Well, here it is January 21st and NO batteries yet!
Has any one else ordered Thundersky batteries through Alliance Renewable Energy in the last few month?
I have gotten through to Richard Hatfield once after half a dozen phone attempts and he stated "let me make a phone call and I'll get back...
Good to hear that LOCK.
I recently purchased 9K worth of Thundersky 400 AH from Alliance Reneable Energy. It is on the slow boat from China 8-9 weeks shipping. I am using the Thunderskies on a 4 wheel drive tractor project for work. I have also bought 2.6K worth of thundersky from Elite a few...
That looks really impressive!! Wish I could of been there.
How did the motor handle that acceleration? any excessive heating? Is the powerband instant from 0 to 80mph or did you find an area of acceleration to have more torque?
Those connectors look really slick, good job. I wonder if I would be able to use these in series [u]safetly[u]for my 72 volt set up?
Last year I tried drawing about 300 amps using them in series without protection and cooked some dewalt packs :shock: , I set them aside for use in my business...