• Howdy! we're looking for donations to finish custom knowledgebase software for this forum. Please see our Funding drive thread

Recent content by evil_elmo

  1. evil_elmo

    Elmo's Escape Vehicle

    Frame has shipped from CN. Time to start cycling cells. I really forgot how tedious this is. Any suggestions on speeding up the cycling process are appreciated! :lowbatt: Also, I am seeing inconsistent mOhm readings(142mOhm for real :?:) . Suspect its cheap Chinese electronics... At least...
  2. evil_elmo

    Elmo's Escape Vehicle

    I got mine as a lot of 100. However, I think those are sold out. https://www.ebay.com/itm/14-x-Tesla-Battery-CELL-21700-Model-3-Lithium-Ion-4800mah-17-8Wh-NEW-Lot-14/303717112681?hash=item46b6f35b69:g:oEMAAOSwO7dfNFx2
  3. evil_elmo

    Elmo's Escape Vehicle

    I did a conversion of a fuji sunfire 2.0 a few months ago. Well, the bug has bitten me and I've ordered a stealth bomber frame and QS273. Got some Tesla 2170 cells and a Sabvoton 72150. Should be pretty fun build :) Cells: