller is VOTOL EM 50S
I have set it with a maximum amperage of 35 amps, but I have a button with a sports mode...
What you see in the pictures, port 4 and 5 are free for me, but I use the port for my speeds, so I have 4 ports (One klick Repair) left free, but how to activate it for cruise control, I have no idea if it's even possible.