Hi,
I fixed a Faraday this way:
https://bikefleetnews.blogspot.com/2021/12/faraday-porteur-s-e-bike-resurrection.html
Having issues now with the Amazon sourced pack cutting OUT at 48volts, not sure if the Faraday
could be shorting it out in vengence...
-T